Effect of hydrogen on the creep behavior of Zr-2.5%Nb alloy at 723 K

被引:23
|
作者
Kishore, R. [1 ]
机构
[1] Bhabha Atom Res Ctr, Mat Grp, Mech Met Sect, Bombay 400085, Maharashtra, India
关键词
HIGH-PURITY IRON; MECHANICAL-PROPERTIES; ZIRCONIUM ALLOYS; DEFORMATION; CRACKING; MODEL;
D O I
10.1016/j.jnucmat.2009.01.034
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Increased plasticity is reported in Ti alloys, stainless steels and Pd by the introduction of hydrogen. The dissolved hydrogen in zirconium and its alloys which have similar properties as those of titanium and its alloys, can modify the creep properties of the matrix. Hydrogen, formed during the corrosion reaction of Zr-2.5%Nb pressure tube, in a CANDU design nuclear reactor, with the coolant can ingress into the metal matrix. This absorbed hydrogen can lead to an unexpected increase in length and in diameter of the pressure tube. In order to evaluate the effect of hydrogen on the creep behavior of the pressure tube material, tensile specimens with longitudinal and transverse orientations were hydrided to 65 and 160 wt ppm and creep tested at 723 K over a stress range. The combined influence of hydrogen and specimen orientations on creep rate is evaluated, and an attempt is made to explain the results using the deformation mechanisms reported in literature. (C) 2009 Elsevier B.V. All rights reserved.
引用
收藏
页码:591 / 594
页数:4
相关论文
共 50 条
  • [1] THE PRECIPITATION BEHAVIOR OF A ZR-2.5 WT PCT NB ALLOY
    LUO, CP
    WEATHERLY, GC
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1988, 19 (05): : 1153 - 1162
  • [2] High temperature mechanical behavior of Zr-2.5% Nb alloy
    Rodchenkov, BS
    Semenov, AN
    NUCLEAR ENGINEERING AND DESIGN, 2005, 235 (17-19) : 2009 - 2018
  • [3] EFFECT OF ALLOYING ELEMENTS ON SOLUBILITY OF HYDROGEN IN ZR-2.5 WT PERCENT NB ALLOY
    SINHA, VK
    JOURNAL OF NUCLEAR MATERIALS, 1976, 59 (02) : 201 - 205
  • [4] CREEP STRENGTH OF QUENCHED AND AGED ZR-2.5 WT PERCENT NB ALLOY
    FIDLERIS, V
    JOURNAL OF NUCLEAR MATERIALS, 1974, 54 (02) : 199 - 211
  • [6] IN-REACTOR CREEP OF ZR-2.5 AT PERCENT NB
    GILBERT, ER
    JOURNAL OF NUCLEAR MATERIALS, 1968, 26 (01) : 105 - &
  • [7] Evaluation of the delayed hydrogen cracking behavior and the hydrogen diffusion coefficient for different microstructures of the Zr-2.5%Nb alloy
    Gomez, Adrian Guillermo
    Ponce, Jose Paez
    Grosse, M.
    Soria, Sergio
    Condo, Adriana
    Flores, Alejandra
    Schulz, Michael
    Vizcaino, Pablo
    Santisteban, J. R.
    JOURNAL OF NUCLEAR MATERIALS, 2023, 587
  • [8] Effect of microstructure on fatigue crack growth in Zr-2.5 Nb alloy
    Ganguly, S
    Dubey, JS
    Haq, A
    Chakravartty, JK
    Biswas, AR
    Banerjee, S
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 1996, 49 (04): : 533 - 540
  • [9] Liquid metal embrittlement of Zr-2.5% Nb alloy
    Cox, B
    Wong, YM
    JOURNAL OF NUCLEAR MATERIALS, 1997, 245 (01) : 34 - 43
  • [10] ULTRASONIC INFLUENCE ON NANOSTRUCTURE IN Zr-2.5%Nb ALLOY
    Mats, A. V.
    Netesov, V. M.
    Sokolenko, V. I.
    PROBLEMS OF ATOMIC SCIENCE AND TECHNOLOGY, 2011, (04): : 108 - 110