Effect of magnetic abrasive treatment on high-temperature oxidation of NiAl and NiAl-Re coatings

被引:6
|
作者
Oliker, V. E. [1 ]
Gridasova, T. Ya. [2 ]
Sirovatka, V. L. [1 ]
Eliseeva, E. N. [1 ]
Timofeeva, I. I. [1 ]
Grechishkin, E. F. [1 ]
机构
[1] Natl Acad Sci Ukraine, Frantsevich Inst Problems Mat Sci, Kiev, Ukraine
[2] Natl Tech Univ Ukraine, Kiev Polytech Inst, Kiev, Ukraine
关键词
NiAl; rhenium; eutectic alloy; detonation coating; oxidation; magnetic abrasive treatment; PLUS GAMMA-RE; MECHANICAL-PROPERTIES; ALLOYS; MICROSTRUCTURE; SCALE;
D O I
10.1007/s11106-009-9142-7
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A comparative microstructural analysis of the scale formed on the NiAl-Re detonation coating shows that the mechanism of its high-temperature oxidation can be changed with preliminary magnetic abrasive treatment (MAT). The scale formed over the NiAl-Re coating in ordinary conditions includes several layers (NiO-NiAl(2)O(4)-Al(2)O(3)), while the scale formed on the MAT coating consists of an Al(2)O(3) monolayer with spinel inclusions. The differences in the oxidation of the NiAl and NiAl-Re coatings after MAT are attributed to changes in their dislocation structure.
引用
收藏
页码:466 / 477
页数:12
相关论文
共 50 条
  • [1] Effect of magnetic abrasive treatment on high-temperature oxidation of NiAl and NiAl–Re coatings
    V. E. Oliker
    T. Ya. Gridasova
    V. L. Sirovatka
    E. N. Eliseeva
    I. I. Timofeeva
    E. F. Grechishkin
    [J]. Powder Metallurgy and Metal Ceramics, 2009, 48 : 466 - 477
  • [2] HIGH-TEMPERATURE OXIDATION OF SPRAYED NiAl-Re COATINGS SUBJECTED TO MAGNETIC TREATMENT
    Oliker, V. E.
    Eliseeva, E. N.
    Gridasova, T. Ya.
    Timofeeva, I. I.
    [J]. POWDER METALLURGY AND METAL CERAMICS, 2010, 49 (5-6) : 339 - 346
  • [3] High-temperature oxidation of sprayed NiAl–Re coatings subjected to magnetic treatment
    V. E. Oliker
    E. N. Eliseeva
    T. Ya. Gridasova
    I. I. Timofeeva
    [J]. Powder Metallurgy and Metal Ceramics, 2010, 49 : 339 - 346
  • [4] EFFECT OF MAGNETIC TREATMENT ON THE MICROSTRUCTURE OF NiAl-Re ALLOY
    Oliker, V. E.
    Eliseeva, E. N.
    Gridasova, T. Ya.
    Timofeeva, I. I.
    Kotko, A. V.
    [J]. POWDER METALLURGY AND METAL CERAMICS, 2010, 49 (3-4) : 245 - 252
  • [5] High-temperature air oxidation of coatings based on eutectic (β-NiAl + γ-Re) alloys and NiAl intermetallide
    V. E. Oliker
    M. Yu. Barabash
    E. F. Grechishkin
    I. I. Timofeeva
    T. Ya. Gridasova
    [J]. Powder Metallurgy and Metal Ceramics, 2007, 46 : 175 - 181
  • [6] EFFECT OF MAGNETIC FIELD ON RESIDUAL STRESSES IN NiAl-Re DETONATION COATINGS
    Polyarus, E. N.
    Oliker, V. E.
    Gridasova, T. Ya.
    Chernega, S. M.
    Grechishkin, E. F.
    [J]. POWDER METALLURGY AND METAL CERAMICS, 2012, 50 (9-10) : 671 - 675
  • [7] High-temperature air oxidation of coatings based on eutectic (β-NiAl plus γ-Re) alloys and NiAl intermetallide
    Oliker, V. E.
    Barabash, M. Yu.
    Grechishkin, E. F.
    Timofeeva, I. I.
    Gridasova, T. Ya.
    [J]. POWDER METALLURGY AND METAL CERAMICS, 2007, 46 (3-4) : 175 - 181
  • [8] Effect of water vapor on high-temperature oxidation of NiAl alloy
    Zhu, Dingding
    Wang, Xinli
    Zhao, Jun
    Lu, Jian
    Zhou, Yichun
    Cai, Canying
    Huang, Jianyu
    Zhou, Guangwen
    [J]. CORROSION SCIENCE, 2020, 177 (177)
  • [9] High-Temperature Stress Measurements During the Oxidation of NiAl
    E. Schumann
    C. Sarioglu
    J. R. Blachere
    F. S. Pettit
    G. H. Meier
    [J]. Oxidation of Metals, 2000, 53 : 259 - 272
  • [10] High-temperature stress measurements during the oxidation of NiAl
    Schumann, E
    Sarioglu, C
    Blachere, JR
    Pettit, FS
    Meier, GH
    [J]. OXIDATION OF METALS, 2000, 53 (3-4): : 259 - 272