Influence of liquid accelerators on shotcrete in karst area tunnels

被引:18
|
作者
Zhang, Ziwei [1 ]
Li, Guoxin [1 ]
Zhang, Ge [1 ,2 ]
Niu, Mengdie [1 ]
机构
[1] Xian Univ Architecture & Technol, Coll Mat Sci & Engn, Xian 710055, Peoples R China
[2] Xian Univ Architecture & Technol, Postdoctoral Mobile Stn Mat Sci & Engn, Xian, Peoples R China
关键词
Shotcrete; Accelerator; Karst; Calcium leaching; EARLY AGE HYDRATION; CEMENTITIOUS MATERIALS; PORTLAND-CEMENT; PART; CONCRETE; WATER; DURABILITY; STRENGTH; SULFATE; PASTES;
D O I
10.1016/j.cscm.2022.e01002
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Tunnel constructions built in karst areas are liable to calcium leaching, which can lead to CaCO3 deposits in tunnel drainage pipes and water gutters, resulting in the blockage of tunnel drainage systems. This research aimed to analyze the influence of liquid accelerators on shotcrete in karst area tunnels. To achieve this, the present study investigated the influence of accelerator type and the karst water environment on the degradation behaviors of shotcrete. More specifically, the calcium leaching processes of hardened cement pastes incorporated with various liquid accelerators were analyzed, and the tunnel drainage system blockage mechanism was expounded in terms of shotcrete lining. The results showed that the compressive strength of shotcrete decreased most significantly in a karst water environment, while the mass of shotcrete decreased most significantly in a flowing water environment. The shotcrete combined with an aluminum sulfatebased alkali-free liquid accelerator performed best in the attack test, and its maximum compressive strength decreased by only 0.33%. The accelerator can change the composition and microstructure of cement hydration, thus altering the deterioration resistance of shotcrete. In terms of shotcrete lining, calcium leaching can increase the pH value and calcium ion concentration of groundwater, resulting in the formation and crystallization of CaCO3.
引用
收藏
页数:14
相关论文
共 50 条
  • [1] SHOTCRETE IN TUNNELS
    MUIRWOOD, AM
    CONCRETE, 1973, 7 (12): : 32 - 32
  • [2] Influence of sodium aluminate on calcium leaching of shotcrete in tunnels
    Ye, Fei
    He, Biao
    Tian, Chong-ming
    Zhao, Meng
    Wang, Jian
    Han, Xing-bo
    Armaghani, Danial Jahed
    TUNNELLING AND UNDERGROUND SPACE TECHNOLOGY, 2021, 117 (117)
  • [3] Design standard for railway shotcrete tunnels in urban area in Japan
    Konishi, S
    Kojima, Y
    Arai, Y
    Tsuno, K
    Kawashima, Y
    Asakura, T
    (RE)CLAIMING THE UNDERGROUND SPACE, VOLS 1 AND 2, PROCEEDINGS, 2003, : 1059 - 1066
  • [4] Experimental study on sulfate resistance of shotcrete with different liquid accelerators
    Yang, Renhe
    He, Tingshu
    Guan, Mengqin
    Xu, Yongdong
    Ma, Xiaodong
    Lin, Yike
    Gui, Miaomiao
    Ke, Yuliang
    CASE STUDIES IN CONSTRUCTION MATERIALS, 2022, 16
  • [5] INFLUENCE OF SHRINKAGE AND CREEP OF SHOTCRETE ON SAFETY OF PRIMARY SUPPORT OF TUNNELS
    Li, Hongquan
    Yang, Chengyong
    Zhang, Qiang
    Kuang, Xing
    KEY TECHNOLOGIES OF RAILWAY ENGINEERING - HIGH SPEED RAILWAY, HEAVY HAUL RAILWAY AND URBAN RAIL TRANSIT, 2010, : 829 - 835
  • [6] Influence of Ground Temperature on Shotcrete-to-Rock Adhesion in Tunnels
    Duan, Limin
    Zhang, Yuanhang
    Lai, Jinxing
    ADVANCES IN MATERIALS SCIENCE AND ENGINEERING, 2019, 2019
  • [7] Influence of shotcrete accelerators on the hydration of cement pastes and their impact on sulfate resistance
    Winnefeld, Frank
    Kaufmann, Josef
    Loser, Roman
    Leemann, Andreas
    CONSTRUCTION AND BUILDING MATERIALS, 2021, 266
  • [8] WATERPROOFING OF TUNNELS BY THE USE OF SHOTCRETE
    ASTAD, U
    HEIMLI, P
    TUNNELS AND WATER, VOLS 1-3: WATER AND ITS INFLUENCE ON THE DESIGN, CONSTRUCTION, AND EXPLOITATION OF TUNNELS AND UNDERGROUND WORKS, 1989, : 393 - 397
  • [9] Shotcrete as final lining for tunnels
    Palermo, G
    Helene, PRDL
    TUNNELS AND METROPOLISES, VOLS 1 AND 2, 1998, : 349 - 354
  • [10] SHOTCRETE SUPPORT IN ROCK TUNNELS IN SCANDINAVIA
    CECIL, OS
    CIVIL ENGINEERING, 1970, 40 (01): : 74 - &