Passivation mechanism of iron in concentrated phosphoric acid

被引:28
|
作者
Bojinov, M
Betova, I
Fabricius, G
Laitinen, T
Raicheff, R
机构
[1] VTT Mfg Technol, FIN-02044 Espoo, Finland
[2] Helsinki Univ Technol, Phys Chem & Electrochem Lab, FIN-02015 Espoo, Finland
[3] Univ Chem Technol & Met, Dept Electrochem & Corros, BU-1756 Sofia, Bulgaria
关键词
Fe 85%; H(3)P(4) system; passivation; electrochemical impedance spectroscopy; rotating ring-disk electrode; contact electric resistance technique; kinetic model;
D O I
10.1016/S0022-0728(99)00343-5
中图分类号
O65 [分析化学];
学科分类号
070302 ; 081704 ;
摘要
The passivation process of pure iron in 85% H(3)PO(4) was studied by conventional and rotating ring-disk voltammetry, impedance spectroscopy. and de contact electric resistance (SER) techniques. The evolution of the film resistance as a function of potential in the passivation domain, demonstrated that the passivation of iron is most probably due to an adsorbed layer or a fairly conductive precursor film. Rotating ring-disk studies indicated the release of both soluble Fe(II) and Fe(III) in the passivation domain, a peak in the release of Fe(III) coinciding with the active-to-passive transition. impedance spectra of Fe passivation, with a peculiar shape circling the origin of the complex plane, were found to be qualitatively analogous to those for a range of metals in concentrated acidic solutions. A kinetic model is proposed which reproduces quantitatively the steady-state and ac impedance results in the passivation region. (C) 1999 Elsevier Science S.A. All rights reserved.