Long-term high-temperature oxidation of iridium coated rhenium by electrical resistance heating method

被引:25
|
作者
Zhu, Li'an [1 ]
Bai, Shuxin [1 ]
Zhang, Hong [1 ]
Ye, Yicong [1 ]
Gao, Wei [2 ]
机构
[1] Natl Univ Def Technol, Coll Aerosp Sci & Engn, Dept Mat Sci & Engn, Changsha 410073, Hunan, Peoples R China
[2] Univ Auckland, Dept Chem & Mat Engn, Auckland 1142, New Zealand
基金
中国国家自然科学基金;
关键词
Iridium; Rhenium; Oxidation; Resistance heating; High temperature; CHEMICAL-VAPOR-DEPOSITION; CARBON-CARBON COMPOSITES; PULSED-LASER DEPOSITION; THIN-FILMS; PLATINUM FILMS; GLOW PLASMA; COATINGS; MICROSTRUCTURE; SUBSTRATE; BEHAVIOR;
D O I
10.1016/j.ijrmhm.2014.01.010
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A continuous and compact iridium (Ir) coating with a thickness of similar to 100 mu m was electrodeposited on a rhenium (Re) rod in molten salt at 580 degrees C for 4 h. The oxidation resistance and failure mechanism of the Ir coated Re (Ir/Re) material were investigated by resistance heating method at 2000 Tin air till the Ir coating failed. The results showed that the lifetime of the Ir/Re rod oxidized at 2000 degrees C in air was 183 min. After high-temperature oxidation, except for the failure position, the Ir. coating in most of the heated regions kept dense and exhibited excellent adhesion on the substrate, with smooth surface and large grain size. The preferred orientation of the Ir coating changed from < 220 > to < 111 > after oxidation test. From the end to the center of the as-oxidized Ir/Re sample, the Ir coating became thinner, and the diffusion layer between Ir and Re got thicker. Meanwhile, the preferential oxidation of grain boundaries of Ir coating was more and more severe. It was found that the lifetime of the Ir/Re material in high-temperature oxidizing environment is closely related to the consumption rates of Ir coating by both the direct oxidation of Ir and the diffusion of Re into Jr coating. Based on the diffusion and oxidation kinetics of Re and Ir, the lifetime of the Ir/Re sample in the present study was calculated to be 242 min. The difference between the calculated and real lifetimes can be attributed to the ignored fact that Re diffuses rapidly along the grain boundaries of In coating in the calculation. (C) 2014 Elsevier Ltd. All rights reserved.
引用
收藏
页码:42 / 48
页数:7
相关论文
共 50 条
  • [1] High-temperature diffusion in couple of electrodeposited iridium/rhenium
    Zhu, Li'an
    Wang, Jiangfan
    Wang, Zhen
    Ye, Yicong
    Bai, Shuxin
    Li, Shun
    Tang, Yu
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2021, 97
  • [2] Processes of phase instability in high-temperature steels subjected to long-term heating
    Tarasenko, L. V.
    Titov, V. I.
    METAL SCIENCE AND HEAT TREATMENT, 2005, 47 (11-12) : 538 - 543
  • [3] Processes of phase instability in high-temperature steels subjected to long-term heating
    L. V. Tarasenko
    V. I. Titov
    Metal Science and Heat Treatment, 2005, 47 : 538 - 543
  • [4] Effect of long-term aging treatment on the structure and oxidation resistance of Cr coatings under high-temperature steam
    Xiang, Yang
    Zhao, Sha
    Liu, Chunhai
    Yang, Hongyan
    Zhang, Wei
    Wang, Hui
    Zhang, Ruiqian
    He, Hengji
    Liu, Sujuan
    CORROSION SCIENCE, 2023, 212
  • [5] Oxidation of iridium coating on rhenium coated graphite at elevated temperature in stagnated air
    Huang, Yongle
    Bai, Shuxin
    Zhang, Hong
    Ye, Yicong
    APPLIED SURFACE SCIENCE, 2015, 328 : 436 - 443
  • [6] Effect of Rhenium addition on the high-temperature oxidation resistance of anodized γ-TiAl alloy
    Yang, Huiting
    Xu, Shenghang
    Lan, Junjie
    Gao, Jing
    Cao, Huazhen
    Zheng, Guoqu
    Zhang, Huibin
    Feng, Wenyu
    JOURNAL OF ALLOYS AND COMPOUNDS, 2025, 1010
  • [7] Long-term high-temperature operation of the HTTR
    Goto, Minoru
    Shinohara, Masanori
    Tochio, Daisuke
    Shimazaki, Yosuke
    Hamamoto, Shinpei
    Tachibana, Yukio
    NUCLEAR ENGINEERING AND DESIGN, 2012, 251 : 181 - 190
  • [8] Long-term carbonation resistance of concrete under initial high-temperature curing
    Li, Guo
    Yao, Feng
    Liu, Ping
    Yan, Chenghua
    MATERIALS AND STRUCTURES, 2016, 49 (07) : 2799 - 2806
  • [9] Long-term carbonation resistance of concrete under initial high-temperature curing
    Guo Li
    Feng Yao
    Ping Liu
    Chenghua Yan
    Materials and Structures, 2016, 49 : 2799 - 2806
  • [10] HIGH-TEMPERATURE SPECIFIC ELECTRICAL RESISTIVITY OF RHENIUM AND MOLYBDENUM - RHENIUM ALLOYS
    PELETSKI.VE
    DRUZHINI.VP
    HIGH TEMPERATURE, 1972, 10 (03) : 584 - 585