Enhancing low-cycle fatigue life of commercially-pure Ti by deformation at cryogenic temperature

被引:14
|
作者
Kim, Geonhyeong [1 ]
Shams, Seyed Amir Arsalan [1 ]
Kim, Jae Nam [1 ]
Won, Jong Woo [2 ]
Choi, Seong Woo [2 ]
Hong, Jae Keun [2 ]
Lee, Chong Soo [1 ]
机构
[1] Pohang Univ Sci & Technol POSTECH, Grad Inst Ferrous Technol GIFT, Pohang 37673, South Korea
[2] Korea Inst Mat Sci KIMS, Chang Won 51508, South Korea
关键词
CP-Ti; Low-cycle fatigue (LCF); Deformation twinning; Cryogenic temperature rolling; PURITY TITANIUM; BEHAVIORS; STRENGTH; ALLOYS; TENSILE;
D O I
10.1016/j.msea.2020.140698
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this study, the low-cycle fatigue behavior of a cryogenic-rolled commercially pure titanium alloy was investigated, and compared with those of undeformed and room-temperature rolled ones. The amounts of deformation twins increased to 69.8% after cryogenic temperature rolling, and to 27.5% after room temperature rolling. Strain-controlled low-cycle fatigue tests were performed at total strain amplitudes 0.4% < Delta(epsilon t)/2 <= 1.2%. The Coffin-Manson and hysteresis energy-based models confirmed that low-cycle fatigue resistance was remarkably improved with increasing the volume fraction of deformation twins by pre-deformation. As the proportion of deformation twins in the microstructure increased, the hysteresis loop area decreased, the striation spacing decreased, and the severity of crack-deflection behavior increased. At low Delta(epsilon t)/2 = 0.4%, dislocation recovery was suppressed in the pre-deformed microstructure, so cyclic behavior was stable. However, at Delta(epsilon t)/2 >= 0.8%, the recovery became the predominant mechanism, so well-defined cell structures formed and cyclic softening occurred. The smaller dislocation cells formed in RTR and CTR were considered to cause more severe crack arrest than in AR.
引用
收藏
页数:9
相关论文
共 50 条
  • [1] Low-cycle fatigue behavior of commercially pure titanium
    Takao, K
    Kusukawa, K
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1996, 213 (1-2): : 81 - 85
  • [2] Tensile and low-cycle fatigue behaviors of commercially pure titanium containing γ hydrides
    Chen, CQ
    Li, SX
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 387 : 470 - 475
  • [3] LOW-CYCLE FATIGUE BEHAVIOR OF TI-MN ALLOYS - FATIGUE LIFE
    SALEH, Y
    MARGOLIN, H
    [J]. METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1982, 13 (07): : 1275 - 1281
  • [4] Low-Cycle Fatigue Deformation Behavior and Evaluation of Fatigue Life on Extruded Magnesium Alloys
    Shiozawa, K.
    Kitajima, J.
    Kaminashi, T.
    Murai, T.
    Takahashi, T.
    [J]. 11TH INTERNATIONAL CONFERENCE ON THE MECHANICAL BEHAVIOR OF MATERIALS (ICM11), 2011, 10 : 1244 - 1249
  • [5] Cyclic deformation behaviour of commercially pure titanium at cryogenic temperature
    Sun, QY
    Song, XP
    Gu, HC
    [J]. INTERNATIONAL JOURNAL OF FATIGUE, 2001, 23 (03) : 187 - 191
  • [6] TEMPERATURE-DEPENDENT DEFORMATION MECHANISMS OF ALLOY 718 IN LOW-CYCLE FATIGUE
    SANDERS, TH
    FRISHMUTH, RE
    EMBLEY, GT
    [J]. METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1981, 12 (06): : 1003 - 1010
  • [7] Low-Cycle Fatigue Crack Growth in Ti-6242 at Elevated Temperature
    Brommesson, Rebecka
    Hornqvist, Magnus
    Ekh, Magnus
    [J]. 11TH INTERNATIONAL FATIGUE CONGRESS, PTS 1 AND 2, 2014, 891-892 : 422 - +
  • [8] PREDICTION OF SERVICE LIFE IN LOW-CYCLE FATIGUE
    BIRGER, IA
    [J]. STRENGTH OF MATERIALS, 1985, 17 (10) : 1379 - 1386
  • [9] Low-cycle fatigue life prediction for Waspaloy
    Yeom, JT
    Williams, SJ
    Park, NK
    [J]. MATERIALS AT HIGH TEMPERATURES, 2002, 19 (03) : 153 - 161
  • [10] EFFECT OF TWINNING ON DEFORMATION OF TEXTURED COMMERCIALLY-PURE TI SHEETS UNDER PLANE-STRESS STATES
    MURAYAMA, Y
    OBARA, K
    IKEDA, K
    [J]. MATERIALS TRANSACTIONS JIM, 1993, 34 (09): : 801 - 808