Sheet metal forming is one of the most popular technologies for obtaining finished products in the automotive industry. The main techniques of sheet metal forming: are sheet microforming, warm/hot forming, incremental sheet forming, flexible-die forming, Electromagnetic sheet forming, Electrohydraulic forming, Spinning and Shear Spinning, Shear Spinning and Flow Forming, and cold sheet forming. One most popular cold stamping process. In the production line of Ravne VPS400 1992, we take twenty details for looking quality review, looking for surface damage reasons-a little changing tonnage and speed. The biggest deformation, when velocity is the slowest the tonnage doesn't have an impact on this radius deformation. Firstly, we measured the surface for all twenty details with Contourograph CV-2100 M4. In one measurement point, we have ten points which are the biggest or slowest tolerance, these results can be the reason why the detail is damaged. These details make one tact process. We can say the recommendation - if the detail will be making for one more tact process, a detail not be damaged, but this extra process is a very grown the price. Second, we see metal steel chemistry alloy elements, and we can be looking which elements have some reason mechanical properties of steels. Samples don't have enough elasticity, and in steel structure, we can recommend taking more carbon C, Silicon Si and Vanadium V. Silicon Si, is important for machinability and tensile properties as well and this element is essential in steel structure. Thirsty, we used the 3D coordinate measuring machine Mitutoyo Surface Measure 606T, looking for tolerances differences. And we see in detail which places will have damage, we have the results lowest from the layout, we see the blue color. If we made detail not one tact process, but more tact's making detail the thickness would be evenly gradually. The crystalline structure of the metal broke due to excessive thinning. Was cut a few details and measured the thickness in 4 points in every detail. 7 counter thickness is low than 28%. This is metal structure damage reason.