The mechanism of oxidation of sputtered Ni-Cr-Al nanocrystalline coatings

被引:0
|
作者
Chen, GF [1 ]
Lou, HY [1 ]
机构
[1] Acad Sinica, State Key Lab Corros & Protect Met, Shenyang 110015, Peoples R China
来源
CORROSION REVIEWS | 2000年 / 18卷 / 2-3期
关键词
nanocrystalline coatings; sputtering; Ni-Cr-Al; oxidation;
D O I
暂无
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Complex layered oxide scales composed of a complete inner layer of alpha-Al2O3 were formed on the formerly Cr203-forming alloy Ni-8Cr-3.5Al (wt%) and the NiO-forming alloy Ni-5Cr-5Al (at%) through nanocrystallization. Due to the formation of the inner layer of alpha-Al2O3, Ni-8Cr-3.5Al (wt%) and Ni-5Cr-5Al (at%) alloys with nano-sized grain were all Al2O3-formers. The results indicated that the oxide types of Ni-Cr-Al alloys could be altered through nanocrystallization. In this paper, the mechanism of oxidation for two Al2O3-forming sputtered Ni-8Cr-3.5Al (wt%) and Ni-5Cr-5Al (at%) nanocrystalline coatings on the substrates of the same alloys was proposed based upon the interaction of Cr and Al during oxidation process.
引用
收藏
页码:195 / 204
页数:10
相关论文
共 50 条
  • [1] Oxidation behaviour of microcrystalline Ni-Cr-Al alloy coatings at 900°C
    Liu, ZY
    Gao, W
    [J]. SCRIPTA MATERIALIA, 1998, 38 (06) : 877 - 885
  • [2] Oxidation behavior of sputtered Ni-Cr-Al-Ti nanocrystalline coating
    Chen, G
    Lou, H
    [J]. SURFACE & COATINGS TECHNOLOGY, 2000, 123 (01): : 92 - 96
  • [3] Synthesis and Characterization of Nanocrystalline Ni-Cr-Al Alloy Powder
    Singh, Daljeet
    Kumar, Rajiv
    [J]. MATERIALS TODAY-PROCEEDINGS, 2021, 41 : 821 - 824
  • [4] MODELING DEGRADATION AND FAILURE OF NI-CR-AL OVERLAY COATINGS
    NESBITT, JA
    HECKEL, RW
    [J]. THIN SOLID FILMS, 1984, 119 (03) : 281 - 290
  • [5] Oxidation and Compressive Properties of Ni-Cr, Ni-Al, and Ni-Cr-Al Foams
    Choe, H.
    Dunand, D. C.
    [J]. POROUS METALS AND METALLIC FOAMS: METFOAM 2007, 2008, : 141 - +
  • [6] Oxidation resistance of sputtered Ni-5Cr-5Al nanocrystalline coating
    Chen, Guo-feng
    Lou, Han-yi
    [J]. Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 2000, 10 (02): : 175 - 178
  • [7] Oxidation behavior of a sputtered Ni-5Cr-5Al nanocrystalline coating
    Chen, GF
    Lou, HY
    [J]. OXIDATION OF METALS, 2000, 53 (5-6): : 467 - 479
  • [8] Oxidation behaviour of sputter-deposited Ni-Cr-Al micro-crystalline coatings
    Univ of Auckland, Auckland, New Zealand
    [J]. Acta Mater, 5 (1691-1700):
  • [9] Oxidation behaviour of sputter-deposited Ni-Cr-Al micro-crystalline coatings
    Liu, ZY
    Gao, W
    Dahm, KL
    Wang, FH
    [J]. ACTA MATERIALIA, 1998, 46 (05) : 1691 - 1700
  • [10] Oxidation behavior of sputtered Ni-3Cr-20Al nanocrystalline coating
    Chen, GF
    Lou, HY
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1999, 271 (1-2): : 360 - 365