摘要
Ceramic thin films have been widely used to protect the metal substrate as coatings in the past years. In order to improve the poor corrosion resistance of AZ31 magnesium alloy, the study in this paper used the electron beam evaporation method to prepare ceramic PVD films on its surface with TiO2 and Al2O3 as donors, respectively. Atomic force microscopy (AFM), scanning electron microscope (SEM), energy dispersive X-ray spectrometer (EDS), Auger electron spectroscopy (AES) and Xray diffraction (XRD) were used to investigate the surface morphology, composition and microstructure of the thin films. Both films deposited on AZ31 took on compact top surface morphologies and grew as amorphous structures on substrate. AES test not only showed that films compositions deviated the standard stoichiometric ratios, but also found that element Mg diffused into films and existed as magnesium oxide in the TiOx film as well as the AlOx film. In the electrochemical corrosion test, the AlOx coating on AZ31 exhibited the largest electrochemical impedance in a 3.5 % NaCl solution. But it did not show better corrosion resistance than others for the poorer adhesion. Even if its thickness was small, the TiOx coating on AZ31 exhibited the best corrosion resistance in this study. According to the observation and analysis, the damage of these films on AZ31 in aggressive solutions was mainly due to the existence of pores, microcracks, vacancies and poor adhesion between coating and substrate. (c) 2005 Elsevier B.V. All rights reserved.
引用
收藏
页码:7422 / 7429
页数:8
相关论文
共 50 条
  • [1] Characterization and residual stress analysis of TiN/TiCN films on AZ31 magnesium alloy by PVD
    Li, Haitao
    Wang, Qiang
    Zhuang, Minghui
    Wu, Junjie
    [J]. VACUUM, 2015, 112 : 66 - 69
  • [2] Corrosion mechanism of PEO films on AZ31 magnesium alloys
    Wang, Li
    Fu, Wen
    Chen, Li
    [J]. ADVANCED BUILDING MATERIALS AND STRUCTURAL ENGINEERING, 2012, 461 : 220 - +
  • [3] Corrosion Characteristics of PEO Films on AZ31 Magnesium Alloys
    Wang, Li
    Chen, Li
    Fu, Wen
    [J]. MANUFACTURING PROCESS TECHNOLOGY, PTS 1-5, 2011, 189-193 : 256 - +
  • [4] Characterisation of TiAlN PVD coatings on AZ31 magnesium alloy
    Chen, Wei
    Huang, Jiamu
    Peng, Jia
    [J]. RESEARCH ON CHEMICAL INTERMEDIATES, 2015, 41 (03) : 1257 - 1266
  • [5] Characterisation of TiAlN PVD coatings on AZ31 magnesium alloy
    Wei Chen
    Jiamu Huang
    Jia Peng
    [J]. Research on Chemical Intermediates, 2015, 41 : 1257 - 1266
  • [6] Corrosion Resistance of Modified Silane Films Formed on AZ31 Magnesium Alloys
    Cao, Xianlong
    Pan, Fusheng
    Deng, Hongda
    Cai, Wei
    [J]. ADVANCED STRUCTURAL MATERIALS, 2011, 686 : 21 - +
  • [7] Characterization of anodic films on AZ31 magnesium alloys in alkaline solutions containing fluoride and phosphate anions
    Lin, C. S.
    Fu, Y. C.
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2006, 153 (10) : B417 - B424
  • [8] Residual Stresses in Microarc Oxidation Ceramic Coatings on Biocompatible AZ31 Magnesium Alloys
    Gu, Yanhong
    Xiong, Wenming
    Ning, Chengyun
    Zhang, Jing
    [J]. JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2012, 21 (06) : 1085 - 1090
  • [9] Characterization of Plasma Electrolytic Oxidation Films Formed on AZ31 Magnesium Alloys by Different Voltage Parameters
    Wang, Li
    Chen, Li
    Fu, Wen
    [J]. ADVANCES IN BUILDING MATERIALS, PTS 1-3, 2011, 168-170 : 1203 - +
  • [10] Residual Stresses in Microarc Oxidation Ceramic Coatings on Biocompatible AZ31 Magnesium Alloys
    Yanhong Gu
    Wenming Xiong
    Chengyun Ning
    Jing Zhang
    [J]. Journal of Materials Engineering and Performance, 2012, 21 : 1085 - 1090