Microindentation deformation of lithium dihydrogen phosphate single crystals: Microhardness measurement and indentation size effect

被引:8
|
作者
Iurchenko, Anton [1 ]
Borc, Jaroslaw [2 ]
Sangwal, Keshra [2 ]
Voronov, Alexei [1 ]
机构
[1] Natl Acad Sci Ukraine, Inst Single Crystals, Lenin Ave 60, UA-61001 Kharkov, Ukraine
[2] Lublin Univ Technol, Dept Appl Phys, Ul Nadbystrzycka 38, PL-20618 Lublin, Poland
关键词
Crystal growth; Indentation; Hardness; Crack; STRAIN GRADIENT PLASTICITY; MECHANICAL-PROPERTIES; INDENTER ANGLE; LIH2PO4; GROWTH; CRACKS; SOLIDS; HARDNESS; GLASSES; SYSTEM;
D O I
10.1016/j.matchemphys.2015.12.052
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The Vickers microhardness H-V of the (110) and (111) as-grown faces of lithium dihydrogen phosphate (LDP) crystals was investigated as a function of applied load P. The microhardness H-V of the two faces increases with load P i.e. reverse indentation size effect (reverse ISE) and the hardness of the (110) face is somewhat lower than that of the (111) face but this difference is not easily recognized for these planes due to large scatter in the data. The origin of observed ISE was analyzed using different approaches. It was found that: (1) Hays-Kendall's and Begley-Hutchinson's relations do not explain the origin of reverse ISE but Meyer's law describes the reverse ISE satisfactorily and its constants provide a link between ISE and formation of radial cracks with applied indentation load P, (2) reverse ISE is associated with tensile surface stresses, (3) despite its failure to explain reverse ISE, Begley-Hutchinson's relation is reliable to obtain load-independent hardness H-0, is 2337 MPa for LDP, and (4) the value of fracture toughness K-C of LDP crystals lies between 4.7 and 12 MPa m(1/2). The load-independent hardness H-0 of LDP is higher by a factor of 1.5 than that reported for undoped KDP and ADP crystals whereas its fracture toughness K-C is higher by factor of about 20 than that of undoped KDP crystals. (C) 2015 Elsevier B.V. All rights reserved.
引用
收藏
页码:276 / 284
页数:9
相关论文
共 50 条
  • [1] Indentation size effect and microhardness study of β-Sn single crystals
    Sahin, O
    Uzun, O
    Kolemen, U
    Duzgun, B
    Ucar, N
    CHINESE PHYSICS LETTERS, 2005, 22 (12) : 3137 - 3140
  • [2] Microhardness and indentation fracture of potassium dihydrogen phosphate (KDP)
    Fang, T
    Lambropoulos, JC
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2002, 85 (01) : 174 - 178
  • [3] THE MICROHARDNESS INDENTATION LOAD SIZE EFFECT IN RUTILE AND CASSITERITE SINGLE-CRYSTALS
    LI, H
    BRADT, RC
    JOURNAL OF MATERIALS SCIENCE, 1993, 28 (04) : 917 - 926
  • [4] MICROHARDNESS INVESTIGATIONS ON POTASSIUM DIHYDROGEN PHOSPHATE CRYSTALS
    JOSHI, MS
    ANTONY, AV
    MOHANRAO, P
    KRISTALL UND TECHNIK-CRYSTAL RESEARCH AND TECHNOLOGY, 1980, 15 (06): : 743 - 746
  • [5] On the reverse indentation size effect and microhardness measurement of solids
    Sangwal, K
    MATERIALS CHEMISTRY AND PHYSICS, 2000, 63 (02) : 145 - 152
  • [6] The Effect of Aluminum Deformation Conditions on Microhardness and Indentation Size Effect Characteristics
    Blasko, Peter
    Petrik, Jozef
    Solc, Marek
    Mihalikova, Maria
    Girmanova, Lenka
    Pribulova, Alena
    Futas, Peter
    Furman, Joanna
    Marzena, Kuczynska-Chalada
    CRYSTALS, 2025, 15 (03)
  • [7] MICROHARDNESS OF SOME CRYSTALS WITH POTASSIUM DIHYDROGEN PHOSPHATE STRUCTURE
    RAO, KK
    SIRDESHMUKH, DB
    INDIAN JOURNAL OF PURE & APPLIED PHYSICS, 1978, 16 (09) : 860 - 861
  • [8] Effect of repeated nanoindentations on the deformation of potassium dihydrogen phosphate crystals
    Yang, Shengyao
    Zhang, Liangchi
    Wu, Zhonghuai
    CERAMICS INTERNATIONAL, 2022, 48 (07) : 9595 - 9601
  • [9] Study of indentation size effect and microhardness of SrLaAlO4 and SrLaGaO4 single crystals
    Sangwal, K
    Surowska, B
    MATERIALS RESEARCH INNOVATIONS, 2003, 7 (02) : 91 - 104
  • [10] PLASTIC DEFORMATION IN AMMONIUM DIHYDROGEN PHOSPHATE CRYSTALS
    SALKOVITZ, EI
    SMITH, PL
    PHYSICAL REVIEW, 1953, 90 (02): : 350 - 350