Oxygen ion conduction in 12CaO•7Al2O3: O2- conduction mechanism and possibility of O- fast conduction

被引:55
|
作者
Hosono, Hideo [1 ,2 ,3 ]
Hayashi, Katsuro [2 ]
Kajihara, Koichi [3 ,4 ]
Sushko, Peter V. [5 ]
Shluger, Alexander L. [5 ]
机构
[1] Tokyo Inst Technol, Frontier Res Ctr, Midori Ku, Yokohama, Kanagawa 2268503, Japan
[2] Tokyo Inst Technol, Mat & Struct Lab, Midori Ku, Yokohama, Kanagawa 2268503, Japan
[3] Tokyo Inst Technol, Transparent Electroact Mat Project, ERATO SORST, Frontier Res Ctr,Midori Ku, Yokohama, Kanagawa 2268503, Japan
[4] Tokyo Metropolitan Univ, Dept Appl Chem, Grad Sch Urban Environm Sci, Hachioji, Tokyo 1920397, Japan
[5] UCL, Dept Phys & Astron, London Ctr Nanotechnol, Mat Simulat Lab, London WC1E 6BT, England
关键词
Oxide ion conduction; Calcium aluminates; Mechanism; Fast oxide ion conduction; OXIDE; DIFFUSION; RADICALS;
D O I
10.1016/j.ssi.2008.10.015
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
12CaO center dot 7Al(2)O(3) (C12A7) with a unique nano-porous structure and free O2- ions entrapped in sub-nanometer-sized cages is a fast oxygen-ion-conducting material. These free O2- may be replaced by various oxygen-related species, OH-, O2- and O-, by tuning the atmosphere during the heat treatment. We examined the conduction mechanism for stoichiometric C12A7 (C12A7: O2-). in which O2- ions exist as counter anions in sub-nanometer-sized cages, by Raman measurement of C12A7:O2- annealed in a dry O-18(2) atmosphere. It was revealed that the primary ion conducting species is an O2- ion which diffuses via exchange with O2- in the cage wall. An experimental result on the sample containing O- ions implied that O- is more mobile than O2- in C12A7. Ab initio calculations on the diffusion paths of O2- and O- ions in C112A7 supported the above experimental results. (C) 2008 Elsevier B.V. All rights reserved
引用
收藏
页码:550 / 555
页数:6
相关论文
共 50 条
  • [1] Maximum incorporation of oxygen radicals, O- and O2-, into 12CaO•7Al2O3 with a nanoporous structure
    Hayashi, K
    Matsuishi, S
    Ueda, N
    Hirano, M
    Hosono, H
    CHEMISTRY OF MATERIALS, 2003, 15 (09) : 1851 - 1854
  • [2] Disorder of O2- ion and incorporation of O- and O2- radicals in nanoporous crystal 12CaO•7Al2O3 studied by low-temperature heat capacity measurements
    Kohama, Y
    Tojo, T
    Kawaji, H
    Atake, T
    Matsuishi, S
    Hosono, H
    CHEMICAL PHYSICS LETTERS, 2006, 421 (4-6) : 558 - 561
  • [3] Microporous crystal 12CaO•7Al2O3 encaging abundant O- radicals
    Hayashi, K
    Hirano, M
    Matsuishi, S
    Hosono, H
    JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 2002, 124 (05) : 738 - 739
  • [4] Intrinsic excitons in 12CaO•7Al2O3
    Feldbach, E.
    Denks, V. P.
    Kirm, M.
    Kunnus, K.
    Maaroos, A.
    RADIATION MEASUREMENTS, 2010, 45 (3-6) : 281 - 283
  • [5] Absolute emission current density of O- from 12CaO•7Al2O3 crystal
    Li, QX
    Hayashi, K
    Nishioka, M
    Kashiwagi, H
    Hirano, M
    Torimoto, Y
    Hosono, H
    Sadakata, M
    APPLIED PHYSICS LETTERS, 2002, 80 (22) : 4259 - 4261
  • [6] VUV and cathodoluminescence spectroscopy of 12CaO · 7Al2O3
    Eduard Feldbach
    Viktor P. Denks
    Marco Kirm
    Peeter Liblik
    Aarne Maaroos
    Hugo Mändar
    Tea Avarmaa
    Kristjan Kunnus
    Journal of Materials Science: Materials in Electronics, 2009, 20 : 260 - 263
  • [7] Czochralski growth of 12CaO, 7Al2O3 crystals
    Kurashige, K
    Toda, Y
    Matstuishi, S
    Hayashi, K
    Hirano, M
    Hosono, H
    CRYSTAL GROWTH & DESIGN, 2006, 6 (07) : 1602 - 1605
  • [8] Excess oxygen in 12CaO•7Al2O3 studied by thermogravimetric analysis
    Hayashi, K
    Hirano, M
    Hosono, H
    CHEMISTRY LETTERS, 2005, 34 (04) : 586 - 587
  • [9] Heavy doping of H- ion in 12CaO • 7Al2O3
    Hayashi, Katsuro
    JOURNAL OF SOLID STATE CHEMISTRY, 2011, 184 (06) : 1428 - 1432
  • [10] XPS and NMR analysis on 12CaO•7Al2O3
    Pan, R. K.
    Feng, S.
    Tao, H. Z.
    1ST INTERNATIONAL CONFERENCE ON NEW MATERIAL AND CHEMICAL INDUSTRY (NMCI2016), 2017, 167