摘要
A bioactive coating with no cracks was produced on the porous titanium by alkali-heat treatment. The morphology, element content and phase composition of the coating were analyzed by SEM, XRD and XPS. It is found that a micro-network structure mainly composed of bioactive sodium titanate and rutile covers the interior and exterior of porous titanium cells. And bioactive network without cracks is achievable with a given set of process parameters of the alkaline solution concentration and alkali-heat treatment time. After immersion into the SBF solution for 3 d, a carbonate-hydroxylapatite was detected by XRD on the cell surface of the porous titanium, showing a good compatibility of the porous titanium with bone.
引用
收藏
页码:1392 / 1396
页数:5
相关论文
共 18 条
  • [1] Biological performance of uncoated and octacalcium phosphate-coated Ti6A14V
    Habibovic, P
    Li, JP
    van der Valk, CM
    Meijer, G
    Layrolle, P
    van Blitterswijk, CA
    de Groot, K
    [J]. BIOMATERIALS, 2005, 26 (01) : 23 - 36
  • [2] Surface modification of a low-modulus Ti-7.5Mo alloy treated with aqueous NaOH
    Ho, Wen-Fu
    Lai, Chien-Hung
    Hsu, Hsueh-Chuan
    Wu, Shih-Ching
    [J]. SURFACE & COATINGS TECHNOLOGY, 2009, 203 (20-21): : 3142 - 3150
  • [3] Hui Liu, 2012, MAT CHINA, V31, P40
  • [4] Porosity of 3D biomaterial scaffolds and osteogenesis
    Karageorgiou, V
    Kaplan, D
    [J]. BIOMATERIALS, 2005, 26 (27) : 5474 - 5491
  • [5] XPS study of bioactive graded layer in Ti-In-Nb-Ta alloy prepared by alkali and heat treatments
    Lee, BH
    Kim, YD
    Lee, KH
    [J]. BIOMATERIALS, 2003, 24 (13) : 2257 - 2266
  • [6] Improving the strength and biocompatibility of porous titanium scaffolds by creating elongated pores coated with a bioactive, nanoporous TiO2 layer
    Lee, Jong-Hoon
    Kim, Hyoun-Ee
    Shin, Kwan-Ha
    Koh, Young-Hag
    [J]. MATERIALS LETTERS, 2010, 64 (22) : 2526 - 2529
  • [7] Liang FH, 2003, RARE METAL MAT ENG, V32, P930
  • [8] Degradation of the strength of porous titanium after alkali and heat treatment
    Lin, J. G.
    Li, Y. C.
    Wong, C. S.
    Hodgson, P. D.
    Wen, C. E.
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 485 (1-2) : 316 - 319
  • [9] Sol-gel deposited TiO2 film on NiTi surgical alloy for biocompatibility improvement
    Liu, JX
    Yang, DZ
    Shi, F
    Cai, YJ
    [J]. THIN SOLID FILMS, 2003, 429 (1-2) : 225 - 230
  • [10] Titanium alloys in total joint replacement - a materials science perspective
    Long, M
    Rack, HJ
    [J]. BIOMATERIALS, 1998, 19 (18) : 1621 - 1639