Hydrocracking; XAFS; XANES; HRTEM; In situ sulfidation; Nickel-tungsten sulfide; THIOPHENE HYDRODESULFURIZATION ACTIVITY; HYDROTREATING CATALYSTS; ELECTRON-MICROSCOPY; SULFIDED W/AL2O3; CHELATING-AGENTS; SULFIDATION; NICKEL; TUNGSTEN; HYDROGENATION; FLUORINE;
D O I
10.1016/j.jcat.2009.01.019
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The detailed structural characterization of the metal function of two fully formulated Ni-W hydrocracking catalysts was investigated by time resolved in situ X-ray absorption spectroscopy (EXAFS and XANES) at both the Ni K-edge and W L-3-edge, and by high resolution transmission electron microscopy. These two hydrocracking catalysts (designated as HCA and HCB) contained the same wt% of Ni and W, the same wt% of the other constituents (gamma-Al2O3/silico-aluminate), and were calcined at the same temperature, but were prepared by different methods in order to highlight the sensitivity of the characterization techniques to the structural differences. The morphology of the WS2 particles in the sulfided catalyst is substantially different between the two catalysts: in the HCA catalyst there are many more particles with Multiple WS2 layers whereas in HCB there are more single layers. The average diameter of the WS2 plates is similar in both. The catalysts show a difference in the amount of W sulfidation after the 410 degrees C sulfidation treatment in 10% H2S/H-2. The W of HCA catalyst was completely sulfided whereas 16% W of HCB catalyst was unsulfided. Similarly there is a difference in the amount of sulfided Ni: 16% Ni in HCA and 60% Ni in HCB remain unsulfided. In the sulfided form of both catalysts the Ni exists in three different morphologies: oxidized Ni (six-fold coordinate as a nickel aluminate), nanoparticulate Ni3S2, and Ni decorating the edge sites of the WS2. In both the Ni3S2, and Ni decorating the edge sites of the WS2, the Ni is in a tetrahedral coordination with sulfur. In both catalysts the sulfidation of the Ni and W occurs essentially simultaneously over most of the temperature range and the sulfidation of the W proceeds through the same tungsten oxysulfide in both samples. The characterization methodology presented here is a powerful one for elucidating the structural differences of complex heterogeneous catalysts. (C) 2009 UOP LLC. Published by Elsevier Inc. All rights reserved.
引用
收藏
页码:16 / 33
页数:18
相关论文
共 50 条
  • [1] In situ XAS of Ni-W hydrocracking catalysts
    Yang, N.
    Mickelson, G. E.
    Greenlay, N.
    Kelly, S. D.
    Bare, Simon R.
    X-RAY ABSORPTION FINE STRUCTURE-XAFS13, 2007, 882 : 663 - +
  • [2] REDUCIBILITY OF NI-W HYDROCRACKING CATALYSTS
    MEYERS, BL
    MIEVILLE, RL
    APPLIED CATALYSIS, 1985, 14 (1-3): : 207 - 213
  • [3] HYDROCRACKING VACUUM RESIDUE WITH NI-W BIFUNCTIONAL SLURRY CATALYSTS
    RANKEL, LA
    FUEL PROCESSING TECHNOLOGY, 1994, 37 (02) : 185 - 202
  • [4] AN EXAFS STUDY ON THE NI AND W-ENVIRONMENT IN CARBON-SUPPORTED, SULFIDED W AND NI-W CATALYSTS
    LOUWERS, SPA
    PRINS, R
    JOURNAL OF CATALYSIS, 1993, 139 (02) : 525 - 539
  • [5] Ni-W/nano zeolite Y catalysts for n-heptane hydrocracking
    Anis, Shaheen Fatima
    Singaravel, Gnanapragasam
    Hashaikeh, Raed
    MATERIALS CHEMISTRY AND PHYSICS, 2018, 212 : 87 - 94
  • [6] In Situ Generated Nanosized Sulfide Ni-W Catalysts Based on Zeolite for the Hydrocracking of the Pyrolysis Fuel Oil into the BTX Fraction
    Kuchinskaya, Tatiana
    Kniazeva, Mariia
    Samoilov, Vadim
    Maximov, Anton
    CATALYSTS, 2020, 10 (10) : 1 - 19
  • [7] Application of Zeolite Y-Based Ni-W Supported and In Situ Prepared Catalysts in the Process of Vacuum Gas Oil Hydrocracking
    Onishchenko, M. I.
    Kulikov, A. B.
    Maksimov, A. L.
    PETROLEUM CHEMISTRY, 2017, 57 (14) : 1287 - 1294
  • [8] Towards understanding the microstructures and hydrocracking performance of sulfided Ni-W catalysts: Effect of metal loading
    Cui, Guoqi
    Wang, Jifeng
    Fan, Hongfei
    Sun, Xiaoyan
    Jiang, Yan
    Wang, Shaojun
    Liu, Dan
    Gui, Jianzhou
    FUEL PROCESSING TECHNOLOGY, 2011, 92 (12) : 2320 - 2327
  • [9] Structural, Compositional and Corrosion Characterization of Ni-W Thin Films
    Singh, Ajay Kumar
    Saini, Himanshu
    Khatri, Manvendra Singh
    PROTECTION OF METALS AND PHYSICAL CHEMISTRY OF SURFACES, 2024, 60 (05) : 970 - 980
  • [10] STUDY OF NI-W CATALYSTS DURING HYDROGENATION
    SHVETS, IS
    SOKOLSKI.DV
    POPOV, NI
    BIZHANOV, FB
    ZHURNAL PRIKLADNOI KHIMII, 1973, 46 (04) : 804 - 807