Kinetic analysis of the thermooxidative degradation of poly(vinyl-chloride) in poly(vinyl chloride)/methyl methacrylate-butadiene-styrene blends 2. Nonisothermal degradation

被引:18
|
作者
Andricic, B [1 ]
Kovacic, T [1 ]
Klaric, L [1 ]
机构
[1] Univ Split, Fac Chem Technol, Dept Organ Chem Technol, Split 21000, Croatia
关键词
nonisothermal kinetics; PVC/MBS blends; thermooxidative degradation;
D O I
10.1016/S0141-3910(02)00290-2
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The thermooxidative degradation of poly(vinyl chloride)/(methyl methacrylate-butadiene-styrene) (PVC/MBS) blends was investigated by nonisothermal thermogravimetry in air. Measurements were carried out in the temperature range of 50-650 degreesC. The kinetic parameters (E-a and A) of the first degradation step were determined by applying the Flynn-Wall-Ozawa method. Their relationship through a compensation effect was discussed and an apparent compensation effect was found. The addition of MBS changes the rate of PVC dehydrochlorination in the blends, while in the blends with 15 and higher MBS ratio, the reaction scheme of degradation also changes. (C) 2002 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:265 / 270
页数:6
相关论文
共 50 条
  • [1] Kinetic analysis of the thermo-oxidative degradation of poly(vinyl chloride) in poly(vinyl chloride)/methyl methacrylate-butadiene-styrene blends 1 - Isothermal degradation
    Andricic, B
    Kovacic, T
    Klaric, I
    [J]. POLYMER DEGRADATION AND STABILITY, 2002, 78 (03) : 459 - 465
  • [2] Thermooxidative degradation of poly(vinyl chloride)/acrylonitrile-butadiene-styrene blends
    Faculty of Technology, Split, Croatia
    [J]. J Appl Polym Sci, 7 (1123-1129):
  • [3] Thermooxidative degradation of poly(vinyl chloride)/acrylonitrile-butadiene-styrene blends
    Klaric, I
    Roje, U
    Bravar, M
    [J]. JOURNAL OF APPLIED POLYMER SCIENCE, 1996, 61 (07) : 1123 - 1129
  • [4] Nonisothermal degradation of poly(vinyl chloride) methylmethacrylate-butadiene-styrene blends
    Andricic, B
    Kovacic, T
    [J]. POLYMER DEGRADATION AND STABILITY, 1999, 65 (01) : 59 - 64
  • [5] The toughness and morphology of (chlorinated poly[vinyl chloride])/(methyl methacrylate-butadiene-styrene) blends
    Ren, Liang
    Zhang, Shenwei
    Zhang, Mingyao
    Chen, Dan
    Zhu, Fupeng
    [J]. JOURNAL OF VINYL & ADDITIVE TECHNOLOGY, 2016, 22 (04): : 501 - 505
  • [6] Thermal degradation studies in poly(vinyl chloride)/poly(methyl methacrylate) blends
    Ahmad, Z.
    Al-Awadi, N. A.
    Al-Sagheer, F.
    [J]. POLYMER DEGRADATION AND STABILITY, 2008, 93 (02) : 456 - 465
  • [7] DEGRADATION OF POLY (VINYL-CHLORIDE) .2. OXIDATIVE DEGRADATION IN SOLUTION
    HENSON, JHL
    HYBART, FJ
    [J]. JOURNAL OF APPLIED POLYMER SCIENCE, 1973, 17 (01) : 129 - 136
  • [8] The influence of the internal structure of core-shell particles on poly(vinyl chloride)/(methyl methacrylate-butadiene-styrene) blends
    Zhou, Chao
    Qi, Xiaoxue
    Gao, Yun Xia
    Sun, Shulin
    Zhang, Huixuan
    [J]. POLYMER INTERNATIONAL, 2012, 61 (07) : 1067 - 1072
  • [9] Kinetics of thermooxidative degradation of poly(vinyl chloride)/chlorinated polyethylene blends
    Vrandecic, NS
    Klaric, I
    Kovacic, T
    [J]. POLYMER DEGRADATION AND STABILITY, 2004, 84 (01) : 31 - 39
  • [10] Degradation of poly(vinyl chloride) in the blend with methyl methacrylate/butadiene/styrene investigated by differential scanning calorimetry
    Andricic, B.
    Kovacic, T.
    [J]. Polimeri (Zagreb), 2000, 21 (06): : 191 - 193