The effect of the deposition sequence of sol-gel SiO2-Al2O3, CeO2 and Y2O3 coatings on the corrosion resistance of the FeCrAl alloy during cyclic high-temperature oxidation

被引:6
|
作者
Checmanowski, Jacek G. [1 ]
Szczygiel, Bogdan [1 ]
机构
[1] Wroclaw Univ Technol, Fac Chem, Dept Adv Mat Technol, Wybrzeze Wyspianskiego 27, PL-50370 Wroclaw, Poland
来源
关键词
Thin films; Coating materials; High-temperature alloys; Sol-gel process; Corrosion; SEM; FE-CR-AL; REACTIVE ELEMENT; ALPHA-AL2O3; SCALES; CERIUM ADDITION; BEHAVIOR; MORPHOLOGY; GROWTH; IMPROVEMENT; STRESSES;
D O I
10.1016/j.surfcoat.2018.03.063
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The surface of a ferritic FeCrAl alloy was covered with three-layer ceramic coatings by the sol-gel method. The SiO2-Al2O3, Y2O3 and CeO2 layers would be deposited in different sequences. The obtained material would be subjected to cyclic oxidation at a temperature of 900 degrees C. It was found that the sequence in which the layers are deposited affects the morphology and chemical composition of the scale. After 20 oxidation cycles (each lasting 12 h) the thickness of the building up oxide film amounted to 2.3-4.2 mu m. Gravimetric analyses showed the parabolic character of the weight gain-oxidation time interdependence. The first layer deposited on the metallic surface determines the distribution of yttrium and cerium in the scale and in the alloy core. The scale building up on the samples in which yttrium oxide formed the first layer was found to have the most advantageous protective properties. After 20 oxidation cycles the FeCrAl alloy coated in turn with the layers: Y2O3, CeO2 and SiO2-Al2O3 showed the smallest relative change in weight. In comparison with the uncoated substrate the protection effectiveness of the deposited coatings amounts to 12-37%.
引用
收藏
页码:458 / 466
页数:9
相关论文
共 50 条
  • [1] High temperature oxidation resistance of FeCrAl alloys covered with ceramic SiO2-Al2O3 coatings deposited by sol-gel method
    Checmanowski, J. G.
    Szczygiel, B.
    CORROSION SCIENCE, 2008, 50 (12) : 3581 - 3589
  • [2] Influence of ceria and yttria on the protective properties of SiO2-Al2O3 coatings deposited by sol-gel method on FeCrAl alloy
    Checmanowski, Jacek
    Pelczarska, Aleksandra J.
    Szczygiel, Irena
    Szczygiel, Bogdan
    JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2016, 126 (02) : 371 - 380
  • [3] High-temperature oxidation resistance of sol–gel-derived ZrO2/(Al2O3–Y2O3) coating on titanium alloy
    Y. B. Yao
    Z. J. Yao
    Y. J. Zhou
    Journal of Sol-Gel Science and Technology, 2016, 80 : 612 - 618
  • [4] Effect of Adding SiO2-Al2O3 Sol into Anodizing Bath on Corrosion Resistance of Oxidation Film on Magnesium Alloy
    Liu, Huicong
    Zhu, Liqun
    Li, Weiping
    MAGNESIUM TECHNOLOGY 2011, 2011, : 623 - 627
  • [5] Improvement of Oxidation Resistance of Mild Steel by SiO2-Al2O3 Sol Gel Coating
    Kirtay, S.
    ACTA PHYSICA POLONICA A, 2015, 128 (2B) : B90 - B92
  • [6] High-temperature oxidation resistance of sol-gel-derived ZrO2/(Al2O3-Y2O3) coating on titanium alloy
    Yao, Y. B.
    Yao, Z. J.
    Zhou, Y. J.
    JOURNAL OF SOL-GEL SCIENCE AND TECHNOLOGY, 2016, 80 (03) : 612 - 618
  • [7] Anticorrosion Performance of Sol-Gel Driven SIO2-Al2O3 Coatings on Low Carbon Steel
    Seo, Bosung
    Kang, Jangwon
    Won, Sori
    Park, Jong Min
    Kim, Hyo Kyu
    Park, Kwangsuk
    PROTECTION OF METALS AND PHYSICAL CHEMISTRY OF SURFACES, 2019, 55 (03) : 539 - 545
  • [8] Sol-Gel Synthesis of Functionally Different Materials in the System Y2O3–Al2O3–SiO2
    Yu. E. Lebedeva
    N. V. Popovich
    L. A. Orlova
    A. S. Chainikova
    Glass and Ceramics, 2015, 71 : 400 - 404
  • [9] Electrical Properties of Nanocrystalline CeO2–Y2O3 Thin Films Prepared by the Sol-Gel Method
    H. M. Yue
    Z. L. Liu
    Y. Wang
    K. L. Yao
    Inorganic Materials, 2003, 39 : 720 - 724
  • [10] PROPERTIES OF RH-EXCHANGED SIO2-AL2O3 SOL-GEL CATALYSTS
    SERMON, PA
    WALTON, TJ
    LUENGO, MAM
    VONG, MSW
    JOURNAL OF THE CHEMICAL SOCIETY-FARADAY TRANSACTIONS, 1991, 87 (01): : 199 - 202