Vacuum-arc chromium-based coatings for protection of zirconium alloys from the high-temperature oxidation in air

被引:119
|
作者
Kuprin, A. S. [1 ]
Belous, V. A. [1 ]
Voyevodin, V. N. [1 ]
Bryk, V. V. [1 ]
Vasilenko, R. L. [1 ]
Ovcharenko, V. D. [1 ]
Reshetnyak, E. N. [1 ]
Tolmachova, G. N. [1 ]
V'yugov, P. N. [1 ]
机构
[1] Kharkov Inst Phys & Technol, Natl Sci Ctr, UA-61108 Kharkov, Ukraine
关键词
Zirconium; Oxidation; Zirconium oxide; Vacuum arc; Coatings; ELASTIC-MODULUS; STEAM OXIDATION; ZIRCALOY-4; TRANSFORMATION; INDENTATION; HARDNESS; OXYGEN; FILMS;
D O I
10.1016/j.jnucmat.2015.06.016
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Multilayer Cr-Zr/Cr/Cr-N coatings for protection of zirconium alloys from the high-temperature oxidation in air have been obtained by the vacuum-arc evaporation technique with application of filters for plasma cleaning from macroparticles. The effect of the coatings on the corrosion resistance of zirconium alloys at test temperatures between 660 and 1100 degrees C for 3600 s has been investigated. The thickness, structure, phase composition, mechanical properties of the coatings and oxide layers before and after oxidation tests were examined by scanning electron microscopy, X-ray diffraction analysis and nanoindentation technique. It is shown that the hard multilayer coating effectively protects zirconium from the oxidation in air for 1 h at test temperatures. As a result of the oxidation in the coating the CrO and Cr2O3 oxides are formed which reduce the oxygen penetration through the coating. At maximum test temperature of 1100 degrees C the oxide layer thickness in the coating is about 5 mu m. The tube shape remains unchanged independent of alloy type. It has been found that uncoated zirconium oxidizes rapidly throughout the temperature range under study. At 1100 degrees C a porous monoclinic ZrO2 oxide layer of >= 120 mu m is formed that leads to the deformation of the samples, cracking and spalling of the oxide layer. (C) 2015 Elsevier B.V. All rights reserved.
引用
收藏
页码:400 / 406
页数:7
相关论文
共 50 条
  • [1] VACUUM-ARC CHROMIUM COATINGS FOR Zr-1Nb ALLOY PROTECTION AGAINST HIGH-TEMPERATURE OXIDATION IN AIR
    Kuprin, A. S.
    Belous, V. A.
    Bryk, V. V.
    Vasilenko, R. L.
    Voyevodin, V. N.
    Ovcharenko, V. D.
    Tolmachova, G. N.
    Kolodiy, I. V.
    Lunyov, V. M.
    Klimenko, I. O.
    [J]. PROBLEMS OF ATOMIC SCIENCE AND TECHNOLOGY, 2015, (02): : 111 - 118
  • [2] Chromium and chromium-based alloys: Problems and possibilities for high-temperature service
    Y. F. Gu
    H. Harada
    Y. Ro
    [J]. JOM, 2004, 56 : 28 - 33
  • [3] Chromium and chromium-based alloys: Problems and possibilities for high-temperature service
    Gu, YF
    Harada, H
    Ro, Y
    [J]. JOM, 2004, 56 (09) : 28 - 33
  • [4] High-Temperature Hardness of Multilayer Vacuum-Arc Metal–Metal Nitride Coatings
    V. F. Gorban’
    A. O. Andreev
    V. A. Stolbovoi
    S. A. Firstov
    V. K. Shkolniy
    [J]. Journal of Superhard Materials, 2021, 43 : 198 - 202
  • [5] High-Temperature Hardness of Multilayer Vacuum-Arc Metal-Metal Nitride Coatings
    Gorban', V. F.
    Andreev, A. O.
    Stolbovoi, V. A.
    Firstov, S. A.
    Shkolniy, V. K.
    [J]. JOURNAL OF SUPERHARD MATERIALS, 2021, 43 (03) : 198 - 202
  • [6] High-temperature oxidation resistance of chromium-based coatings deposited by DLI-MOCVD for enhanced protection of the inner surface of long tubes
    Michau, A.
    Maury, F.
    Schuster, F.
    Lomello, F.
    Brachet, J. -C.
    Rouesne, E.
    Le Saux, M.
    Boichot, R.
    Pons, M.
    [J]. SURFACE & COATINGS TECHNOLOGY, 2018, 349 : 1048 - 1057
  • [7] EVALUATION OF PROPERTIES OBTAINED FROM AN AIR-INDUCTION AND VACUUM-ARC MELTED HIGH-TEMPERATURE ALLOY
    BULINA, J
    BROWN, JT
    [J]. TRANSACTIONS OF THE AMERICAN INSTITUTE OF MINING AND METALLURGICAL ENGINEERS, 1959, 215 (04): : 571 - 577
  • [8] High temperature oxidation protective chromium-based coatings prepared by IBAD and PACVD methods
    Cerny, F.
    Pitter, J.
    Konvickova, S.
    Jech, V.
    [J]. SURFACE & COATINGS TECHNOLOGY, 2009, 203 (17-18): : 2566 - 2570
  • [9] Protection of Niobium and Alloys Based on It from High-Temperature Oxidation.
    Prokoshkin, D.A.
    Mashkovich, A.I.
    Demin, Yu.N.
    Yakushin, V.P.
    [J]. 1600,
  • [10] Chromium-based high-temperature selective solar absorber
    Cao, Yuchun
    Feng, Yongtao
    Chen, Ning
    Liu, Haotuo
    Zhang, Heng
    Meng, Zhaoqing
    Wu, Xiaohu
    [J]. APPLIED OPTICS, 2024, 63 (18) : 4983 - 4992