- [1] Anisotropic threshold stress intensity factor, KIH and crack growth rate in delayed hydride cracking of Zr-2.5Nb pressure tubes Metallurgical and Materials Transactions A, 2002, 33 : 919 - 925
- [4] Threshold stress intensity factor, KIH for delayed hydride cracking of a Zr-2.5Nb tube with loading mode Journal of Alloys and Compounds, 2008, 462 (1-2): : 367 - 375
- [6] Temperature dependence of threshold stress intensity factor, KIH in Zr-2.5Nb alloy and its effect on temperature limit for delayed hydride cracking Experimental Mechanics in Nano and Biotechnology, Pts 1 and 2, 2006, 326-328 : 919 - 922
- [8] Crack tip stress effect on delayed hydride cracking velocity of Zr-2.5Nb tubes MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 490 (1-2): : 146 - 150