Using cone calorimeter to study thermal degradation of flexible PVC filled with zinc ferrite and Mg(OH)2

被引:32
|
作者
Qu, Hongqiang [1 ]
Liu, Caihong [1 ]
Wu, Weihong [2 ]
Chen, Lingzhi [1 ]
Xu, Jianzhong [1 ]
机构
[1] Hebei Univ, Coll Chem & Environm Sci, Baoding 071002, Hebei, Peoples R China
[2] Agr Univ Hebei, Coll Sci, Baoding 071000, Peoples R China
关键词
Poly(vinyl chloride); Mg(OH)(2); ZnFe2O4; Thermal analysis; Cone calorimeter; POLY(VINYL CHLORIDE); SMOKE-SUPPRESSION; FLAME-RETARDANT; HEAT-FLUX; DECOMPOSITION; ADDITIVES; EMISSION; BEHAVIOR; HALOGEN; CABLE;
D O I
10.1007/s10973-013-3434-3
中图分类号
O414.1 [热力学];
学科分类号
摘要
Flame-retarded poly(vinyl chloride) (PVC) materials have been prepared by using zinc ferrite (ZnFe2O4 (ZFO)) combined with magnesium hydroxide (Mg(OH)(2) (MH)). The effects of these additives on the combustion and thermal degradation of PVC samples were studied using the limiting oxygen index test, the smoke density rating test, thermogravimetric-differential thermogravimetry, and the cone calorimeter test. The results showed that ZFO and MH were good synergists for improving the flame retardancy and smoke-suppressing of PVC/MH/ZFO blends. ZFO can significantly improve the maximum mass loss velocity in the first stage, and reduce the initial decomposition temperature and the decomposition range in the PVC/MH/ZFO blends. The char yield at 700 A degrees C of flame-retarded PVC clearly decreased below theoretical values due to the cationic cracking reactions in the presence of ZFO. Furthermore, the PVC/10MH/10ZFO showed strong flame-retarding synergism since the decreased average heat release rate value. And the PVC/19MH/1ZFO presented a significant smoke-suppressing effect by the least average specific extinction area, peak smoke production rate, and total smoke produce. Moreover, the CO and CO2 production was increased because of a large amount of fragment of char residue in contact air in the presence of ZFO.
引用
收藏
页码:1081 / 1087
页数:7
相关论文
共 50 条
  • [1] Using cone calorimeter to study thermal degradation of flexible PVC filled with zinc ferrite and Mg(OH)2
    Hongqiang Qu
    Caihong Liu
    Weihong Wu
    Lingzhi Chen
    Jianzhong Xu
    Journal of Thermal Analysis and Calorimetry, 2014, 115 : 1081 - 1087
  • [2] Investigation of thermal degradation, flame retardancy and smoke suppression of rigid PVC by using cone calorimeter
    Li, Bin
    Wang, Jianqi
    Ding, Yangbing
    Gaofenzi Cailiao Kexue Yu Gongcheng/Polymeric Materials Science and Engineering, 1999, 15 (05): : 124 - 127
  • [3] Thermal Degradation Properties of Flexible PVC Filled with Alumina Trihydrate and Magnesium Hydroxide
    He Yi
    CHINESE JOURNAL OF INORGANIC CHEMISTRY, 2012, 28 (01) : 207 - 212
  • [4] Experimental study of suppressing PVC fire with water mist using a cone calorimeter
    Zhang, Yongfeng
    Zhu, Wei
    Zhou, Xiaomeng
    Qin, Jun
    Liao, Guanxuan
    JOURNAL OF FIRE SCIENCES, 2007, 25 (01) : 45 - 63
  • [5] A study of the effect of thickness on the thermal degradation and flammability characteristics of some composite materials using a cone calorimeter
    Fateh, Talal
    Kahanji, Charles
    Joseph, Paul
    Rogaume, Thomas
    JOURNAL OF FIRE SCIENCES, 2017, 35 (06) : 547 - 564
  • [6] Zinc Hydroxystannate-coated Mineral Grade Mg(OH)2 as Flame-Retardant and Smoke Suppression for Flexible PVC
    Chunzheng Wang
    Weihong Wu
    Xia Ye
    Lei Liu
    ADVANCES IN MATERIALS AND MATERIALS PROCESSING, PTS 1-3, 2013, 652-654 : 481 - +
  • [7] Experimental study on fire behaviors of flexible photovoltaic panels using a cone calorimeter
    Ju, Xiaoyu
    Zhou, Xiaodong
    Zhao, Kun
    Peng, Fei
    Yang, Lizhong
    JOURNAL OF FIRE SCIENCES, 2018, 36 (01) : 63 - 77
  • [8] Study on thermal degradation and flame retardant property of halogen-free polypropylene composites using XPS and cone calorimeter
    Tsai, Kuang-Chung
    Kuan, Chen-Feng
    Chen, Chia-Hsun
    Kuan, Hsu-Chiang
    Hsu, Shu-Wei
    Lee, Fang-Mei
    Chiang, Chin-Lung
    JOURNAL OF APPLIED POLYMER SCIENCE, 2013, 127 (02) : 1084 - 1091
  • [9] Study on Application of Modified Mg(OH)2 Flame Retardant in Fire Resistant PVC
    任拥军
    河南化工, 2007, (07) : 31 - 32
  • [10] KINETICS OF THE STABILIZING EFFECT OF CALCIUM AND ZINC STEARATES IN THE THERMAL-DEGRADATION OF PVC .2.
    LEVAI, G
    OCSKAY, G
    NYITRAI, Z
    POLYMER DEGRADATION AND STABILITY, 1989, 26 (01) : 11 - 20