The effect of in vitro modeling conditions on the surface reactions of bioactive glass

被引:0
|
作者
Radin, S
Ducheyne, P
Rothman, B
Conti, A
机构
[1] UNIV PENN, SCH ENGN & APPL SCI, DEPT BIOENGN, PHILADELPHIA, PA 19104 USA
[2] UNIV PENN, SCH MED, DEPT ORTHOPAED SURG, PHILADELPHIA, PA 19104 USA
[3] UNIV PENN, SCH ENGN & APPL SCI, DEPT MAT SCI & ENGN, PHILADELPHIA, PA 19104 USA
来源
关键词
bioactive glass; surface reactions; in vitro;
D O I
10.1002/(SICI)1097-4636(19971205)37:3<363::AID-JBM7>3.0.CO;2-J
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
Using one parametric variation in solution composition, this paper documents that the surface reactions on bioactive glass (BG) 45S5 are exquisitely dependent upon the modeling conditions. The solutions used were 0.05M tris hydroxymethyl aminomethane/HCl (tris buffer), tris buffer complemented with plasma electrolyte and/or serum, and serum. The reacted surfaces were analyzed using Fourier transform infrared (FTIR), scanning electron microscopy (SEM) with energy dispersive X-ray analysis (EDXA), and Rutherford backscattering spectroscopy (RBS). Post-immersion solutions were analyzed for changes in Ca and PO4 concentrations. After a short immersion (3 h), a crystalline, carbonated hydroxyapatite (c-HA) layer formed only in tris. Reaction surfaces of different structure, morphology, and composition were observed after various short and longer term immersions in all other solutions. They comprised two layers with the layer in contact with the bulk consisting mainly of Si; the outer layer, composed of Si, Ca, and P, was amorphous, and had a Ca/P ratio of about 1. Serum proteins adsorbed on the BG surfaces at the early stages of the solution-mediated BG reactions. Formation of a crystalline c-HA layer was delayed up to three or more days in solution with plasma ions. In the presence of serum, only amorphous surfaces composed of Si, Ca, and P were observed for any time up to seven days of immersion. The present data suggest that serum proteins adsorb in tandem with the occurrence of solution-mediated reactions leading to formation of a silica-gel. Amorphous Ca-P phases accumulate in the Si-rich matrix. Furthermore, the present data, in conjunction with the data published before,(1) suggest that physicochemical and cell-mediated reactions occur in parallel to form the glass-tissue interfacial layer. (C) 1997 John Wiley & Sons, Inc.
引用
收藏
页码:363 / 375
页数:13
相关论文
共 50 条
  • [1] Characterization of microrough bioactive glass surface:: Surface reactions and osteoblast responses in vitro
    Itälä, A
    Ylänen, HO
    Yrjans, J
    Heino, T
    Hentunen, T
    Hupa, M
    Aro, HT
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 2002, 62 (03): : 404 - 411
  • [2] “In vitro” apatite formation on the surface of bioactive glass
    X. V. Bui
    V. B. Nguyen
    T. T. H. Le
    Q. M. Do
    Glass Physics and Chemistry, 2013, 39 : 64 - 66
  • [3] "In vitro" apatite formation on the surface of bioactive glass
    Bui, X. V.
    Nguyen, V. B.
    Le, T. T. H.
    Do, Q. M.
    GLASS PHYSICS AND CHEMISTRY, 2013, 39 (01) : 64 - 66
  • [4] SOLUTION EFFECTS ON THE SURFACE-REACTIONS OF A BIOACTIVE GLASS
    FILGUEIRAS, MR
    LATORRE, G
    HENCH, LL
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1993, 27 (04): : 445 - 453
  • [5] The effect of submicron bioactive glass particles on in vitro osteogenesis
    Liu, Shaoqing
    Gong, Weiyu
    Dong, Yanmei
    Hu, Qing
    Chen, Xiaofeng
    Gao, Xuejun
    RSC ADVANCES, 2015, 5 (49) : 38830 - 38836
  • [6] Effect of Process Conditions on Microstructure and Properties of Bioactive Glass
    Chen, Xiaofeng
    Hu, Jing
    Zhao, Naru
    Meng, Yongchun
    Li, Yuli
    MATERIALS RESEARCH, PTS 1 AND 2, 2009, 610-613 : 1059 - 1065
  • [7] Effect of local ion concentrations on the in vitro reactions of bioactive glass 45S5 particles
    Siekkinen, Minna
    Karlstrom, Oskar
    Hupa, Leena
    INTERNATIONAL JOURNAL OF APPLIED GLASS SCIENCE, 2022, 13 (04) : 695 - 707
  • [8] SOLUTION EFFECTS ON THE SURFACE-REACTIONS OF 3 BIOACTIVE GLASS COMPOSITIONS
    FILGUEIRAS, MRT
    LATORRE, G
    HENCH, LL
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1993, 27 (12): : 1485 - 1493
  • [9] Influence of physicochemical reactions of bioactive glass on the behavior and activity of human osteoblasts in vitro
    Josset, Y
    Nasrallah, F
    Jallot, E
    Lorenzato, M
    Dufour-Mallet, O
    Balossier, G
    Laurent-Maquin, D
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART A, 2003, 67A (04) : 1205 - 1218
  • [10] Mimicking physiological flow conditions to study alterations of bioactive glass surfaces in vitro
    Hoener, Miriam
    Boeke, Frederik
    Weber, Michael
    Fischer, Horst
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2018, 106 (01) : 228 - 236