Microtensile bond strength testing of luting cements to prefabricated CAD/CAM ceramic and composite blocks

被引:132
|
作者
El Zohairy, AA
De Gee, AJ
Mohsen, MM
Feilzer, AJ
机构
[1] Acad Ctr Dent Amsterdam, Dept Dent Mat Sci, NL-1066 EA Amsterdam, Netherlands
[2] Cairo Univ, Fac Oral & Dent Med, Dept Operat Dent, Cairo, Egypt
关键词
microtensile testing; adhesion; bond strength; resin cements; ceramic; composite; fracture; CAD/CAM;
D O I
10.1016/S0109-5641(02)00107-0
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives. To investigate the Microtensile bond strength (muTBS) and failure mode of resin cements bonded to composite and ceramic CAD/CAM blocks following various surface treatments. Methods. Paradigm composite blocks and Cerec Vitablocs received three surface treatments following the control treatment of surface grinding with 600 SiC grit. (1) Application of adhesive resin (Adh), (2) etching with hydrofluoric acid and silanization (HF + S) or (3) combination of the previous two treatments (HF + S + Adh). Three resin cements (Tetric Flow, Nexus 2, RelyX ARC) were applied to these surfaces and built-up in layers. After 24 h water storage at 37 degreesC, the non-trimming version of muTBS test was used to produce I nun 2 microbars. The Microbars were subjected to a tensile load using a modified testing device. The broken specimens were examined with a stereomicroscope and SEM to determine the failure mode. Results. All control and adhesive treated groups of the ceramic substrate showed premature debonding during cutting. The overall mean muTBS for the three resin cements bonded to ceramic following HF + S and HF + S + Adh surface treatment, was 27 and 29.2 MPa and for the resin cements bonded to composite substrate was 42.3 and 54.2 MPa, respectively. The mode of failure was 98% adhesive with composite as a substrate and 68% mixed failures with ceramic as a substrate. Clinical significance. CAD/CAM restorations fabricated from processed composite blocks may have advantage over the ceramic blocks with regard to the higher bond strength with resin cements. (C) 2003 Academy of Dental Materials. Published by Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:575 / 583
页数:9
相关论文
共 50 条
  • [1] Microtensile bond strength testing of luting cements to ceramic and composite inlay materials.
    El Zohairy, A
    De Gee, AJ
    Pallay, P
    Feilzer, AJ
    Davidson, CL
    [J]. JOURNAL OF DENTAL RESEARCH, 2002, 81 : B269 - B269
  • [2] Microtensile bond strength of CAD/CAM blocks using different resin cements
    Samborski, Jackie
    [J]. JOURNAL OF THE CANADIAN DENTAL ASSOCIATION, 2010, 76
  • [3] Microtensile bond strength of self-adhesive luting cements to ceramic
    Escribano, Nuria
    de la Macorra, Jose C.
    [J]. JOURNAL OF ADHESIVE DENTISTRY, 2006, 8 (05): : 337 - 341
  • [4] Microtensile Bond Strength Between Self-Adhesive Resin Cements and Resin Based Ceramic CAD/CAM Block
    Berkman, Meric
    Tuncer, Safa
    Tekce, Neslihan
    Karabay, Ferda
    Demirci, Mustafa
    [J]. ODOVTOS INTERNATIONAL JOURNAL OF DENTAL SCIENCES, 2021, 23 (01) : 116 - 125
  • [5] Microtensile bond strength testing of resin cements
    Yesil, Zeynep Duymus
    [J]. INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2009, 29 (04) : 352 - 355
  • [6] Microtensile Bond Strength of Self-Adhesive Luting Cements to Ceramics
    Abo, Tomoko
    Uno, Shigeru
    Yoshiyama, Masahiro
    Yamada, Toshimoto
    Hanada, Nobuhiro
    [J]. INTERNATIONAL JOURNAL OF DENTISTRY, 2012, 2012
  • [7] Bond strength of hybrid glass ionomer luting cements using prefabricated composite cones.
    Mora, KR
    Solano, E
    Lafuente, JD
    [J]. JOURNAL OF DENTAL RESEARCH, 2000, 79 : 359 - 359
  • [8] Bonding of resin cements for luting CAD/CAM ceramic restoration.
    Kamada, K
    Yoshida, K
    Matsumura, H
    Atsuta, M
    [J]. JOURNAL OF DENTAL RESEARCH, 1997, 76 : 1424 - 1424
  • [9] Effects of ceramic surface treatments on the bond strength of an adhesive luting agent to CAD-CAM ceramic
    Peumans, M.
    Hikita, K.
    De Munck, J.
    Van Landuyt, K.
    Poitevin, A.
    Larnbrechts, P.
    Van Meerbeek, B.
    [J]. JOURNAL OF DENTISTRY, 2007, 35 (04) : 282 - 288
  • [10] BOND STRENGTHS OF LUTING CEMENTS BETWEEN CAD/CAM CERAMICS AND ENAMEL
    CHANG, JC
    DAVIS, RJ
    HURST, TL
    ESTEY, AW
    [J]. JOURNAL OF DENTAL RESEARCH, 1995, 74 : 424 - 424