Assessment of thermal and thermo-oxidative stability of multiextruded recycled PP, HDPE and a blend thereof

被引:107
|
作者
Camacho, W [1 ]
Karlsson, S [1 ]
机构
[1] Royal Inst Technol, Dept Polymer Technol, S-10044 Stockholm, Sweden
关键词
PP; HDPE; blends; stability;
D O I
10.1016/S0141-3910(02)00192-1
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Differential scanning calorimetry (DSC), thermo gravimetric analysis (TGA) and chemiluminescence (CL) techniques have been used for assessment of thermal and thermo-oxidative stability of recycled PP, HDPE and their blend containing 20 wt.% of PP. The pure polymers and the blend were subjected to six extrusion cycles. The oxidation induction time (OIT) of the PP, PE and the blend decreased with the number of extrusion cycles also did the temperature of oxidation (T-ox). The thermal stability of PE decreased with the number of number of processing cycles, which may indicate that the shear forces during processing induce chain scission of the polymer backbone leading mainly to shortening of the chains. PP, however showed a decrease in thermal stability up to the third extrusion, and about the same stability during further processing. Thus chain scission predominated during all the extrusions and no chain branching or crosslinking were observed. The behaviour of the blend showed a synergetic tendency and did not obey the "mixture rule". The CL runs produced a clearer picture of the oxidation process in blends since two peaks were observed, a sharp one corresponding to the PP and the other of bimodal shape to PE. The PP appeared to oxidize first and accelerated the oxidation of PE due to the presence of oxidation sites in the PE-PP interfaces. The blend of PP an HDPE mechanically mixed appeared to be a two-phase system in the molten state. This information can not be obtained from DSC and TG experiments. (C) 2002 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:385 / 391
页数:7
相关论文
共 50 条
  • [1] Influence of grape seed oil into recycled polypropylene (PP) thermo-oxidative degradation
    da Costa, Helson Moreira
    Ramos, Valeria Dutra
    Andrade Estanislau Cyrino, Jacques Satler
    MATERIA-RIO DE JANEIRO, 2021, 26 (01):
  • [2] The effect of thermal and thermo-oxidative degradation conditions on rheological, chemical and thermal properties of HDPE
    Cuadri, A. A.
    Martin-Alfonso, J. E.
    POLYMER DEGRADATION AND STABILITY, 2017, 141 : 11 - 18
  • [3] An assessment of the role of morphology in thermal/thermo-oxidative degradation mechanism of PP/EVA/clay nanocomposites
    Goodarzi, Vahabodin
    Jafari, Seyed Hassan
    Khonakdar, Hossein Ali
    Monemian, Seyed Ali
    Mortazavi, Mehdi
    POLYMER DEGRADATION AND STABILITY, 2010, 95 (05) : 859 - 869
  • [4] Thermo-oxidative stability of PP waste films studied by imaging chemiluminescence
    Ahlblad, G
    Gijsman, P
    Terselius, B
    Jansson, A
    Möller, K
    POLYMER DEGRADATION AND STABILITY, 2001, 73 (01) : 15 - 22
  • [5] Thermo-Oxidative Degradation Behavior of Recycled Polypropylene
    Nasir, Asad
    Yasin, Tariq
    Islam, Atif
    JOURNAL OF APPLIED POLYMER SCIENCE, 2011, 119 (06) : 3315 - 3320
  • [6] Thermal and thermo-oxidative stability of reprocessed poly(ethylene terephthalate)
    Badia, J. D.
    Martinez-Felipe, A.
    Santonja-Blasco, L.
    Ribes-Greus, A.
    JOURNAL OF ANALYTICAL AND APPLIED PYROLYSIS, 2013, 99 : 191 - 202
  • [7] Thermal and thermo-oxidative stability of reprocessed poly(ethylene terephthalate)
    Ribes-Greus, A. (aribes@ter.upv.es), 1600, Elsevier B.V., Netherlands (99):
  • [8] Evaluation of Thermo-oxidative Stability of Biodiesel
    Savi, Elton L.
    Herculano, Leandro S.
    Lukasievicz, Gustavo V. B.
    Torquato, Alex S.
    Baesso, Mauro L.
    Astrath, Nelson G. C.
    Malacarne, Luis C.
    ENERGY & FUELS, 2017, 31 (07) : 7132 - 7137
  • [9] On the thermal behaviour and thermo-oxidative stability of liquid crystalline triphenylene compounds
    Schartel, B
    Kettner, A
    Kunze, R
    Wendorff, JH
    Hennecke, M
    ADVANCED MATERIALS FOR OPTICS AND ELECTRONICS, 1999, 9 (02): : 55 - 64
  • [10] THERMAL AND THERMO-OXIDATIVE DEGRADATION OF "POLYNAPHTHYLIMIDOPHENYLQUINOXALINES
    KORSHAK, VV
    PAVLOVA, SSA
    GRIBKOVA, PN
    VLASOVA, IV
    KRONGAUZ, ES
    BELOMOINA, NM
    VYSOKOMOLEKULYARNYE SOEDINENIYA SERIYA A, 1979, 21 (01): : 93 - 99