Long-term aging characteristics of co-filled nano-silica and micro-ATH in HTV silicone rubber composite insulators

被引:4
|
作者
Rashid, Arooj [1 ]
Saleem, Jawad [1 ]
Amin, Muhammad [2 ]
Ali, Sahibzada Muhammad [1 ]
机构
[1] COMSATS Univ Islamabad, Dept Elect Engn, Abbottabad Campus, Abbottabad 22010, Pakistan
[2] Ghulam Ishaq Inst Sci & Technol, Dept Elect Engn, Swabi, Pakistan
来源
POLYMERS & POLYMER COMPOSITES | 2021年 / 29卷 / 01期
关键词
Leakage current; FTIR; hydrophobicity; breakdown strength; aging characteristics;
D O I
10.1177/0967391120901421
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Multiple environmental stresses produce complex phenomena of aging in polymeric insulators. The main aim of this research is to investigate the improved aging characteristics of silica (SiO2)/alumina trihydrate (ATH) hybrid samples (HSs) in high-temperature vulcanized rubber. For this purpose, three HSs comprising 20% micro-ATH with 2% nano-SiO2 (S2), 4% nano-SiO2 (S4), 6% nano-SiO2 (S6) along with sample-virgin (SV) are subjected to long-term accelerated aging of 9000 h. A special aging chamber is fabricated for the aging process of samples. The aging characteristics of these samples are investigated by measuring leakage current (LC) and hydrophobicity classification (HC) after every weathering cycle. Similarly, Fourier transform infrared (FTIR) spectroscopy is performed to observe the important structural changes over the entire aging time. The dielectric strength of AC is also performed after every 1000 h of aging. Tracking and erosion resistance and mechanical properties are also investigated before and after aging. From the critical investigation, it is observed that HSs possess improved results in all the conducted tests. S2 has the lowest LC and HC values throughout the aging time. Similarly, S6 described the highest breakdown strength at the end of the accelerated aging. In the case of FTIR, it is analyzed that the important wave numbers remain intact for all the HSs in the accelerated aging environment. The loss percentage in the wave number for SV is higher, compared to the HSs. After performing the tracking and erosion resistance test, HSs have superior performance. For some of the mechanical properties, HSs showed improved values. Thus, from the experimental analysis, it is deducted that the sample S2 offers the highest resistance to the aging conditions, compared to the SV and other HSs.
引用
收藏
页码:40 / 56
页数:17
相关论文
共 18 条
  • [1] Comparative Properties of HTV Silicone Rubber for Composite Insulators - ATH and Silica Fillers
    Ilhan, S.
    Tuzun, D.
    Ozdemir, A.
    IEEE TRANSACTIONS ON DIELECTRICS AND ELECTRICAL INSULATION, 2021, 28 (02) : 414 - 422
  • [2] Resistance against AC Corona Discharge of Micro-ATH/Nano-Al2O3 Co-Filled Silicone Rubber Composites
    Nazir, M. Tariq
    Phung, B. T.
    Yu, Shihu
    Li, Shengtao
    IEEE TRANSACTIONS ON DIELECTRICS AND ELECTRICAL INSULATION, 2018, 25 (02) : 657 - 667
  • [3] Interpreting Surface Degradation of HTV Silicone Rubber Filled with Micro/Nano-Silica Under AC and DC Voltages
    Akbar, Muhammad
    Ullah, Rahmat
    Abdul Karim, M. R.
    JOURNAL OF ELECTRONIC MATERIALS, 2020, 49 (09) : 5399 - 5410
  • [4] Interpreting Surface Degradation of HTV Silicone Rubber Filled with Micro/Nano-Silica Under AC and DC Voltages
    Muhammad Akbar
    Rahmat Ullah
    M. R. Abdul Karim
    Journal of Electronic Materials, 2020, 49 : 5399 - 5410
  • [5] AC Corona Resistance of Micro-ATH/Nano-Al2O3 filled Silicone Rubber Composites
    Nazir, M. Tariq
    Phung, B. T.
    2016 IEEE INTERNATIONAL CONFERENCE ON HIGH VOLTAGE ENGINEERING AND APPLICATION (ICHVE), 2016,
  • [6] Multi-stress aging investigations of HTV silicone rubber filled with Silica/ATH composites for HVAC and HVDC transmission
    Akbar, Muhammad
    Ullah, Rahmat
    Qazi, Ibrahim
    ENGINEERING FAILURE ANALYSIS, 2020, 110 (110)
  • [7] Recovery and Preparation of Nano-silica by Pyrolysis From Waste Silicone Rubber Sheath of Composite Insulators
    Wang X.
    Cheng L.
    Liao R.
    Zhang S.
    Wang T.
    Gaodianya Jishu/High Voltage Engineering, 2021, 47 (01): : 269 - 278
  • [8] Aging mechanism of HTV silicone rubber loaded with hybrid nano/micro silica and alumina exposed to concurrent multistress
    Ullah, Rahmat
    Rahman, Rahisham Abd
    Ahmed, Rizwan
    Wali, Khan
    Ullah, Israr
    POLYMER TESTING, 2023, 121
  • [9] Nano and micro co-filled aluminum nitride/magnesium dihydrate-Silicone rubber composites for high voltage insulation
    Ashitha, Parambalath Narendran
    Shanker, Tangella Bhavani
    Meena, K. Parameswaran
    Varughese, Konnanilkunnathil Thomas
    JOURNAL OF APPLIED POLYMER SCIENCE, 2024, 141 (26)
  • [10] Measuring electrical, thermal and mechanical properties of DC-stressed HTV silicone rubber loaded with nano/micro-fillers exposed to long-term aging
    Ullah, Rahmat
    Akbar, Muhammad
    Amin, Salman
    APPLIED NANOSCIENCE, 2020, 10 (07) : 2101 - 2111