共 50 条
- [2] Effect of temperature and pre-sintering on phase transformation, texture and mechanical properties of silicon nitride ceramics [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 731 : 140 - 148
- [4] Improvement of creep rupture life in magnesium-aluminum by high temperature pre-creep binary solid solutions [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2001, 319 : 746 - 750
- [5] Creep behavior of NiTi shape memory alloys and the effect of pre-creep on the martensitic phase transformation [J]. SHAPE MEMORY MATERIALS, 2000, 327-3 : 183 - 186
- [6] THE PREVENTION ROLE OF PRE-CREEP ON STRESS CORROSION CRACKING [J]. Science Bulletin, 1992, (23) : 2018 - 2020
- [8] Effect of the mechanical properties of silicon nitride by coated zirconia [J]. Rengong Jingti Xuebao/Journal of Synthetic Crystals, 2015, 44 (11): : 3260 - 3264
- [9] EFFECT OF PRE-CREEP ON THE SUCCEEDING CREEP-BEHAVIOR OF A 2.25CR-1MO STEEL [J]. SCRIPTA METALLURGICA ET MATERIALIA, 1993, 29 (05): : 643 - 646
- [10] Mechanical properties of magnesium silicon nitride - Silicon nitride ceramics [J]. SILICATES INDUSTRIELS, 2004, 69 (7-8): : 275 - 280