Repairing additive-manufactured 316L stainless steel using direct energy deposition

被引:118
|
作者
Oh, Wook Jin [1 ]
Lee, Wook Jin [2 ]
Kim, Min Seob [1 ]
Jeon, Jong Bae [2 ]
Shim, Do Sik [1 ]
机构
[1] Korea Maritime & Ocean Univ, Dept Ocean Adv Mat Convergence Engn, 727 Taejong Ro, Busan 49112, South Korea
[2] Korea Inst Ind Technol, Adv Surface Coating & Proc R&D Grp, 14,Namyangsan 1 Gil, Yangsan 506356, Gyeongsangnam D, South Korea
来源
基金
新加坡国家研究基金会;
关键词
Tensile behavior; Stainless steel SUS316L; Laser melting deposition; Cell structure; MECHANICAL-PROPERTIES; TOOL STEEL; LASER; MICROSTRUCTURE;
D O I
10.1016/j.optlastec.2019.04.012
中图分类号
O43 [光学];
学科分类号
070207 ; 0803 ;
摘要
Powder bed fusion (PBF), a 3D printing process, is widely used for manufacturing 316L stainless steel parts. When these PBF parts are damaged or worn severely during service, they can be repaired by conventional repair processes such as GTAW welding, metal spraying, brazing etc. However, these processes have several disadvantages such as creating a large heat affected zone and repair defects (pores and cracks). In contrast, directed energy deposition (DED) provides good metallurgical bonds, minimal dilution, and a small heat-affected zone. In this study, to verify the applicability of DED to repair of damaged PBF parts, we repaired sample parts and observed their tensile properties, hardness, and metallurgical characteristics. First, we designed hot-rolled and PBF specimens with trapezoidal grooves of varying depth. After filling the groove using DED, the specimens were tested for tensile properties. We found that in specimens with large groove depths (1 mm and 2 mm), cracks occurred around the repair due to thermal stresses and oxide inclusion. For this reason, strength and elongation were lower in these specimens. We also found that the micro-hardness of the deposition zone is greater than the original hot-rolled specimens and similar to the PBF specimens. The microstructure of the repaired area is mainly composed of complicated dendrite structures due to irregular nucleation. In addition, dimples were observed in the fracture surfaces, indicating that ductile fracture occurred. We conclude that the DED process can be employed to repair damaged 316L stainless steel parts, with the low severity of the damage to be repaired.
引用
收藏
页码:6 / 17
页数:12
相关论文
共 50 条
  • [1] On the Friction Stir Processing of Additive-Manufactured 316L Stainless Steel
    Sajadifar, Seyed Vahid
    Hosseinzadeh, Ali
    Richter, Julia
    Krochmal, Marcel
    Wegener, Thomas
    Bolender, Artjom
    Heidarzadeh, Akbar
    Niendorf, Thomas
    Yapici, Guney Guven
    [J]. ADVANCED ENGINEERING MATERIALS, 2022, 24 (10)
  • [2] Direct laser deposition of 316L stainless steel
    Majumdar, JD
    Manna, I
    Li, L
    [J]. TRENDS IN MATERIALS AND MANUFACTURING TECHNOLOGIES FOR TRANSPORTATION INDUSTRIES AND POWDER METALLURGY RESEARCH AND DEVELOPMENT IN THE TRANSPORTATION INDUSTRY, 2005, : 41 - 44
  • [3] Inclusion evolution in additive manufactured 316L stainless steel by laser metal deposition process
    Eo, Du-Rim
    Park, Sun-Hong
    Cho, Jung-Wook
    [J]. MATERIALS & DESIGN, 2018, 155 : 212 - 219
  • [4] Crack healing via electropulsing treatment applied to additive-manufactured TiC/316L stainless steel composites
    Cai, Qing
    Rey Rodriguez, Pilar
    Carracelas Santos, Sara
    Castro, Gemma
    Mendis, Chamini L.
    Chang, Isaac T.H.
    Assadi, Hamid
    [J]. Materials Letters, 2024, 365
  • [5] Enhancement and underlying fatigue mechanisms of laser powder bed fusion additive-manufactured 316L stainless steel
    Hamada, Atef
    Jaskari, Matias
    Gundgire, Tejas
    Jarvenpaa, Antti
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2023, 873
  • [6] Crack healing via electropulsing treatment applied to additive-manufactured TiC/316L stainless steel composites
    Cai, Qing
    Rodriguez, Pilar Rey
    Santos, Sara Carracelas
    Castro, Gemma
    Mendis, Chamini L.
    Chang, Isaac T. H.
    Assadi, Hamid
    [J]. MATERIALS LETTERS, 2024, 365
  • [7] Mechanical Properties and Behavior of Additive Manufactured Stainless Steel 316L
    Bevan, M. A.
    Ameri, A. A. H.
    East, D.
    Austin, D. C.
    Brown, A. D.
    Hazell, P. J.
    Escobedo-Diaz, J. P.
    [J]. CHARACTERIZATION OF MINERALS, METALS, AND MATERIALS 2017, 2017, : 577 - 583
  • [8] Investigation of hybrid manufacturing of stainless steel 316L components using direct energy deposition
    Tapoglou, Nikolaos
    Clulow, Joseph
    [J]. PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART B-JOURNAL OF ENGINEERING MANUFACTURE, 2021, 235 (10) : 1633 - 1643
  • [9] The Effect of the Deposition Strategy and Heat Treatment on Cold Spray Additive Manufactured 316L Stainless Steel
    Vaz, Rodolpho F.
    Luzin, Vladimir
    Salvemini, Filomena
    Ribamar, Giovani G.
    Avila, Julian A.
    Albaladejo, Vicente
    Sanchez, Javier
    Cano, Irene Garcia
    [J]. ADVANCED ENGINEERING MATERIALS, 2024, 26 (14)
  • [10] Effects of scanning pattern and laser power reduction in stainless Steel 316L additive manufactured by direct laser metal deposition
    Liu, Weiwei
    Abdelrahman, Ahmed
    Al-Hammadi, Gamal
    Saleheen, Kazi Mojtaba
    [J]. OPTICAL ENGINEERING, 2022, 61 (06)