Kinetic studies on sorption of n-hexane in vanadium substituted MFI type zeolites of various crystal morphologies

被引:1
|
作者
Kornatowski, Jan [1 ,2 ]
Wloch, Jerzy [2 ]
机构
[1] Max Planck Inst Kohlenforsch, D-45470 Mulheim An Der Ruhr, Germany
[2] Nicholas Copernicus Univ, Fac Chem, PL-87100 Torun, Poland
关键词
V-Sil-1; n-Hexane uptake; n-Hexane kinetics; MOLECULAR-SIEVES; ZSM-5; ZEOLITE; DIFFUSION; SILICALITE; TRANSPORT; MICROSCOPY; TOPOLOGY; BARRIERS; IODINE; GROWTH;
D O I
10.1016/j.micromeso.2009.04.028
中图分类号
O69 [应用化学];
学科分类号
081704 ;
摘要
The MFI type materials isomorphously substituted with vanadium form crystals of two morphology types. Investigations of sorption kinetics for n-hexane indicated for both morphologies a non-typical increase in the value of corrected transport diffusion coefficient with the crystals dimensions. An increase in the D-0 values with the vanadium content of the crystals has also been found, although it is not so well expressed as that with the dimensions. The increase in the D-0 values is from 1.1 x 10(-11) to 1.1 x 10(-10) m(2)/s and may be a consequence of an additional system of larger pores, which is not reflected in the adsorption isotherms due to common occurrence of these pores in all crystals. It is also possible that vanadium causes a superior structure ordering and a decrease in/weakening of diffusion barriers. (C) 2009 Elsevier Inc. All rights reserved.
引用
收藏
页码:17 / 22
页数:6
相关论文
共 48 条
  • [1] Sorption kinetics of n-hexane in MFI-type zeolites investigated by micro-FTIR spectroscopy
    Hermann, M
    Niessen, W
    Karge, HG
    CATALYSIS BY MICROPOROUS MATERIALS, 1995, 94 : 131 - 138
  • [2] Is diffusion controlled by crystal morphology?: Inclusion of morphology to modelling the n-hexane diffusion in MFI-type zeolites
    Wloch, Jerzy
    Kornatowski, Jan
    MICROPOROUS AND MESOPOROUS MATERIALS, 2008, 108 (1-3) : 303 - 310
  • [3] Crystal size of MFI-type zeolites for catalytic cracking of n-hexane under reaction-control conditions
    Nakasaka, Yuta
    Okamura, Takuya
    Konno, Hiroki
    Tago, Teruoki
    Masuda, Takao
    MICROPOROUS AND MESOPOROUS MATERIALS, 2013, 182 : 244 - 249
  • [4] Concentration and temperature dependence of the diffusivity of n-hexane in MFI-zeolites
    Lab. of Inorg. Chem. and Catalysis, Schuit Institute of Catalysis, Eindhoven University of Technology, P.O. Box 513, 5600 MB Eindhoven, Netherlands
    不详
    1600, 119-129 (January 26, 2005):
  • [5] Concentration and temperature dependence of the diffusivity of n-hexane in MFI-zeolites
    Koriabkina, AO
    de Jong, AM
    Hensen, EJM
    van Santen, RA
    MICROPOROUS AND MESOPOROUS MATERIALS, 2005, 77 (2-3) : 119 - 129
  • [6] Deactivation mechanism of MFI-type zeolites by coke formation during n-hexane cracking
    Nakasaka, Yuta
    Nishimura, Jun-ichi
    Tago, Teruoki
    Masuda, Takao
    CHEMICAL ENGINEERING JOURNAL, 2015, 278 : 159 - 165
  • [7] Deactivation mechanism of MFI-type zeolites by coke formation during n-hexane cracking
    Nakasaka, Yuta (nakasaka@eng.hokudai.ac.jp), 1600, Elsevier B.V., Netherlands (278):
  • [8] Hydrogen transfer reaction of N-hexane over various zeolites
    Zhu, H.Y.
    He, M.Y.
    Zhang, X.
    Song, J.Q.
    Shi You Lian Zhi Yu Hua Gong/Petroleum Processing and Petrochemicals, 2001, 32 (09):
  • [9] Temperature programmed desorption of n-hexane and n-heptane from MFI and FAU zeolites
    Wacław Makowski
    Dorota Majda
    Journal of Porous Materials, 2007, 14 : 27 - 35
  • [10] Temperature programmed desorption of n-hexane and n-heptane from MFI and FAU zeolites
    Makowski, Waclaw
    Majda, Dorota
    JOURNAL OF POROUS MATERIALS, 2007, 14 (01) : 27 - 35