The effect of ultrasonic treatment on iron-chromium pillared bentonite synthesis and catalytic wet peroxide oxidation of phenol

被引:29
|
作者
Tomul, Fatma [1 ]
机构
[1] Mehmet Akif Ersoy Univ, Fac Arts & Sci, Dept Chem, Burdur, Turkey
关键词
Fe/Cr-pillared bentonite; Phenol; Ultrasonic treatment; CWPO; AL-CE-FE; TEXTURAL PROPERTIES; HYDROGEN-PEROXIDE; CLAYS; DEGRADATION; COPPER; 2-CHLOROPHENOL; COMPOSITE; REMOVAL; SULFATE;
D O I
10.1016/j.clay.2015.11.007
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In this study, compared to traditional methods, Fe/Cr-pillared bentonite synthesis whose Fe/Cr mol ratio is 1/9 is carried out by considerably reducing the water consumption and synthesis time. Fe/Cr-pillared bentonites were characterized by scanning electron microscope with energy dispersive system (SEM-EDS), powder X-ray diffraction (XRD) and N-2-adsorption/desorption isotherm. The characterization results indicated that the Fe/Cr-DC sample prepared by adding dry clay to the pillaring solution directly exhibits comparable surface properties to those of the sample (Fe/Cr-SS) prepared by adding the pillaring solution on clay dispersion slowly. Catalytic behavior of Fe/Cr-pillared bentonites was tested for the catalytic wet peroxide oxidation (CWPO) of phenol with ultrasonic heating. No significant difference is observed among the phenol conversions for all of the synthesized samples. Phenol conversion increased with increasing temperature until 45 degrees C, but further increasing the temperature in higher than 45 degrees C was not very effective. The phenol conversion at pH 5 was higher than at pH 7. Additionally, a nearly complete removal of phenol was obtained over 2 h using Fe/Cr-DC catalysts, at the experimental conditions of T = 45 degrees C, pH 5, m(cat) = 5 g/L, [H2O2/phenol] = 16, during reaction peroxide addition (2 x 10(-4) mol/h) and ultrasonic heating. It is obtained that, aromatic intermediate products as catechol, hydroquinone and benzoquinones which are obtained in the beginning of oxidation oxidated into carboxylic acids. However, carboxylic acids such as oxalic and formic acid showing resistance to oxidation results by the level of total organic carbon (TOC) conversion being low. (C) 2015 Elsevier B.V. All rights reserved.
引用
收藏
页码:121 / 134
页数:14
相关论文
共 50 条
  • [1] Active iron species in the catalytic wet peroxide oxidation of phenol over pillared clays containing iron
    Guélou, E
    Barrault, J
    Fournier, J
    Tatibouët, JM
    [J]. APPLIED CATALYSIS B-ENVIRONMENTAL, 2003, 44 (01) : 1 - 8
  • [2] Catalytic wet peroxide oxidation of phenol over pillared clays containing iron or copper species
    Barrault, J
    Tatibouët, JM
    Papayannakos, N
    [J]. COMPTES RENDUS DE L ACADEMIE DES SCIENCES SERIE II FASCICULE C-CHIMIE, 2000, 3 (10): : 777 - 783
  • [3] Catalytic wet oxidation of phenol by hydrogen peroxide over pillared clay catalyst
    Guo, J
    Al-Dahhan, M
    [J]. INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2003, 42 (12) : 2450 - 2460
  • [4] Catalytic wet peroxide oxidation of phenol over AlFe-pillared montmorillonite
    Ernő E. Kiss
    Jonjaua G. Ranogajec
    Radmila P. Marinković-Nedučin
    Tatjana J. Vulić
    [J]. Reaction Kinetics and Catalysis Letters, 2003, 80 : 255 - 260
  • [5] Catalytic wet peroxide oxidation of phenol over AlFe-pillared montmorillonite
    Kiss, EE
    Ranogajec, JG
    Marinkovic-Neducin, RP
    Vulic, TJ
    [J]. REACTION KINETICS AND CATALYSIS LETTERS, 2003, 80 (02): : 255 - 260
  • [6] Catalytic wet peroxide oxidation of phenol over Fe-exchanged pillared beidellite
    Catrinescu, C
    Teodosiu, C
    Macoveanu, M
    Miehe-Brendlé, J
    Le Dred, R
    [J]. WATER RESEARCH, 2003, 37 (05) : 1154 - 1160
  • [7] Catalytic Activity of Phenol Oxidation over Iron and Cooper-Exchanged Pillared Bentonite
    Khalida Chellal
    Fahim Hamidouche
    Naima Boudieb
    Zineb Meguellati
    Mohamed Trari
    [J]. Chemistry Africa, 2024, 7 : 1563 - 1573
  • [8] Catalytic Activity of Phenol Oxidation over Iron and Cooper-Exchanged Pillared Bentonite
    Chellal, Khalida
    Hamidouche, Fahim
    Boudieb, Naima
    Meguellati, Zineb
    Trari, Mohamed
    [J]. CHEMISTRY AFRICA-A JOURNAL OF THE TUNISIAN CHEMICAL SOCIETY, 2024, 7 (03): : 1563 - 1573
  • [9] Synthesis of MFI structured iron silicates and their catalytic performance in phenol removal by wet peroxide oxidation
    Horova, Dorota
    Novakova, Jana
    Peliskova, Lenka
    Kohout, Jan
    Safar, Jan
    Hrachovcova, Katerina
    Tokarova, Venceslava
    [J]. REACTION KINETICS MECHANISMS AND CATALYSIS, 2020, 130 (02) : 1077 - 1092
  • [10] Synthesis of MFI structured iron silicates and their catalytic performance in phenol removal by wet peroxide oxidation
    Dorota Horová
    Jana Nováková
    Lenka Pelíšková
    Jan Kohout
    Jan Šafář
    Kateřina Hrachovcová
    Věnceslava Tokarová
    [J]. Reaction Kinetics, Mechanisms and Catalysis, 2020, 130 : 1077 - 1092