- [5] THE BENEFIT OF HYDROGEN ADDITION TO THE BOILING WATER-REACTOR ENVIRONMENT ON STRESS-CORROSION CRACK INITIATION AND GROWTH IN TYPE-304 STAINLESS-STEEL JOURNAL OF ENGINEERING MATERIALS AND TECHNOLOGY-TRANSACTIONS OF THE ASME, 1986, 108 (01): : 10 - 19
- [6] Intergranular stress corrosion cracking behavior of types 308 and 316 stainless steel weld metals in a simulated boiling water reactor environment METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2002, 33 (09): : 2907 - 2919
- [7] Intergranular stress corrosion cracking behavior of types 308 and 316 stainless steel weld metals in a simulated boiling water reactor environment Metallurgical and Materials Transactions A, 2002, 33 : 2907 - 2919
- [10] Quantitative prediction of EAC crack growth rate of sensitized type 304 stainless steel in boiling water reactor environments based on EPFEM JOURNAL OF PRESSURE VESSEL TECHNOLOGY-TRANSACTIONS OF THE ASME, 2007, 129 (03): : 460 - 467