Anodic oxide layer formation on A357 aluminium alloy produced by Thixocasting

被引:4
|
作者
Forn, A. [1 ]
Picas, J. A. [1 ]
Baile, M. T. [1 ]
Menargues, S. [1 ]
Garcia, V. G. [1 ]
机构
[1] Univ Politecn Catalunya, Light Alloys & Surface Treatments Design Ctr, CDAL, Dept Mat Sci, Vilanova I La Geltru 08800, Barcelona, Spain
关键词
Thixocasting; A357; ageing heat treatments; anodizing; SEM observation; friction coefficient; wear rate;
D O I
10.4028/www.scientific.net/SSP.116-117.80
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Anodizing is widely used in the surface treatment of aluminium alloys in order to preserve the integrity of the alloy surface, to minimize the need for maintenance and repair, and to maximize the component life. The aim of this work is to study the influence heat treatments (T5 and T6) have on the anodization of A357 aluminium alloy produced by a Thixocasting process. In particular the effect of shape, size and distribution of silicon and intermetallic phases on the anodic oxide film formation. SEM and EDS analyses were used to examine the microstructural features found on, within and under the anodic oxide layer. Experiments using a tribometer (pin-on-disc tests) were performed in order to evaluate the friction and wear properties of the different layers.
引用
收藏
页码:80 / 83
页数:4
相关论文
共 50 条
  • [1] Thixoextrusion of A357 aluminium alloy
    Forn, A.
    Vaneetveld, G.
    Pierret, J. C.
    Menargues, S.
    Baile, M. T.
    Campillo, M.
    Rassili, A.
    [J]. TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2010, 20 : S1005 - S1009
  • [2] Thixoextrusion of A357 aluminium alloy
    A.FORN
    G.VANEETVELD
    J.C.PIERRET
    S.MENARGUES
    M.T.BAILE
    M.CAMPILLO
    A.RASSILI
    [J]. Transactions of Nonferrous Metals Society of China, 2010, 20 (S3) : 1005 - 1009
  • [3] Effects of the thixocasting injection velocity on tensile properties of an A357 Al alloy
    Ozer, Melika
    Akar, Neset
    Kocatepe, Kadir
    Erdogan, Mehmet
    [J]. MATERIALS TESTING, 2015, 57 (09) : 790 - 794
  • [4] A357 aluminium alloy produced by LPBF: Tribological behaviour in dry sliding conditions
    Lorenzetti, L.
    Tonelli, L.
    Ceschini, L.
    Liverani, E.
    Martini, C.
    [J]. WEAR, 2022, 510-511
  • [5] Wear analysis of A357 aluminium alloy under fretting
    Elleuch, K
    Fouvry, S
    [J]. WEAR, 2002, 253 (5-6) : 662 - 672
  • [6] Pitting corrosion of A357 aluminium alloy obtained by semisolid processing
    Bastidas, JM
    Forn, A
    Baile, MT
    Polo, JL
    Torres, CL
    [J]. MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2001, 52 (09): : 691 - 696
  • [7] Microstructure and properties of A357 aluminium alloy treated by pulsed magnetic field
    Zhang, L.
    Zhan, W.
    Jin, F.
    Zhou, Q.
    [J]. MATERIALS SCIENCE AND TECHNOLOGY, 2018, 34 (06) : 698 - 702
  • [8] The origins for tensile properties of selective laser melted aluminium alloy A357
    Rao, Jeremy H.
    Zhang, Yong
    Fang, Xiya
    Chen, Yu
    Wu, Xinhua
    Davies, Chris H. J.
    [J]. ADDITIVE MANUFACTURING, 2017, 17 : 113 - 122
  • [9] SLM-fabricated A357 Aluminium alloy: dry sliding behaviour
    Lorenzetti, L.
    Tonetti, L.
    Ceschini, L.
    Martini, C.
    [J]. METALLURGIA ITALIANA, 2021, Associazione Italiana di Metallurgia (05): : 22 - 31
  • [10] The influence of processing parameters on aluminium alloy A357 manufactured by Selective Laser Melting
    Rao, Heng
    Giet, Stephanie
    Yang, Kun
    Wu, Xinhua
    Davies, Chris H. J.
    [J]. MATERIALS & DESIGN, 2016, 109 : 334 - 346