The effect of γ-Al2O3 surface hydroxylation on the stability and nucleation of Ni in Ni/γ-Al2O3 catalyst: a theoretical study

被引:33
|
作者
Liu, Zhixue [1 ]
Wang, Yuhan [2 ]
Li, Jingrui [1 ]
Zhang, Riguang [1 ]
机构
[1] Taiyuan Univ Technol, Key Lab Coal Sci & Technol, Minist Educ & Shanxi Prov, Taiyuan 030024, Shanxi, Peoples R China
[2] Beijing Inst Technol, Sch Chem Engn & Environm, Beijing 100081, Peoples R China
来源
RSC ADVANCES | 2014年 / 4卷 / 26期
基金
中国国家自然科学基金;
关键词
NONSPINEL STRUCTURAL MODELS; METAL-SUPPORT INTERACTION; GAMMA-ALUMINA SURFACES; NI/AL2O3; CATALYSTS; CO2; HYDROGENATION; CARBON NANOFIBERS; ALPHA-AL2O3(0001) SURFACE; CU/GAMMA-AL2O3; CATALYST; METHANE DECOMPOSITION; CLUSTER-SIZE;
D O I
10.1039/c3ra46352d
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
Using recent well-defined models of gamma-Al2O3 surfaces, the interactions of Ni-n(n = 1-7) clusters with different gamma-Al2O3 surfaces have been investigated in order to illustrate, by density functional theory periodic calculations, the effect of gamma-Al2O3 surface hydroxylation on the stability and nucleation of Ni in Ni/gamma-Al2O3 catalyst. Three types of gamma-Al2O3 surfaces, dehydrated gamma-Al2O3(100), dehydrated gamma-Al2O3(110) and hydrated gamma-Al2O3(110) were considered. Our results show that for the adsorption of Ni-n(n = 3-7) clusters, the gamma-Al2O3(110) surface is more favorable than the gamma-Al2O3(100) surface, however, for single Ni atoms and Ni-2 clusters, the reverse becomes true. Meanwhile, for the adsorption of Ni-n(n = 2-7) clusters, the hydrated (110) surface is not favorable compared to the dehydrated (110) surface, due to the presence of surface hydroxyls on the former. The reverse is true for single Ni atoms due to weaker surface deformation. Further, the support stabilizes Ni-n(n = 2-7) clusters well in the supported state, in which the presence of surface hydroxyls reduces the stability of the supported Ni-n clusters. On the other hand, the nucleation ability of Ni-n clusters on different gamma-Al2O3 surfaces, is more favorable on the gamma-Al2O3(110) surface than on the gamma-Al2O3(100) surface, and the dehydrated (110) surface is more favorable than the hydrated (110) surface due to the presence of surface hydroxyls, namely, surface hydroxylation reduces the nucleation ability of Ni-n clusters on the gamma-Al2O3 surface. More importantly, the exothermicity of supported Ni-n(n = 2-7) clusters on different gamma-Al2O3 surfaces is lower than that of isolated Ni-n clusters, indicating that the support is not favorable for the nucleation of Ni-n(n = 2-7) clusters, as a result, the support can inhibit the aggregation of clusters, and favors the formation of small clusters.
引用
收藏
页码:13280 / 13292
页数:13
相关论文
共 50 条
  • [1] Catalytic Hydrogenation of Benzaldehyde on Ni/Al2O3 or Co-Ni/Al2O3 Catalyst
    Liu, Wei
    Li, Ying
    Chen, Xianlan
    Zhang, Pei
    Yi, Ping
    Zhou, Yongfu
    Huang, Zhaolong
    ASIAN JOURNAL OF CHEMISTRY, 2013, 25 (03) : 1565 - 1568
  • [2] The catalytic performance of Ni2P/Al2O3 catalyst in comparison with Ni/Al2O3 catalyst in dehydrogenation of cyclohexane
    Li, Jingfeng
    Chai, Yongming
    Liu, Bin
    Wu, Yilan
    Li, Xuehui
    Tang, Zhe
    Liu, Yunqi
    Liu, Chenguang
    APPLIED CATALYSIS A-GENERAL, 2014, 469 : 434 - 441
  • [3] Raman spectroscopic study of Ni/Al2O3 catalyst
    Aminzadeh, A
    Sarikhani-fard, H
    SPECTROCHIMICA ACTA PART A-MOLECULAR AND BIOMOLECULAR SPECTROSCOPY, 1999, 55 (7-8) : 1421 - 1425
  • [4] Carbon deposition on A Ni/-Al2O3 catalyst
    Castro Luna A.E.
    Becerra A.M.
    Reaction Kinetics and Catalysis Letters, 1997, 61 (2): : 375 - 381
  • [5] Influence of the hydroxylation of γ-Al2O3 surfaces on the stability and growth of Cu for Cu/γ-Al2O3 catalyst: A DFT study
    Li, Jingrui
    Zhang, Riguang
    Wang, Baojun
    APPLIED SURFACE SCIENCE, 2013, 270 : 728 - 736
  • [6] Characterization method of Ni/Al2O3 catalyst
    Yu, Chen
    Huang, Xingliang
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2013, 246
  • [7] Preparation of Ni/Al2O3 catalyst by impregnation
    Zrncevic, S.
    Gomzi, Z.
    Kemija u industriji, 1995, 44 (03):
  • [8] REACTIONS OF ADSORBED HYDROGEN WITH OXYGEN ON FE/AL2O3, NI/AL2O3 AND FE-NI/AL2O3 CATALYSTS
    LESNIEWSKA, E
    RYNKOWSKI, J
    PARYJCZAK, T
    PRZEMYSL CHEMICZNY, 1995, 74 (01): : 21 - 22
  • [9] Steam reforming of ethanol for hydrogen production: influence of catalyst composition (Ni/Al2O3, Ni/Al2O3–CeO2, Ni/Al2O3–ZnO) and process conditions
    O. Shtyka
    Z. Dimitrova
    R. Ciesielski
    A. Kedziora
    G. Mitukiewicz
    J. Leyko
    W. Maniukewicz
    A. Czylkowska
    T. Maniecki
    Reaction Kinetics, Mechanisms and Catalysis, 2021, 132 : 907 - 919
  • [10] Experimental Study on CO2 Methanation over Ni/Al2O3, Ru/Al2O3, and Ru-Ni/Al2O3 Catalysts
    Chein, Rei-Yu
    Wang, Chih-Chang
    CATALYSTS, 2020, 10 (10) : 1 - 17