摘要
Al2+ (320 keV) ions were implanted at room temperature into p-type (1 1 1)-Hg0.78Cd0.22Te with fluences ranging From 3x10(11) to 3x10(14) cm(-2). The implanted samples were analyzed by infrared reflectivity and by diffuse X-ray scattering. These two contactless and non-destructive techniques provide quantitative results on free carriers and on structural defects which are induced by ion implantation into p-type (1 1 1)-Hg0.78Cd0.22Te. Comparison between the evolution of the free carrier concentration and the evolution of the structural defects with increasing the fluence suggests that extended structural defects directly influence the doping concentration in as-implanted samples. (C) 2000 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:40 / 46
页数:7
相关论文
共 22 条
  • [1] POSITRON LIFETIME AND HOLE CONCENTRATION IN P-TYPE HG0.78CD0.22TE CRYSTALS
    GELYSIKES, C
    CORBEL, C
    TRIBOULET, R
    SOISSON, F
    BAROUX, L
    ANNALES DE CHIMIE-SCIENCE DES MATERIAUX, 1991, 16 (07): : 541 - 546
  • [2] Defects in ion implanted Hg0.78Cd0.22Te probed by monoenergetic positron beams
    Uedono, A
    Ebe, H
    Tanaka, M
    Suzuki, R
    Ohdaira, T
    Tanigawa, S
    Mikado, T
    Yamamoto, K
    Miyamoto, Y
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS, 1998, 37 (07): : 3910 - 3914
  • [3] Simple way to analyze infrared reflectivity spectra of p-type Hg0.78Cd0.22Te implanted in various conditions
    Leveque, P.
    Declemy, A.
    Nuclear Instruments and Methods in Physics Research, Section B: Beam Interactions with Materials and Atoms, 1999, 147 (1-4): : 181 - 186
  • [4] A simple way to analyze infrared reflectivity spectra of p-type Hg0.78Cd0.22Te implanted in various conditions
    Lévêque, P
    Declémy, A
    NUCLEAR INSTRUMENTS & METHODS IN PHYSICS RESEARCH SECTION B-BEAM INTERACTIONS WITH MATERIALS AND ATOMS, 1999, 147 (1-4): : 181 - 186
  • [5] OBSERVATION OF A DEEP LEVEL IN P-TYPE HG0.78CD0.22TE WITH HIGH DISLOCATION DENSITY
    CHEN, MC
    SCHIEBEL, RA
    JOURNAL OF APPLIED PHYSICS, 1992, 71 (10) : 5269 - 5271
  • [6] Defects and their annealing properties in B+-implanted Hg0.78Cd0.22Te studied by positron annihilation
    Uedono, A
    Ebe, H
    Tanaka, M
    Tanigawa, S
    Yamamoto, K
    Miyamoto, Y
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS, 1998, 37 (3A): : 786 - 791
  • [7] THE MINORITY-CARRIER LIFETIME IN DOPED AND UNDOPED P-TYPE HG0.78CD0.22TE LIQUID-PHASE EPITAXY FILMS
    CHEN, MC
    COLOMBO, L
    DODGE, JA
    TREGILGAS, JH
    JOURNAL OF ELECTRONIC MATERIALS, 1995, 24 (05) : 539 - 544
  • [8] ELECTRICAL EFFECTS OF DISLOCATIONS AND OTHER CRYSTALLOGRAPHIC DEFECTS IN HG0.78CD0.22TE N-ON-P PHOTODIODES
    LIST, RS
    JOURNAL OF ELECTRONIC MATERIALS, 1993, 22 (08) : 1017 - 1025
  • [9] IMPLANTATION-INDUCED DEFECTS IN HG0.78CD0.22TE STUDIED USING SLOW POSITRONS
    LISZKAY, L
    CORBEL, C
    BAROUX, L
    HAUTOJARVI, P
    DECLEMY, A
    RENAULT, PO
    JOURNAL OF PHYSICS-CONDENSED MATTER, 1995, 7 (45) : 8529 - 8538
  • [10] STRUCTURAL CHARACTERIZATION OF HG0.78CD0.22TE/CDTE LPE HETEROSTRUCTURES GROWN FROM TE SOLUTIONS
    BERNARDI, S
    BOCCHI, C
    FERRARI, C
    FRANZOSI, P
    LAZZARINI, L
    JOURNAL OF CRYSTAL GROWTH, 1991, 113 (1-2) : 53 - 60