Development and characterization of edible plant-based fibers using a wet-spinning technique

被引:26
|
作者
Cui, Bing [1 ,3 ]
Liang, Hongshan [1 ,3 ]
Li, Jing [1 ,3 ]
Zhou, Bin [2 ]
Chen, Wenxin [1 ,3 ]
Liu, Jiao [5 ]
Li, Bin [1 ,3 ,4 ]
机构
[1] Huazhong Agr Univ, Coll Food Sci & Technol, Wuhan 430070, Peoples R China
[2] Hubei Univ Technol, Natl Ctr Cellular Regulat & Mol Pharmaceut 111, Sch Biol Engn & Food, Key Lab Fermentat Engn,Minist Educ,Hubei Key Lab I, Wuhan 430068, Peoples R China
[3] Huazhong Agr Univ, Key Lab Environm Correlat Dietol, Minist Educ, Wuhan, Peoples R China
[4] Funct Food Engn & Technol Res Ctr Hubei Prov, Wuhan, Peoples R China
[5] South Cent Minzu Univ, Coll Life Sci, Wuhan, Peoples R China
基金
中国国家自然科学基金;
关键词
Edible fiber; Meat analogue; Wet spinning; Solution behavior; Mechanical properties; Soybean protein isolate; DELIVERY-SYSTEMS; SODIUM ALGINATE; HYDROGEN-BONDS; PROTEIN; FABRICATION; EXTRUSION; BLENDS; IMPACT; HEAT;
D O I
10.1016/j.foodhyd.2022.107965
中图分类号
O69 [应用化学];
学科分类号
081704 ;
摘要
Analogous to those of natural animal muscle fibers is considered to be a major challenge in improving the texture of meat analog foods. Herein, in this current work, a facile and effective wet-spinning strategy is introduced for edible fibers fabrication based on sodium alginate/soybean protein isolate composite, which, to a large extent, significantly regulated by the interactions between polysaccharides and proteins. As illustrated, the ratio of polysaccharide/protein and pH values tailored the solution behavior of composite solutions, suggesting an influence of the spinning medium on the spinnability outcomes. The FTIR result after Gaussian multi-peaks-fitting additionally proved the types and relative strengths of hydrogen bonds in composite fibers, modulated by varying the preparation parameters. The SEM images of fibers showed that it could easily lead to the generation of porous structure inside the fiber in higher protein content or in alkaline pH condition. Importantly, increasing protein content could improve the water holding capacity, also impacting the stronger tensile strength of the composite fiber under neutral condition. In general, the facile preparation of edible fibers and the use of naturally abundant components in their synthesis provide a novel subassembly for the industrialized production of plantbased meat analogue.
引用
收藏
页数:12
相关论文
共 50 条
  • [1] Fabrication and characterization of Alginate Fibers by Wet-Spinning
    Xu, Guokai
    Liu, Lin
    Yao, Juming
    SILK, PROTECTIVE CLOTHING AND ECO-TEXTILES, 2013, 796 : 87 - 91
  • [2] Wet-spinning and applications of functional fibers based on chitin and chitosan
    Hirano, S
    MACROMOLECULAR SYMPOSIA, 2001, 168 : 21 - 30
  • [3] THE CRYSTALLIZATION DURING WET-SPINNING FOR MODACRYLIC FIBERS
    TSAI, JS
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1992, 11 (14) : 1017 - 1019
  • [5] Microstructure of PAN precursor fibers in wet-spinning
    Ge, He-Yi
    Liu, Hua-Shi
    Chen, Juan
    Cailiao Gongcheng/Journal of Materials Engineering, 2009, (07): : 50 - 53
  • [6] Production of pure nanotube fibers using a modified wet-spinning method
    Steinmetz, J
    Glerup, M
    Paillet, M
    Bernier, P
    Holzinger, M
    CARBON, 2005, 43 (11) : 2397 - 2400
  • [7] The Coagulation Process of Nascent Fibers in PAN Wet-spinning
    陈娟
    葛曷一
    Journal of Wuhan University of Technology(Materials Science), 2010, (02) : 200 - 205
  • [8] The formation of polyacrylonitrile nascent fibers in wet-spinning process
    Chen, Juan
    Ge, He-Yi
    Dong, Xing-Guang
    Wang, Cheng-Guo
    JOURNAL OF APPLIED POLYMER SCIENCE, 2007, 106 (01) : 692 - 696
  • [9] The Coagulation Process of Nascent Fibers in PAN Wet-spinning
    陈娟
    葛曷一
    Journal of Wuhan University of Technology(Materials Science Edition), 2010, 25 (02) : 200 - 205
  • [10] The coagulation process of nascent fibers in PAN wet-spinning
    Juan Chen
    Heyi Ge
    Huashi Liu
    Guozhong Li
    Chengguo Wang
    Journal of Wuhan University of Technology-Mater. Sci. Ed., 2010, 25 : 200 - 205