Hydrogen-assisted fatigue crack propagation in a pure BCC iron. Part II: Accelerated regime manifested by quasi-cleavage fracture at relatively high stress intensity range values

被引:7
|
作者
Birenis, Domas [1 ]
Ogawa, Yuhei [2 ,3 ]
Matsunaga, Hisao [4 ,5 ,6 ]
Takakuwa, Osamu [5 ]
Yamabe, Junichiro [5 ,6 ,7 ]
Prytz, Oystein [1 ]
Thogersen, Annett [8 ]
机构
[1] Univ Oslo, Dept Phys, Ctr Mat Sci & Nanotechnol, NO-0316 Oslo, Norway
[2] Kyushu Univ, Grad Sch Engn, Nishi Ku, 744 Motooka, Fukuoka, Fukuoka 8190395, Japan
[3] Japan Soc Promot Sci, Nishi Ku, 744 Motooka, Fukuoka, Fukuoka 8190395, Japan
[4] Japan Soc Promot Sci, Dept Mech Engn, Nishi Ku, 744 Motooka, Fukuoka, Fukuoka 8190395, Japan
[5] Japan Soc Promot Sci, Res Ctr Hydrogen Ind Use & Storage HYDROGENIUS, Nishi Ku, 744 Motooka, Fukuoka, Fukuoka 8190395, Japan
[6] Japan Soc Promot Sci, I2CNER, Nishi Ku, 744 Motooka, Fukuoka, Fukuoka 8190395, Japan
[7] AIST Kyushu Univ Hydrogen Mat Lab HydroMate, Nishi Ku, 744 Motooka, Fukuoka, Fukuoka 8190395, Japan
[8] SINTEF Mat & Chem, POB 124 Blindern, NO-0314 Oslo, Norway
关键词
GROWTH; EMBRITTLEMENT; MECHANISM; DEFORMATION; TEMPERATURE; BEHAVIOR; STEEL;
D O I
10.1051/matecconf/201816503010
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Hydrogen effect on fatigue performance at relatively high values of stress intensity factor range, Delta K, of pure BCC iron has been studied with a combination of various electron microscopy techniques. Hydrogen-assisted fatigue crack growth rate is manifested by a change of fracture features at the fracture surface from ductile transgranular in air to quasi-cleavage in hydrogen gas. Grain reference orientation deviation (GROD) analysis has shown a dramatic suppression of plastic deformation around the crack wake in samples fatigued in hydrogen. These results were verified by preparing site-specific specimens from different fracture features by using Focused Ion Beam (FIB) technique and observing them with Transmission Electron Microscope (TEM). The FIB lamella taken from the sample fatigued in air was decorated with dislocation cell structure indicating high amount of plasticity, while the lamella taken from the quasi-cleavage surface of the sample fatigued in hydrogen revealed a distribution of dislocation tangles which corresponds to smaller plastic strain amplitude involved at the point of fracture. These results show that a combination of critical hydrogen concentration and critical stress during fatigue crack growth at high Delta K values triggers cleavage-like fracture due to reduction of cohesive force between matrix atoms.
引用
收藏
页数:6
相关论文
共 2 条
  • [1] Hydrogen-assisted fatigue crack propagation in a pure BCC iron. Part I: Intergranular crack propagation at relatively low stress intensities
    Ogawa, Yuhei
    Birenis, Domas
    Matsunaga, Hisao
    Takakuwa, Osamu
    Yamabe, Junichiro
    Prytz, Oystein
    Thogersen, Annett
    12TH INTERNATIONAL FATIGUE CONGRESS (FATIGUE 2018), 2018, 165
  • [2] The role of intergranular fracture on hydrogen-assisted fatigue crack propagation in pure iron at a low stress intensity range
    Ogawa, Yuhei
    Birenis, Domas
    Matsunaga, Hisao
    Takakuwa, Osamu
    Yamabe, Junichiro
    Prytz, Oystein
    Thogersen, Annett
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 733 : 316 - 328