Corrosion of Binary Fe-Si Alloys in Reducing Oxidizing and Sulfidizing-Oxidizing Atmospheres at 700 A°C

被引:7
|
作者
Liu, L. L. [1 ]
Guo, Q. Q. [1 ]
Zeng, C. L. [1 ]
Niu, Y. [1 ]
机构
[1] Chinese Acad Sci, Inst Met Res, State Key Lab Corros & Protect, Shenyang 110016, Peoples R China
来源
OXIDATION OF METALS | 2014年 / 81卷 / 3-4期
关键词
Fe-Si alloys; Sulfidation; Oxidation; Si effect; HIGH-TEMPERATURE OXIDATION; INTERNAL OXIDATION; CONTAINING STEELS; FERROUS SULFIDE; SELF-DIFFUSION; IRON; CARBON; 600-800-DEGREES-C; SILICON; OXYGEN;
D O I
10.1007/s11085-013-9459-y
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The corrosion behavior of three Fe-Si alloys containing approximately 5, 9 and 13 at.% Si was studied at 700 A degrees C in an H-2-CO2 gas mixture providing 10(-20) atm O-2 as well as in an H-2-H2S-CO2 gas mixture providing the same oxygen pressure coupled to an S-2 pressure of 10(-8) atm. All the alloys followed complex kinetics which were mostly linear for Fe-5Si, but showed one or two parabolic stages for the other two alloys. Simple oxidation produced essentially two-layered scales in which Si was confined to the alloy consumption zone in the form of silicon oxide and iron-silicon double oxide. Corrosion in the oxidizing-sulfidizing gas mixture produced scales composed of a thick external zone of pure FeS followed by an internal region containing complex mixtures of FeS with Si and Fe oxides. Internal oxidation of silicon was only observed for the oxidation of Fe-5Si in both environments. The extent of corrosion decreased in both gas mixtures with an increase in the Si content of the alloys. Finally, the addition of sulfur produced a significant increase of the overall mass gains for each alloy.
引用
收藏
页码:477 / 502
页数:26
相关论文
共 50 条
  • [1] Corrosion of Binary Fe–Si Alloys in Reducing Oxidizing and Sulfidizing–Oxidizing Atmospheres at 700 °C
    L. L. Liu
    Q. Q. Guo
    C. L. Zeng
    Y. Niu
    Oxidation of Metals, 2014, 81 : 477 - 502
  • [2] Corrosion of Fe-Cr-Si Alloys in Oxidizing and Sulphidizing-Oxidizing Atmospheres
    Li, Wenbo
    Xu, Chenghao
    Chen, Ken
    Liu, Lanlan
    Yang, Haiyun
    Cheng, Qiao
    Zeng, Minyu
    COATINGS, 2022, 12 (10)
  • [3] The corrosion of Fe-15 wt% Y and Fe-30 wt% Y in sulfidizing-oxidizing atmospheres at 600-800°C
    Niu, Y
    Gesmundo, F
    Yan, R
    Wu, W
    CORROSION SCIENCE, 1999, 41 (05) : 989 - 1012
  • [4] The corrosion of Co-15 wt.% Y at 600-800°C in sulfidizing-oxidizing atmospheres
    Niu, Y
    Gesmundo, F
    Li, YS
    OXIDATION OF METALS, 1999, 51 (5-6): : 421 - 447
  • [5] The Corrosion of Co-15 wt.% Y at 600-800°C in Sulfidizing-Oxidizing Atmospheres
    Y. Niu
    F. Gesmundo
    Y. S. Li
    Oxidation of Metals, 1999, 51 : 421 - 447
  • [6] The corrosion of Fe-15 wt% Y and Fe-30 wt% Y in sulfidizing-oxidizing atmospheres at 600-800°C
    State Key Lab. Corros. and Protect., Wencui Road 62, 110015, Shenyang, China
    不详
    Corros. Sci., 5 (989-1012):
  • [7] High Temperature Corrosion of Fe-C-S Cast Irons in Oxidizing and Sulfidizing Atmospheres
    Thuan-Dinh NGUYEN
    Dong-Bok LEE
    Journal of Materials Science & Technology, 2008, (03) : 327 - 329
  • [8] High temperature corrosion of Fe-C-S cast irons in oxidizing and sulfidizing atmospheres
    Nguyen, Thuan-Dinh
    Lee, Dong-Bok
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2008, 24 (03) : 327 - 329
  • [9] High temperature corrosion of Fe-C-S cast irons in oxidizing and sulfidizing atmospheres
    Nguyen, Thuan-Dinh
    Lee, Dong-Bok
    Journal of Materials Science and Technology, 2008, 24 (03): : 327 - 329
  • [10] Stability of lithium aluminate in reducing and oxidizing atmospheres at 700 °C
    Heo, Su Jeong
    Hu, Boxun
    Manthina, Venkata
    Hilmi, Abdelkader
    Yuh, Chao-Yi
    Surendranath, Arun
    Singh, Prabhakar
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2016, 41 (41) : 18884 - 18892