Degradation of high temperature MEA with PBI-H3PO4 membrane in a life test

被引:95
|
作者
Modestov, A. D. [1 ]
Tarasevich, M. R. [1 ]
Filimonov, V. Ya. [1 ]
Zagudaeva, N. M. [1 ]
机构
[1] Russian Acad Sci, AN Frumkin Inst Phys Chem & Electrochem, Moscow 119991, Russia
关键词
PEMFC; Fuel cell; Degradation; Lifetime; PBI; EIS; ELECTROLYTE FUEL-CELLS; ACID DOPED POLYBENZIMIDAZOLE; POLYMER-ELECTROLYTE; PHOSPHORIC-ACID; ELECTROCHEMICAL IMPEDANCE; COMPOSITE MEMBRANES; OXYGEN REDUCTION; CATALYST LAYER; PBI MEMBRANE; PERFORMANCE;
D O I
10.1016/j.electacta.2009.07.031
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
The article reports on the results of a 780 h life test of high temperature MEA with PBI-H3PO4 membrane. The MEA was loaded by current density 0.2 A cm(-2) for 763 h at 160 degrees C in hydrogen-air feed. The load was discontinued 14 times during the life test including three complete shut downs. In the course of the life test MEA characteristics were studied by electrochemical methods. Pt particle size growth was evaluated by ex situ measurements of electrochemical hydrogen adsorption/desorption with the cathode catalyst sampled after the life test and with pristine catalyst. Possible changes of electrochemically active surface area (ESA) of carbon support were monitored by electrochemical impedance studies (EIS) performed in the course of the MEA life test. Average Pt particle diameter was found 3.8 and 7.8 nm for pristine catalyst and for catalyst sampled after the life test, respectively. ESA of carbon support remained unchanged, membrane resistance decreased by similar to 20%, hydrogen crossover increased by a factor of 14, although remained insignificant. Voltage loss rate in the life test was similar to 25 mu V h(-1). The major cause of the MEA degradation was identified as a loss of Pt ESA by particle size growth. (C) 2009 Elsevier Ltd. All rights reserved.
引用
收藏
页码:7121 / 7127
页数:7
相关论文
共 50 条
  • [1] Degradation study on MEA in H3PO4/PBI high-temperature PEMFC life test
    Zhai, Yunfeng
    Zhang, Huamin
    Liu, Gang
    Hu, Jingwei
    Yia, Baolian
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2007, 154 (01) : B72 - B76
  • [2] CO electrooxidation study on Pt and Pt-Ru in H3PO4 using MEA with PBI-H3PO4 membrane
    Modestov, A. D.
    Tarasevich, M. R.
    Leykin, A. Y.
    JOURNAL OF POWER SOURCES, 2011, 196 (06) : 2994 - 3002
  • [3] Investigation of methanol electrooxidation on Pt and Pt-Ru in H3PO4 using MEA with PBI-H3PO4 membrane
    Modestov, A. D.
    Tarasevich, M. R.
    Pu, Hongting
    JOURNAL OF POWER SOURCES, 2012, 205 : 207 - 214
  • [4] Effect of open circuit voltage on performance and degradation of high temperature PBI-H3PO4 fuel cells
    Qi, Zhigang
    Buelte, Steve
    JOURNAL OF POWER SOURCES, 2006, 161 (02) : 1126 - 1132
  • [5] Study of the influence of the amount of PBI-H3PO4 in the catalytic layer of a high temperature PEMFC
    Lobato, Justo
    Canizares, Pablo
    Rodrigo, Manuel A.
    Linares, Jose J.
    Javier Pinar, F.
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2010, 35 (03) : 1347 - 1355
  • [6] A study of water adsorption and desorption by a PBI-H3PO4 membrane electrode assembly
    Gu, T.
    Shimpalee, S.
    Van Zee, J. W.
    Chen, C. -Y.
    Lin, C. -W.
    JOURNAL OF POWER SOURCES, 2010, 195 (24) : 8194 - 8197
  • [7] 500h continuous aging life test on PBI/H3PO4 high-temperature PEMFC
    Hu, Jingwei
    Zhang, Huamin
    Zhai, Yunfeng
    Liu, Gang
    Yi, Baolian
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2006, 31 (13) : 1855 - 1862
  • [8] The stability of Pt/C catalyst in H3PO4/PBI PEMFC during high temperature life test
    Zhai, Yunfeng
    Zhang, Huamin
    Xing, Danmin
    Shao, Zhi-Gang
    JOURNAL OF POWER SOURCES, 2007, 164 (01) : 126 - 133
  • [9] Studies of performance degradation of a high temperature PEMFC based on H3PO4-doped PBI
    Liu, Gang
    Zhang, Huamin
    Hu, Jingwei
    Zhai, Yunfeng
    Xu, Dongyan
    Shao, Zhi-gang
    JOURNAL OF POWER SOURCES, 2006, 162 (01) : 547 - 552
  • [10] Degradation Studies of Single Cell and Short Stack for High Temperature Proton Exchange Membrane Fuel Cells Based on PBI/H3PO4 Membrane
    Sun, Xuejing
    Li, Yinhua
    Qi, Fulai
    Jing, Fenning
    Sun, Hai
    Sun, Gongquan
    CHEMISTRYSELECT, 2019, 4 (42): : 12313 - 12319