Effect of test speed and twist level on the hairiness of worsted yarns

被引:0
|
作者
Wang, XG [1 ]
Huang, W
Huang, XB
机构
[1] Deakin Univ, Sch Engn & Technol, Geelong, Vic 3217, Australia
[2] Univ New S Wales, Dept Text Technol, Sydney, NSW 2052, Australia
[3] China Text Univ, Coll Text Sci & Technol, Shanghai 200051, Peoples R China
关键词
D O I
暂无
中图分类号
TB3 [工程材料学]; TS1 [纺织工业、染整工业];
学科分类号
0805 ; 080502 ; 0821 ;
摘要
This paper examines the effect of test speed and yarn twist level on the hairiness of worsted yarns. Pure wool yarns of three different twist levels are spun on a worsted ring frame, then tested for hairiness on the hairiness attachment to a Uster Tester 3 at three speeds of 25, 100, and 400 m/min. The results indicate that regardless of the yam's twist level, yarn hairiness tested at 400 m/min is higher than that obtained at 25 and 100 m/min, and the difference is statistically significant at the 5% significance level. But there is no statistically significant difference between hairiness results obtained at 25 and 100 m/min. In addition, yarn hairiness readings in single measurements follow a lognormal distribution.
引用
收藏
页码:889 / 892
页数:4
相关论文
共 50 条