Fretting wear behaviour of plasma nitrided Ti-6Al-4V fretted against unnitrided Ti-6Al-4V and alumina counterbodies

被引:0
|
作者
Ali, M. Mubarak [1 ]
Raman, S. Ganesh Sundara [1 ]
Pathak, S. D. [1 ]
Gnanamoorthy, R. [2 ]
机构
[1] Indian Inst Technol, Dept Met & Mat Engn, Madras 600036, Tamil Nadu, India
[2] Indian Inst Technol, Dept Mech Engn, Madras 600036, Tamil Nadu, India
关键词
Fretting wear; plasma nitriding time; plasma nitriding environment; Ti-6Al-4V; tangential force coefficient; MECHANICAL-PROPERTIES; TITANIUM; FATIGUE; ALLOY;
D O I
暂无
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Ti-6Al-4V samples were plasma nitrided at 520 degrees C in two environments (nitrogen and a mixture of nitrogen and hydrogen in the ratio of 3: 1) for two different time periods (4 h and 18 h). Fretting wear tests were conducted on unnitrided and nitrided samples for 50,000 cycles using two counterbody materials (unnitrided Ti-6Al-4V and alumina). Gross slip prevailed at a normal load of 4.9 N while mixed stick-slip prevailed at 9.8 N. Tangential force coefficient values of plasma nitrided samples were lower than those of unnitrided samples. The tangential force coefficient nearly stabilised after thousand cycles in case of samples tested against Ti-6Al-4V counterbody. On the other hand, it showed a continuously increasing trend in case of specimens tested against alumina counterbody. The samples nitrided for 4 h exhibited higher hardness and lower tangential force coefficient compared to the specimens nitrided for 18 h. The samples nitrided in nitrogen-hydrogen mixture environment exhibited higher hardness and lower tangential force coefficient compared to the specimens nitrided in nitrogen. The samples plasma nitrided in nitrogen-hydrogen mixture for 4 h exhibited the highest hardness and the lowest tangential force coefficient. The wear volume of the plasma nitrided samples was lower than that of the unnitrided samples. Owing to tribochemical reactions, the wear volume of unnitrided and nitrided samples fretted against alumina ball was higher than that of the samples fretted against Ti-6Al-4V. A consistent trend was not observed regarding which nitriding condition would result in lower wear volume at different loads.
引用
收藏
页码:59 / 64
页数:6
相关论文
共 50 条
  • [1] Fretting wear behaviour of plasma nitrided Ti-6Al-4V fretted against unnitrided Ti-6Al-4V and alumina counterbodies
    Ali M.M.
    Raman S.G.S.
    Pathak S.D.
    Gnanamoorthy R.
    [J]. Transactions of the Indian Institute of Metals, 2009, 62 (1) : 59 - 64
  • [2] Influence of plasma nitriding on fretting wear behaviour of Ti-6Al-4V
    Ali, M. Mubarak
    Raman, S. Ganesh Sundara
    Pathak, S. D.
    Gnanamoorthy, R.
    [J]. TRIBOLOGY INTERNATIONAL, 2010, 43 (1-2) : 152 - 160
  • [3] Plain fatigue and fretting fatigue behaviour of plasma nitrided Ti-6Al-4V
    Rajasekaran, B.
    Raman, S. Ganesh Sundara
    [J]. MATERIALS LETTERS, 2008, 62 (15) : 2473 - 2475
  • [4] Effect of mean stress on fretting fatigue of Ti-6Al-4V on Ti-6Al-4V
    Lovrich, NR
    Neu, RW
    [J]. FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2006, 29 (01) : 41 - 55
  • [5] Effect of shot peening on the fretting wear of Ti-6Al-4V
    Fridrici, V
    Fouvry, S
    Kapsa, P
    [J]. WEAR, 2001, 250 : 642 - 649
  • [6] Wear of diffusion hardened Ti-6Al-4V sliding against alumina
    Stratton, P. F.
    Graf, M.
    [J]. HTM-JOURNAL OF HEAT TREATMENT AND MATERIALS, 2009, 64 (06): : 364 - 369
  • [7] Fretting Wear Behavior of Laser Peened Ti-6Al-4V
    Kumar, S. Anand
    Sundar, R.
    Raman, S. Ganesh Sundara
    Kumar, H.
    Gnanamoorthy, R.
    Kaul, R.
    Ranganathan, K.
    Oak, S. M.
    Kukreja, L. M.
    [J]. TRIBOLOGY TRANSACTIONS, 2012, 55 (05) : 615 - 623
  • [8] Oscillating and unidirectional sliding wear behaviour of cold sprayed Ti-6Al-4V coating on Ti-6Al-4V substrate
    Sirvent, P.
    Garrido, M. A.
    Lozano-Perez, S.
    Poza, P.
    [J]. SURFACE & COATINGS TECHNOLOGY, 2020, 382
  • [9] Crystallographic plasticity in fretting of Ti-6AL-4V
    Goh, CH
    Neu, RW
    McDowell, DL
    [J]. INTERNATIONAL JOURNAL OF PLASTICITY, 2003, 19 (10) : 1627 - 1650
  • [10] Friction and wear behaviour of carbon nitride films deposited on plasma nitrided Ti-6Al-4V
    Fu, YQ
    Loh, NL
    Wei, J
    Yan, BB
    Hing, P
    [J]. WEAR, 2000, 237 (01) : 12 - 19