Hydrogen embrittlement of catholically hydrogen-precharged 304L austenitic stainless steel: Effect of plastic pre-strain

被引:98
|
作者
Wang, Yanfei [1 ]
Wang, Xiaowei [1 ]
Gong, Jianming [1 ]
Shen, Limin [2 ]
Dong, Weinan [1 ]
机构
[1] Nanjing Univ Technol, Coll Mech & Power Engn, Nanjing 211816, Jiangsu, Peoples R China
[2] China Univ Min & Technol, Coll Chem Engn & Technol, Xuzhou 221116, Peoples R China
关键词
Hydrogen embrittlement; Pre-strain; Austenitic stainless steel; Cold working; FATIGUE-CRACK GROWTH; INDUCED MARTENSITE; LOW-TEMPERATURES; ENVIRONMENT EMBRITTLEMENT; MECHANICAL-PROPERTIES; DEFORMATION; TRANSFORMATION; ALLOYS; PERMEATION; BEHAVIOR;
D O I
10.1016/j.ijhydene.2014.04.122
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Prior plastic deformation introduced by fabrication process such as cold working is an important factor for hydrogen embrittlement (HE) of austenitic stainless steels. In order to clarify the relationship between HE susceptibility of type 304L stainless steel and prior tensile plastic deformation, a group of flat specimens with different degrees of pre-strain (0 i.e. without pre-strain, 3, 6, 10, 15, 20 and 25% true strain) was catholically hydrogen charged and then was strained immediately to fracture by means of tensile testing. The resulting tensile properties and fracture morphologies were compared with those of a second reference group of specimens without charging. The results reveal a detrimental effect of high degrees of pre-strain on HE of the steel. When the pre-strain was less than 6%, the effect of pre-strain on HE of the steel was minor. While when the pre-strain was higher than 10%, the pre-strain greatly enhanced HE of the steel. This occurrence could be attributed to strain-induced alpha' martensite transformation during pre-straining. The higher the pre-strain, the higher the content of alpha' martensite transformed and so the HE occurred. Fracture morphology investigations suggest that the pre-strain-induced alpha' martensite greatly enhanced the hydrogen diffusivity, and the mode of brittle fracture due to hydrogen strongly depended on the pre-strain level. Copyright (C) 2014, Hydrogen Energy Publications, LLC. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:13909 / 13918
页数:10
相关论文
共 50 条
  • [1] Warm Pre-Strain: Strengthening the Metastable 304L Austenitic Stainless Steel without Compromising Its Hydrogen Embrittlement Resistance
    Wang, Yanfei
    Zhou, Zhiling
    Wu, Weijie
    Gong, Jianming
    [J]. MATERIALS, 2017, 10 (11):
  • [2] The Effect of Pre-Strain on the Resistance to Hydrogen Embrittlement in 316L Austenitic Stainless Steel
    Park, Il-Jeong
    Jung, Jae-Gil
    Jo, Seo Yeon
    Lee, Sang-Min
    Lee, Young-Kook
    [J]. MATERIALS TRANSACTIONS, 2014, 55 (06) : 964 - 970
  • [3] Anisotropic effect of pre-strain on hydrogen embrittlement susceptibility in a stable austenitic stainless steel
    Cho, Hyung-Jun
    Park, Jinheung
    Cho, Yeonggeun
    Kim, Kyung-Shik
    Lee, Myoung-Gyu
    Kim, Sung-Joon
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2023, 887
  • [4] Effect of pre-strain on hydrogen embrittlement of metastable austenitic stainless steel under different hydrogen conditions
    Zhou, Chengshuang
    Song, Yangyang
    Shi, Qiaoying
    Hu, Shiyin
    Zheng, Jinyang
    Xu, Peng
    Zhang, Lin
    [J]. INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2019, 44 (47) : 26036 - 26048
  • [5] Effect of α′ Martensite Content Induced by Tensile Plastic Prestrain on Hydrogen Transport and Hydrogen Embrittlement of 304L Austenitic Stainless Steel
    Wang, Yanfei
    Wu, Xuanpei
    Wu, Weijie
    [J]. METALS, 2018, 8 (09):
  • [6] HYDROGEN EMBRITTLEMENT OF TYPE 304L STAINLESS STEEL
    HOLZWORTH, ML
    [J]. CORROSION, 1969, 25 (03) : 107 - +
  • [7] Effect of pre-strain on hydrogen induced cracking of PAW welded 304 austenitic stainless steel
    Zhou, Chilou
    Ren, Yingjie
    Yokogawa, Kiyoshi
    Xue, Jinxin
    Li, Xiang
    [J]. INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2024, 54 : 713 - 728
  • [8] Hydrogen effect on nitriding process of 304L austenitic stainless steel
    Garamoon, A.
    Rashed, U. M.
    Abouelela, A.
    Eissa, M. A.
    Saudi, A. H.
    El-zeer, D. M.
    El-Hossary, F.
    [J]. IEEE TRANSACTIONS ON PLASMA SCIENCE, 2006, 34 (04) : 1066 - 1073
  • [9] Effect of pre-strain on microstructure and hydrogen embrittlement of K-TIG welded austenitic stainless steel
    Li, Xiaogang
    Gong, Baoming
    Deng, Caiyan
    Li, Yizhe
    [J]. CORROSION SCIENCE, 2019, 149 : 1 - 17
  • [10] The effect of pre-strain on hydrogen embrittlement in 310S stainless steel
    Ji, Hyunju
    Park, Il-Jeong
    Lee, Sang-Min
    Lee, Young-Kook
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 598 : 205 - 212