Microstructure and wear behaviors of WC-Ni coatings fabricated by laser cladding under high frequency micro-vibration

被引:65
|
作者
Li, Chonggui [1 ]
Zhang, Qunsen [1 ]
Wang, Feifei [1 ]
Deng, Peiran [1 ]
Lu, Qinghua [1 ]
Zhang, Youfeng [1 ]
Li, Shuai [1 ]
Ma, Pan [1 ]
Li, Wenge [2 ]
Wang, You [3 ]
机构
[1] Shanghai Univ Engn Sci, Sch Mat Engn, Shanghai 201600, Peoples R China
[2] Shanghai Maritime Univ, Inst Marine Mat Sci & Engn, Shanghai 201306, Peoples R China
[3] Harbin Inst Technol, Dept Mat Sci, Lab Nano Surface Engn, Harbin 150001, Heilongjiang, Peoples R China
基金
中国国家自然科学基金;
关键词
Laser cladding; Composite coating; High frequency micro-vibration; WC; Wear resistance; PLASMA ELECTROLYTIC OXIDATION; COMPOSITE COATINGS; MECHANICAL-PROPERTIES; RESISTANCE PROPERTIES; ALLOY; EVOLUTION; CORROSION; PROPERTY; SIZE;
D O I
10.1016/j.apsusc.2019.04.245
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
WC-Ni composite coatings were fabricated on Ti-6Al-4V alloy substrates by laser cladding under high frequency micro-vibration. The microstructure, phase composition, microhardness and wear resistance of the cladding coatings were investigated by X-ray diffractometer (XRD), scanning electron microscope (SEM), energy disperse spectroscope (EDS), microhardness tester and friction and wear testing apparatus, respectively. The high frequency micro-vibration produced by a vibration exciter system made of magnetostrictive materials was used to assist laser cladding of nickel composite coatings. The effects of high frequency micro-vibration on the microstructure and properties of the cladding coatings are investigated. The results showed that high frequency microvibration promoted the formation of W2C and (Ti, W) C during the laser cladding process. Alloying carbide with rich tungsten is uniformly distributed in eutectic (Ti) Ni solid solution under the vibration frequency of 556 Hz, with some new W2C phases generated in the composite coating. In addition, at the bonding interface, the number of coarse dendrites is continuously reduced and that of fine grains is gradually increased. Appropriate increase of vibration frequency contributes to the refinement of the grains. The vibration makes the coating microstructure more uniform, which helps to reduce the microhardness fluctuation in the cladding coating. With the help of the fine-grained hard phase, the microhardness of the cladding coating is enhanced by the vibration. By choosing appropriate vibration parameters, high frequency micro-vibration helps to decrease the friction coefficient and wear loss of the composite coating.
引用
下载
收藏
页码:513 / 519
页数:7
相关论文
共 50 条
  • [1] Effect of high-frequency micro-vibration on microstructure and properties of laser cladding aluminum coatings
    Chonggui Li
    Shuai Li
    Ming Zeng
    Shuai Sun
    Feifei Wang
    You Wang
    The International Journal of Advanced Manufacturing Technology, 2019, 103 : 1633 - 1642
  • [2] Effect of high-frequency micro-vibration on microstructure and properties of laser cladding aluminum coatings
    Li, Chonggui
    Li, Shuai
    Zeng, Ming
    Sun, Shuai
    Wang, Feifei
    Wang, You
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2019, 103 (1-4): : 1633 - 1642
  • [3] High temperature wear resistance of laser cladding NiCrBSi and NiCrBSi/WC-Ni composite coatings
    Guo, Chun
    Zhou, Jiansong
    Chen, Jianmin
    Zhao, Jierong
    Yu, Youjun
    Zhou, Huidi
    WEAR, 2011, 270 (7-8) : 492 - 498
  • [4] Al2O3/TiO2-Ni-WC Composite Coatings Designed for Enhanced Wear Performance by Laser Cladding Under High-Frequency Micro-Vibration
    Wang, Feifei
    Li, Chonggui
    Sun, Shuai
    Zeng, Ming
    Liu, Chuanming
    Lu, Qinghua
    Wang, You
    JOM, 2020, 72 (11) : 4060 - 4068
  • [5] Al2O3/TiO2-Ni-WC Composite Coatings Designed for Enhanced Wear Performance by Laser Cladding Under High-Frequency Micro-Vibration
    Feifei Wang
    Chonggui Li
    Shuai Sun
    Ming Zeng
    Chuanming Liu
    Qinghua Lu
    You Wang
    JOM, 2020, 72 : 4060 - 4068
  • [6] Preparing WC-Ni coatings with laser cladding technology: A review
    Sun, Shengyuan
    Wang, Jiale
    Xu, Jihao
    Cheng, Xiangyu
    Jing, Chenghu
    Chen, Zhendong
    Ru, Haolei
    Liu, Yongyue
    Jiao, Junke
    MATERIALS TODAY COMMUNICATIONS, 2023, 37
  • [7] Effects of WC-Ni content on microstructure and wear resistance of laser cladding Ni-based alloys coating
    Guo, Chun
    Chen, Jianmin
    Zhou, Jiansong
    Zhao, Jierong
    Wang, Lingqian
    Yu, Youjun
    Zhou, Huidi
    SURFACE & COATINGS TECHNOLOGY, 2012, 206 (8-9): : 2064 - 2071
  • [8] Microstructure characteristic of laser welded joint under high frequency micro-vibration condition
    Chen, Xuan
    Lu, Qinghua
    Zhang, Jing
    Zhang, Cheng
    Cai, Zunwu
    Jixie Gongcheng Xuebao/Journal of Mechanical Engineering, 2016, 52 (20): : 60 - 65
  • [9] Microstructure and property of laser welded joint with high frequency micro-vibration process
    Zhang C.
    Lu Q.
    Cai Z.
    Zhang P.
    Hanjie Xuebao/Transactions of the China Welding Institution, 2019, 40 (02): : 86 - 90
  • [10] Wear mechanisms and micro-evaluation on WC particles investigation of WC-Fe composite coatings fabricated by laser cladding
    Xiao, Qi
    Sun, Wen lei
    Yang, Kai xin
    Xing, Xue feng
    Chen, Zi hao
    Zhou, Hao nan
    Lu, Jing
    SURFACE & COATINGS TECHNOLOGY, 2021, 420