Materials selection for the in situ mirrors of laser diagnostics in fusion devices

被引:18
|
作者
Voitsenya, VS [1 ]
Konovalov, VG
Becker, MF
Motojima, O
Narihara, K
Schunke, B
机构
[1] Inst Plasma Phys, UA-310108 Kharkov, Ukraine
[2] Univ Texas, Dept Elect & Comp Engn, Austin, TX 78712 USA
[3] Natl Inst Fus Sci, Toki 5095292, Japan
[4] JET Joint Undertaking, Abingdon OX14 3EA, Oxon, England
来源
REVIEW OF SCIENTIFIC INSTRUMENTS | 1999年 / 70卷 / 04期
关键词
D O I
10.1063/1.1149704
中图分类号
TH7 [仪器、仪表];
学科分类号
0804 ; 080401 ; 081102 ;
摘要
When mirrors for the laser scattering diagnostic for large fusion devices need to be inside the vacuum chamber, they are subjected to irradiation by multiple high-energy laser pulses and bombardment by charge exchange atoms. Both of these assaults are known to degrade and eventually damage metal laser mirrors given sufficient time and flux. Our aim in this article is to use current data on these damage mechanisms to make design selections of metal mirror materials for application in fusion device diagnostics. We identify tradeoffs between low sputtering rates and multipulse laser damage resistance in candidate metals. The data for multipulse laser damage are incomplete and extend to a maximum of only 10(4) shots for a few metals. However, there is a clear trend of decreasing laser-damage threshold with increasing number of shots, and damage threshold fluences can fall to 10% of the single-pulse damaging laser fluence. Further experiments up to 10(6) or 10(8) laser shots need to be conducted on the likely mirror candidate metals for use in new plasma devices. We define a figure-of-merit based on current laser damage data and employ it in our analysis. Recent data on the sputtering yield and reflectance degradation of metal mirrors give a different priority ranking of candidate metals. Overall, the preferred material selection depends on the number of laser shots and the number of plasma pulses that the mirror must endure before replacement is allowed. For example, we find that for conditions typical of the LHD (10 s plasma pulses with a 10 Hz laser PRF), Au, Ag, and Cu are candidate materials if mirrors are replaced after 10(3) plasma pulses; Au and Rh are candidates if the replacement interval is 10(4) pulses; and if the replacement interval is further increased to 10(5) plasma pulses, then Mo is the candidate material. Other materials might also be candidates but the data on them are still insufficient. (C) 1999 American Institute of Physics. [S0034-6748(99)02104-8].
引用
收藏
页码:2016 / 2025
页数:10
相关论文
共 50 条
  • [1] Investigations of mirrors for ITER diagnostics in modern fusion devices
    Voitsenya, V. S.
    Litnovsky, A.
    PLASMA DEVICES AND OPERATIONS, 2009, 17 (04): : 309 - 318
  • [2] On the choice of materials for the first mirrors of plasma diagnostics in a fusion reactor
    Voitsenya, V.S.
    Bardamid, A.F.
    Gritsyna, V.T.
    Konovalov, V.G.
    Motojima, O.
    Orlinskij, D.V.
    Palladino, R.
    Peterson, B.J.
    Shapoval, A.N.
    Shtan, A.F.
    Solodovchenko, S.I.
    Yakimov, K.I.
    Young, K.
    Journal of Nuclear Materials, 1998, 258-263 (pt B): : 1919 - 1923
  • [3] On the choice of materials for the first mirrors of plasma diagnostics in a fusion reactor
    Voitsenya, VS
    Bardamid, AF
    Gritsyna, VT
    Konovalov, VG
    Motojima, O
    Orlinskij, DV
    Palladino, R
    Peterson, BJ
    Shapoval, AN
    Shtan, AF
    Solodovchenko, SI
    Yakimov, KI
    Young, K
    JOURNAL OF NUCLEAR MATERIALS, 1998, 258 : 1919 - 1923
  • [4] Probe diagnostics for fusion devices
    Van Oost, G
    FUSION SCIENCE AND TECHNOLOGY, 2006, 49 (2T) : 357 - 366
  • [5] Ultrafast laser processing of transparent materials supported by in-situ diagnostics
    Kumkar, M.
    Kaiser, M.
    Kleiner, J.
    Grossmann, D.
    Flamm, D.
    Bergner, K.
    Nolte, S.
    LASER APPLICATIONS IN MICROELECTRONIC AND OPTOELECTRONIC MANUFACTURING (LAMOM) XXI, 2016, 9735
  • [6] PARABOLIC-MIRRORS FOR LASER FUSION
    HOWARD, JE
    BULLETIN OF THE AMERICAN PHYSICAL SOCIETY, 1977, 22 (09): : 1120 - 1120
  • [7] On the choice of material for the first mirrors of fusion reactor plasma diagnostics
    Voitsenya, VS
    Bardamid, AF
    Borisenko, YN
    Gritsyna, VI
    Gritsyna, VT
    Konovalov, VG
    Odintsov, NB
    Orlinski, DV
    Palladino, R
    Ruzhitskij, VV
    Rybin, VV
    Shapoval, AN
    Shtan, AF
    Solodovchenko, S
    Yakimov, KI
    Young, K
    PLASMA DEVICES AND OPERATIONS, 1999, 7 (04): : 243 - 254
  • [8] Development of laser-based diagnostics for surface characterisation of wall components in fusion devices
    Huber, A.
    Schweer, B.
    Philipps, V.
    Gierse, N.
    Zlobinski, M.
    Brezinsek, S.
    Biel, W.
    Kotov, V.
    Leyte-Gonzales, R.
    Mertens, Ph
    Samm, U.
    FUSION ENGINEERING AND DESIGN, 2011, 86 (6-8) : 1336 - 1340
  • [9] Laser damage thresholds of ITER mirror materials and first results on in situ laser cleaning of stainless steel mirrors
    Wisse, M.
    Marot, L.
    Eren, B.
    Steiner, R.
    Mathys, D.
    Meyer, E.
    FUSION ENGINEERING AND DESIGN, 2013, 88 (05) : 388 - 399
  • [10] Selection of plasma-facing materials in next-step fusion devices
    Federici, G
    Barabash, V
    Janeschitz, G
    Tivey, R
    Loarte, A
    Roth, J
    Skinner, CH
    Wampler, WR
    19TH IEEE/NPSS SYMPOSIUM ON FUSION ENGINEERING, PROCEEDINGS, 2002, : 311 - 320