Effect of Pt addition on sulfur dioxide and water vapor tolerance of Pd-Mn-hexaaluminate catalysts for high-temperature oxidation of methane

被引:70
|
作者
Yashnik, S. A. [1 ]
Chesalov, Yu. A. [1 ,2 ]
Ishchenko, A. V. [1 ]
Kaichev, V. V. [1 ,2 ]
Ismagilov, Z. R. [1 ,3 ]
机构
[1] Boreskov Inst Catalysis, Lavrentieva Ave 5, Novosibirsk 630090, Russia
[2] Novosibirsk State Univ, Pirogova Str 2, Novosibirsk 630090, Russia
[3] Inst Coal Chem & Mat Sci, Sovetskiy Ave 18, Kemerovo 650000, Russia
基金
俄罗斯基础研究基金会;
关键词
Methane oxidation; Mn-hexaaluminate; Pt-catalyst; Pd-catalyst; Sulfur-resistance; PALLADIUM-BASED CATALYSTS; NOBLE-METAL CATALYSTS; SUPPORTED PALLADIUM; PT CATALYSTS; PDO/AL2O3; CATALYST; PROPANE OXIDATION; GAMMA-ALUMINA; COMBUSTION; PLATINUM; GAS;
D O I
10.1016/j.apcatb.2016.11.018
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
An effect of Pt addition to improve the catalytic performance of Pd-modified Mn-hexaaluminate in the high-temperature oxidation of methane, especially in SO2 and water presence, has been studied. X-ray diffraction, high-resolution transmission electron microscopy, X-ray photoelectron spectroscopy, thermogravimetry and differential thermal analysis were used for the characterization of fresh and spent catalysts. Temperature-programmed reduction by hydrogen was employed to study the redbx properties of the catalysts. Four high-temperature tests (at 670 degrees C) of the methane oxidation were applied to reveal the water and sulfur resistance of the catalysts: 1) dry methane-air feed; 2) wet methane-air feed containing 3 wt% of water vapor; 3) methane-air feed containing 1000 ppm of SO2; and 4) wet methane-air feed with 1000 ppm of SO2. The Pt-doped Pd-Mn-hexaaluminate catalyst with the atomic ratio of Pt/Pd <0.3 has been shown to possess the highest catalytic activity in the oxidation of methane, high water and sulfur tolerance, and reducibility by hydrogen as compared to the monometallic Pd-Mn-hexaaluminate catalyst and the bimetallic catalysts with Pt/Pd > 0.5. From the formal kinetic data of the oxidation of methane on the fresh and deactivated catalysts, we assumed that deactivation of the catalysts is due to a decrease in the amount of catalytically active sites in the bimetallic 0.33Pt-0.67Pd(0.27)/MnLaAl11O19 catalyst and a change in the state of active component in the other catalysts. Their oxidation ability and redox behavior were shown to be associated with the highly dispersed PdO particles, a Pd0 layer (3-5 nm) covering the metal palladium particles as well as the Mn3+-enriched MnLaAl11O19. The improved water and sulfur resistance is found to correlate with the presence of particles of PtPd alloy, with its fraction not exceeding 50%. (C) 2016 Elsevier B.V. All rights reserved.
引用
收藏
页码:89 / 106
页数:18
相关论文
共 41 条
  • [1] Structure and properties of Pd–Mn hexaaluminate catalysts modified with platinum for the high-temperature oxidation of methane
    S. A. Yashnik
    T. A. Surovtsova
    A. V. Ishchenko
    V. V. Kaichev
    Z. R. Ismagilov
    Kinetics and Catalysis, 2016, 57 : 528 - 539
  • [2] Structure and properties of Pd-Mn hexaaluminate catalysts modified with platinum for the high-temperature oxidation of methane
    Yashnik, S. A.
    Surovtsova, T. A.
    Ishchenko, A. V.
    Kaichev, V. V.
    Ismagilov, Z. R.
    KINETICS AND CATALYSIS, 2016, 57 (04) : 528 - 539
  • [3] Effect of water vapor on high-temperature oxidation of FeCr alloys
    W. J. Quadakkers
    J. Żurek
    M. Hänsel
    JOM, 2009, 61 : 44 - 50
  • [4] Effect of Water Vapor on the High-Temperature Oxidation of Pure Ni
    M. Auchi
    S. Hayashi
    K. Toyota
    S. Ukai
    Oxidation of Metals, 2012, 78 : 51 - 61
  • [5] Effect of water vapor on high-temperature oxidation of FeCr alloys
    Quadakkers, W. J.
    Zurek, J.
    Haensel, M.
    JOM, 2009, 61 (07) : 44 - 50
  • [6] EFFECT OF WATER-VAPOR ON HIGH-TEMPERATURE OXIDATION OF SIC
    ISHIKAWA, M
    NAKANO, Y
    ISHIDA, S
    TAKEUCHI, N
    WAKAMATSU, M
    WATANABE, K
    NIPPON SERAMIKKUSU KYOKAI GAKUJUTSU RONBUNSHI-JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1992, 100 (10): : 1200 - 1205
  • [7] Effect of Water Vapor on the High-Temperature Oxidation of Pure Ni
    Auchi, M.
    Hayashi, S.
    Toyota, K.
    Ukai, S.
    OXIDATION OF METALS, 2012, 78 (1-2): : 51 - 61
  • [8] Effect of water vapor on high-temperature oxidation of NiAl alloy
    Zhu, Dingding
    Wang, Xinli
    Zhao, Jun
    Lu, Jian
    Zhou, Yichun
    Cai, Canying
    Huang, Jianyu
    Zhou, Guangwen
    CORROSION SCIENCE, 2020, 177 (177)
  • [9] Low-temperature methane oxidation over oxide-supported Pd catalysts:: inhibitory effect of water vapor
    Kikuchi, R
    Maeda, S
    Sasaki, K
    Wennerström, S
    Eguchi, K
    APPLIED CATALYSIS A-GENERAL, 2002, 232 (1-2) : 23 - 28
  • [10] High-temperature methane oxidation over metallic monolith-supported zeolite catalysts containing Mn, Co, and Pd ions
    Slovetskaya, KL
    Kustov, LM
    RUSSIAN CHEMICAL BULLETIN, 2003, 52 (09) : 1933 - 1939