Shrinkage behavior of high performance concrete at different elevated temperatures under different sealing conditions

被引:3
|
作者
Pan Zhihua [1 ]
Hidemi, Nakamura
Tionghuan, Wee
机构
[1] Nanjing Univ Technol, Coll Mat Sci & Engn, Nanjing 210009, Peoples R China
[2] Taiheiyo Cement Corp, Ctr Res & Dev, Chiba 2858655, Japan
[3] Natl Univ Singapore, Dept Civil Engn, Singapore 117548, Singapore
关键词
high performance concrete; shrinkage; granulated blast-furnace slag; fly ash; elevated temperature; sealing condition;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The shrinkage behavior of high performance cement concrete made from Portland cement, ultra fine granulated blast furnace slag and pulverized fly ash with addition of superplasticizer at, different temperatures from ambient temperature to 120 degrees C under different sealing conditions was investigated by means of length change measurement on cylindrical concrete specimens along with curing age. Results show that drying shrinkage deformations of titled concrete specimens increased rapidly as the curing temperature rose. The development of drying shrinkage deformation can be efficiently controlled with the aid of aluminum tape sealing as compared with the unsealed specimens, especially when the curing temperature is below 60 degrees C, although it will increase dramatically when the curing temperature is elevated to above 90 degrees C. Polymer coating on concrete specimens showed a similar effect on the control of drying shrinkage as the sealing operation with aluminum tape.
引用
收藏
页码:138 / 141
页数:4
相关论文
共 50 条
  • [1] Shrinkage Behavior of High Performance Concrete at Different Elevated Temperatures under Different Sealing Conditions
    潘志华
    NAKAMURA Hidemi
    WEE Tionghuan
    [J]. Journal of Wuhan University of Technology(Materials Science), 2006, (03) : 138 - 141
  • [2] Shrinkage behavior of high performance concrete at different elevated temperatures under different sealing conditions
    Pan Z.
    Nakamura H.
    Wee T.
    [J]. Journal of Wuhan University of Technology-Mater. Sci. Ed., 2006, 21 (3): : 138 - 141
  • [3] Autogenous shrinkage of high performance concrete containing mineral admixtures under different curing temperatures
    Jiang, Chenhui
    Yang, Yang
    Wang, Yong
    Zhou, Yuenian
    Ma, Chengchang
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2014, 61 : 260 - 269
  • [4] High performance concrete under elevated temperatures
    Akca, Abdullah Huzeyfe
    Zihnioglu, Nilufer Ozyurt
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2013, 44 : 317 - 328
  • [5] Performance of Different Concrete Types Exposed to Elevated Temperatures: A Review
    Alhamad, Amjad
    Yehia, Sherif
    Lubloy, Eva
    Elchalakani, Mohamed
    [J]. MATERIALS, 2022, 15 (14)
  • [6] Flexural Properties of Ultra-high Performance Concrete Under Different Temperatures
    Fang, Zhi
    Liu, Shaokun
    Huang, Zhengyu
    Chen, Junting
    [J]. Kuei Suan Jen Hsueh Pao/Journal of the Chinese Ceramic Society, 2020, 48 (11): : 1732 - 1739
  • [7] Performance of steel fiber reinforced concrete colu mns exposed to high temperatures under different cooling conditions
    Reddy, K. Ratna Tej
    Rao, K. Srinivasa
    Rambabu, K.
    [J]. Indian Concrete Journal, 2019, 93 (08): : 32 - 42
  • [8] Influence of Different Curing Conditions on Shrinkage of Concrete
    Chen, Jing
    Li, Xiaohuan
    Wang, Fengling
    Xu, Fenlian
    [J]. CIVIL, STRUCTURAL AND ENVIRONMENTAL ENGINEERING, PTS 1-4, 2014, 838-841 : 36 - 41
  • [9] Restrained Shrinkage Behavior in Ring Test of Ultra High Performance Concrete with Different Tensile Properties
    Wang, Jun-Yan
    Bian, Chen
    Xiao, Ru-Cheng
    Ma, Biao
    [J]. Zhongguo Gonglu Xuebao/China Journal of Highway and Transport, 2019, 32 (09): : 115 - 123
  • [10] Investigation of the effect of different curing conditions on the mechanical performance of calcium aluminate cement concrete at elevated temperatures
    Gulec, Abdulkadir
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2023, 409