Effect of Intercritical Annealing Time on Microstructure and Axial Mechanical Properties of TRIP Seamless Steel Tube

被引:5
|
作者
Zhang, Zicheng [1 ,2 ]
Li, Yanmei [3 ]
Kong, Xiangwei [1 ]
Manabe, Ken-ichi [2 ]
Wang, Na [4 ]
机构
[1] Northeastern Univ, Sch Mech Engn & Automat, Shenyang 110819, Peoples R China
[2] Tokyo Metropolitan Univ, Dept Mech Engn, Hachioji, Tokyo 1920397, Japan
[3] Northeastern Univ, State Key Lab Rolling & Automat, Shenyang 110819, Peoples R China
[4] Shanghai Baosteel Hydroforming Parts Co Ltd, Shanghai 201908, Peoples R China
关键词
heat treatment; TRIP steel; hydroformability; mechanical properties; seamless steel tube; RETAINED AUSTENITE; HEAT-TREATMENT; TRANSFORMATION; COMPONENTS; STABILITY; FERRITE; CARBON;
D O I
10.1002/srin.201300153
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The transformation-induced plasticity (TRIP) seamless steel tube, which is expected to be used in the hydroforming process, was prepared with piercing, cold-drawing and two-stage heat treatment process (intercritical annealing, IA and isothermal bainite treatment, IBT). The current study focused on the effect of IA holding time on microstructure and mechanical properties of TRIP seamless steel tube at a predetermined other heat treatment conditions, to maximize the volume fraction and stability of retained austenite as well as to obtain a TRIP seamless steel tube with good combination of strength and ductility. The microstructure and retained austenite volume fraction of the heat-treated steel tubes were studied via optical microscopy, transmission electron microscopy and X-ray diffraction. Two-stage heat treatment carried out in an electrical resistance furnace and a salt-bath furnace showed that for a predetermined IA temperature, IBT temperature and time, the content of retained austenite as well as total elongation increased first and then decreased with increasing IA time in the set time range in this study. When IA time was 10min, the largest retained austenite volume fractions for both steel tubes was obtained. As a result, the TRIP seamless steel tube with an austenite volume fraction of 7.02%, total elongation of 35.5% and ultimate tensile strength of 618MPa was successfully obtained.
引用
收藏
页码:632 / 639
页数:8
相关论文
共 50 条
  • [1] Effect of Heat Treatment on Microstructure and Mechanical Properties of TRIP Seamless Steel Tube
    Zhang, Zicheng
    Li, Yanmei
    Manabe, Ken-ichi
    Zhu, Fuxian
    [J]. MATERIALS TRANSACTIONS, 2012, 53 (05) : 833 - 837
  • [2] The Effect of Intercritical Annealing on the Microstructure and Mechanical Properties in a High Strength TRIP Steel with C-Partitioning
    Wang, Chao
    Ding, Hua
    Tang, Zhengyou
    Zhang, Jun
    Di, Huafang
    [J]. STEEL RESEARCH INTERNATIONAL, 2014, 85 (03) : 388 - 394
  • [3] Effects of intercritical annealing on microstructure and mechanical properties of low silicon trip steel with phosphorus addition
    Chen, Peng
    Xu, Yun-Bo
    Shen, Chun-Yu
    Wang, Guo-Dong
    [J]. Dongbei Daxue Xuebao/Journal of Northeastern University, 2013, 34 (11): : 1562 - 1565
  • [4] Effect of Microstructure before Intercritical Annealing on Mechanical Properties of 5% Mn Steel
    Natsumeda, Hirokazu
    Kitahara, Amane
    Hashimoto, Shunichi
    [J]. ISIJ INTERNATIONAL, 2017, 57 (05) : 945 - 952
  • [5] Effect of Intercritical Annealing Time on the Microstructures and Tensile Properties of a High Strength TRIP Steel
    Chao Wang
    Hua Ding
    Jun Zhang
    Hongyan Wu
    [J]. Acta Metallurgica Sinica(English Letters), 2014, 27 (03) : 457 - 463
  • [6] Effect of Isothermal Bainite Treatment on Microstructure and Mechanical Properties of Low-Carbon TRIP Seamless Steel Tube
    Zhang, Zicheng
    Manabe, Ken-ichi
    Li, Yanmei
    Zhu, Fuxian
    [J]. STEEL RESEARCH INTERNATIONAL, 2012, 83 (07) : 645 - 652
  • [7] Effect of Intercritical Annealing Time on the Microstructures and Tensile Properties of a High Strength TRIP Steel
    Wang, Chao
    Ding, Hua
    Zhang, Jun
    Wu, Hongyan
    [J]. ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2014, 27 (03) : 457 - 463
  • [8] Effect of Intercritical Annealing Time on the Microstructures and Tensile Properties of a High Strength TRIP Steel
    Chao Wang
    Hua Ding
    Jun Zhang
    Hongyan Wu
    [J]. Acta Metallurgica Sinica (English Letters), 2014, 27 : 457 - 463
  • [9] Microstructure and mechanical properties of medium manganese steel in intercritical annealing
    Feng, Yan
    Jing, Cainian
    Lin, Tao
    Wu, Zhonglin
    Li, Zhaotong
    Zhao, Jingrui
    [J]. MATERIALS SCIENCE AND TECHNOLOGY, 2023, 39 (15) : 2102 - 2110
  • [10] Effect of Holding Time on the Microstructure and Mechanical Properties of Dual-Phase Steel during Intercritical Annealing
    李壮
    WU Di
    Lü Wei
    YU Huanhuan
    SHAO Zhenyao
    LUO Lei
    [J]. Journal of Wuhan University of Technology(Materials Science Edition), 2015, 30 (01) : 156 - 161