Fine machining of large-diameter 6H-SiC wafers

被引:0
|
作者
Chen, Xiufang [1 ]
Li, Juan [1 ]
Ma, Deying [1 ]
Hu, Xiaobo [1 ]
Xu, Xiangang [1 ]
机构
[1] Shandong Univ, State Key Lab Crystal Mat, Jinan 250100, Peoples R China
关键词
6H-SiC; chemo-mechanical polishing (CMP); roughness;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Three main machining processes of large-diameter 6H-SiC wafers were introduced in this paper. These processes include cutting, lapping and polishing. Lapping causes great residual stresses and deep damage layer which can be reduced gradually with subsequent polishing processes. Surfaces prepared by mechanical polishing (MP) appeared a large number of scratches with depth of 5 similar to 8 nm. These scratches can be effectively removed by chemo-mechanical polishing (CMP). After CMP, extremely smooth and low damage layer surface with roughness R-a=0.3 nm was obtained. Atomic force microscopy (AFM) and optical microscopy were used to observe the surface morphology of samples and a high resolution X-ray diffractometer (HRXRD) was used for the crystal lattice perfection of the subsurface region. Changes of surface residual stresses during machining processes were investigated by HRXRD.
引用
收藏
页码:681 / 684
页数:4
相关论文
共 50 条
  • [1] Fine machining of large-diameter 6H-SiC wafers
    State Key Laboratory of Crystal Materials, Shandong University, Jinan 250100, China
    J Mater Sci Technol, 2006, 5 (681-684):
  • [2] Fine Machining of Large-Diameter 6H-SiC Wafers
    Xiufang CHEN
    Journal of Materials Science & Technology, 2006, (05) : 681 - 684
  • [3] LARGE-DIAMETER 6H-SIC FOR MICROWAVE DEVICE APPLICATIONS
    HOBGOOD, HM
    BARRETT, DL
    MCHUGH, JP
    CLARKE, RC
    SRIRAM, S
    BURK, AA
    GREGGI, J
    BRANDT, CD
    HOPKINS, RH
    CHOYKE, WJ
    JOURNAL OF CRYSTAL GROWTH, 1994, 137 (1-2) : 181 - 186
  • [5] Observation of surface defects in 6H-SiC wafers
    1600, American Inst of Physics, Woodbury, NY, USA (74):
  • [6] STRUCTURAL MACRO-DEFECTS IN 6H-SIC WAFERS
    GLASS, RC
    KJELLBERG, LO
    TSVETKOV, VF
    SUNDGREN, JE
    JANZEN, E
    JOURNAL OF CRYSTAL GROWTH, 1993, 132 (3-4) : 504 - 512
  • [7] Nonuniformities of electrical resistivity in undoped 6H-SiC wafers
    Li, Q
    Polyakov, AY
    Skowronski, M
    Sanchez, EK
    Loboda, MJ
    Fanton, MA
    Bogart, T
    Gamble, RD
    JOURNAL OF APPLIED PHYSICS, 2005, 97 (11)
  • [8] OBSERVATION OF SURFACE-DEFECTS IN 6H-SIC WAFERS
    EVWARAYE, AO
    SMITH, SR
    SKOWRONSKI, M
    MITCHEL, WC
    JOURNAL OF APPLIED PHYSICS, 1993, 74 (08) : 5269 - 5271
  • [9] Resistivity distribution in undoped 6H-SiC boules and wafers
    Li, Q.
    Polyakov, A. Y.
    Skowronski, M.
    Sanchez, E. K.
    Loboda, M. J.
    Fanton, M. A.
    Bogart, T.
    Gamble, D.
    Smirnov, N. B.
    Makarov, Yu.
    Silicon Carbide and Related Materials 2005, Pts 1 and 2, 2006, 527-529 : 51 - 54
  • [10] X-ray characterization of 3 inch diameter 4H and 6H-SiC experimental wafers
    Kuhr, TA
    Vetter, WM
    Dudley, M
    Skowronski, M
    SILICON CARBIDE AND RELATED MATERIALS - 1999 PTS, 1 & 2, 2000, 338-3 : 473 - 476