Development and testing of a high-chromium, Ni-based filler metal resistant to ductility dip cracking and solidification cracking

被引:17
|
作者
Hope, Adam T. [1 ]
Lippold, John C. [1 ]
机构
[1] Ohio State Univ, Dept Mat Sci & Engn, Welding Engn Program, 116 W 19Th Ave, Columbus, OH 43210 USA
关键词
Nickel alloys; Fillermaterials; Hot cracking; Solidification cracking; Eutectics; CR-HF SYSTEM;
D O I
10.1007/s40194-016-0417-6
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Ni-based filler metals for repair and construction of nuclear reactor components require 30 wt% Cr to insure resistance to primary water stress corrosion cracking (PWSCC). Current generation alloys can be susceptible to solidification cracking and ductility dip cracking, depending on Nb content and the amount of eutectic that forms during weld solidification. Computational thermodynamic modeling was used to identify alternative eutectic-forming elements to Nb, such as Hf and Ta. Previous work has utilized a design of experiment methodology (DOE) in conjunction with computational and experimental techniques to optimize a new filler metal composition that should be resistant to weld cracking. In this paper, the optimized compositions were subjected to further weldability testing, namely the cast pin tear test (CPTT) and the strain-to-fracture (STF) test. An optimized Ta-bearing compositionwas found to be crack resistant, while an optimized Hf-bearing composition was highly susceptible to solidification cracking. Differences may be related to the nature of the eutectic constituents that form at the end of solidification. The Hf-bearing composition did not form Laves phase as its final eutectic constituent, while Laves is present in both the Nb- and Ta-bearing systems.
引用
收藏
页码:325 / 332
页数:8
相关论文
共 50 条
  • [1] Development and testing of a high-chromium, Ni-based filler metal resistant to ductility dip cracking and solidification cracking
    Adam T. Hope
    John C. Lippold
    Welding in the World, 2017, 61 : 325 - 332
  • [2] Ductility-Dip Cracking in High Chromium, Ni-Base Filler Metals
    Lippold, J. C.
    Nissley, N. E.
    HOT CRACKING PHENOMENA IN WELDS II, 2008, : 409 - +
  • [3] Further investigations of ductility-DIP cracking in high chromium, NI-base filler metals
    Lippold J.C.
    Nissley N.E.
    Welding in the World, 2007, 51 (9-10) : 24 - 30
  • [4] A STUDY OF DUCTILITY DIP CRACKING OF INCONEL 690 WELDING FILLER METAL - DEVELOPMENT OF A REFUSION CRACKING TEST
    Rapetti, Abel
    Todeschini, Patrick
    Hendili, Sofiane
    Christien, Frederic
    Tancret, Franck
    PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE, 2017, VOL 6B, 2017,
  • [5] Effect of Welding Parameters on the Liquation Cracking Behavior of High-Chromium Ni-Based Superalloy
    Mashhuriazar, Amirhossein
    Omidvar, Hamid
    Gur, C. Hakan
    Sajuri, Zainuddin
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2020, 29 (12) : 7843 - 7852
  • [6] Effect of Welding Parameters on the Liquation Cracking Behavior of High-Chromium Ni-Based Superalloy
    Amirhossein Mashhuriazar
    Hamid Omidvar
    C. Hakan Gur
    Zainuddin Sajuri
    Journal of Materials Engineering and Performance, 2020, 29 : 7843 - 7852
  • [7] Metallurgical Investigation into Ductility Dip Cracking in Ni-Based Alloys: Part II
    Noecker, F. F., II
    DuPont, J. N.
    WELDING JOURNAL, 2009, 88 (03) : 62S - 77S
  • [8] Surfactant effect of impurity sulphur in ductility dip cracking of a high-chromium nickel model alloy
    Rapetti, A.
    Christien, F.
    Tancret, F.
    Todeschini, P.
    Hendili, S.
    Stodolna, J.
    SCRIPTA MATERIALIA, 2021, 194
  • [9] Metallurgical Investigation into Ductility Dip Cracking in Ni-Based Alloys: Part I
    Noecker, F. F., II
    DuPont, J. N.
    WELDING JOURNAL, 2009, 88 (01) : 7S - 20S
  • [10] Influence of grain boundary sliding on ductility-dip cracking of Ni-based alloy
    Lu, H. (luhao@sjtu.edu.cn), 1600, Central South University of Technology (23):