Effects of intermetallic particles on cavitation during superplastic forming of aluminium alloy

被引:1
|
作者
Jin, H. [1 ]
Gerlich, A. P. [2 ]
机构
[1] Nat Resources Canada, CanmetMAT, Hamilton, ON L8P 0A5, Canada
[2] Univ Waterloo, Dept Mech & Mechatron Engn, Waterloo, ON, Canada
关键词
Aluminium alloy; superplasticity; friction stir processing; cavitation; CAVITY GROWTH; DEFORMATION; BEHAVIOR; MECHANISMS; FRACTURE; FAILURE;
D O I
10.1080/02670836.2019.1627498
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
An Al-4.6%Mg-1.5%Mn-0.27%Fe alloy was specially processed with friction stir processing followed by cold rolling. Half of the sheet thickness contains a large number of blocky or irregular-shaped Al-6(Mn,Fe) coarse intermetallic particles, while the other half, smaller and more spherical ones. The particle-induced cavitation upon uni-axial tension at 475 degrees C with 2 x 10(-4)-2 x 10(-2 )s(-1) strain rates was investigated. The density of nuclei for cavities was estimated based on quantitative image analysis of the particles, and the strain controlled growth rate, calculated assuming the cavities are nucleated before or in the early stage of straining. The number, size and morphology of intermetallic particles are found to control the cavitation by determining the nucleation rate, but the strain controlled growth rate appears unaffected.
引用
收藏
页码:1428 / 1435
页数:8
相关论文
共 50 条
  • [1] Cavitation During Superplastic Forming
    Campbell, John
    MATERIALS, 2011, 4 (07) : 1271 - 1286
  • [2] Superplastic forming of aluminium alloy 7475
    Horent, G
    COMPETITIVE ADVANTAGES BY NEAR-NET SHAPE MANUFACTURING, 1997, : 129 - 134
  • [3] Superplastic blow forming of 2219 aluminium alloy
    Kaibyshev, R
    Kazakulov, I
    Gromov, D
    Lesuer, DR
    Nieh, TG
    SUPERPLASTICITY IN ADVANCED MATERIALS, 2003, 447-4 : 265 - 270
  • [4] Superplastic forming and diffusion bonding of aluminium alloy
    Niu, JT
    Zhang, J
    Wang, MZ
    Wang, ZR
    THERMEC '97 - INTERNATIONAL CONFERENCE ON THERMOMECHANICAL PROCESSING OF STEELS AND OTHER MATERIALS, VOLS I-II, 1997, : 1923 - 1928
  • [5] Rapid forming of superplastic aluminium alloy 5083
    Lee, S
    Yu, YH
    Wu, HY
    Wang, JY
    Chang, CP
    MATERIALS SCIENCE AND TECHNOLOGY, 2001, 17 (11) : 1413 - 1416
  • [6] ON CONTROL OF CAVITATION IN AN AL-LI BASED ALLOY DURING SUPERPLASTIC FORMING
    PANDEY, MC
    MUKHERJEE, AK
    INDIAN JOURNAL OF TECHNOLOGY, 1987, 25 (12): : 579 - 585
  • [7] Deformation characteristics and cavitation during multiaxial blow forming in superplastic 8090 alloy
    Wu, Horng-yu
    Hwang, Jiin-her
    Chiu, Chui-hung
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2009, 209 (04) : 1654 - 1661
  • [8] Cavitation characteristics of a superplastic 5083 Al alloy during gas blow forming
    Horng-yu Wu
    Jau-yuean Perng
    Shyh-hung Shis
    Chui-hung Chiu
    Shyong Lee
    Jian-yih Wang
    Journal of Materials Science, 2006, 41 : 7446 - 7453
  • [9] Cavitation characteristics of a superplastic 5083 Al alloy during gas blow forming
    Wu, Horng-yu
    Perng, Jau-yuean
    Shis, Shyh-hung
    Chiu, Chui-hung
    Lee, Shyong
    Wang, Jian-yih
    JOURNAL OF MATERIALS SCIENCE, 2006, 41 (22) : 7446 - 7453
  • [10] Cavitation during multiaxial deformation of superplastic forming
    Khaleel, MA
    Smith, MT
    Lund, AL
    SUPERPLASTICITY IN ADVANCED MATERIALS - ICSAM-97, 1997, 243-2 : 155 - 160