Testing of Mode-I Fracture Toughness of Sandstone Based on the Fracturing Mechanism of an Explosion Stress Wave

被引:3
|
作者
Xiao, Dingjun [1 ,2 ]
Yang, Wentao [2 ]
Liu, Chuanju [2 ]
Hu, Rong [3 ]
机构
[1] Southwest Univ Sci & Technol, Shock & Vibrat Engn Mat & Struct Key Lab Sichuan, Mianyang 621010, Sichuan, Peoples R China
[2] Southwest Univ Sci & Technol, Sch Environm & Resource, Mianyang 621010, Sichuan, Peoples R China
[3] Sichuan Univ, Coll Architecture & Environm, Chengdu 610065, Peoples R China
关键词
Blast loading; Surface blast wave; Blast-induced first wave; Crack propagation velocity; Dynamic stress intensity factor; INTENSITY FACTORS; ROCK; PRESSURE; STRENGTH; BEHAVIOR; DAMAGE;
D O I
10.1007/s00603-022-03047-8
中图分类号
P5 [地质学];
学科分类号
0709 ; 081803 ;
摘要
The dynamic fracture toughness of rock materials under blast load is the basis for studying the stability of rock blasting engineering. To study the dynamic fracture characteristics of sandstone with an explosive load, the initiation and propagation times of pre-crack samples with different lengths were obtained through physical experiments. The experimental-numerical method was used to obtain the stress intensity factor (SIF) curve and the crack initiation toughness of the specimens with different pre-crack lengths. By comparing and analyzing the dynamic SIF and explosion load curves at different pre-crack lengths, the following results and conclusions were obtained: (1) a polyvinylidene fluoride pressure gauge effectively measured the blast pressure curves at the blast hole wall and the blast hole with a diameter of 40 mm in the presence of a coupling water medium that could effectively avoid the formation of crushed zones and reduce the attenuation of the blast energy. (2) The crack-tip SIF curves were well correlated to the blast pressure curves with a minimal SIF lagging of 0.3-2.9 mu s after the peak of the blast pressure curve and a maximum SIF lagging of 0.1-22.9 mu s after the time when the peak blast pressure decayed to zero, and the lagging time increased with the pre-crack length. (3) The crack was affected by the reflected wave during the propagation process, and the reflected wave did not affect the crack propagation within 0-109.8 mu s. The longer the pre-crack length was, the longer the reflected wave influence time was. (4) The SIF at the pre-crack tip was controlled to a degree such that the first wave was superposed on the surface wave of the crack surface. Both the peak value of the stress intensity factor curve and the crack initiation toughness value decreased with the increase of the pre-crack length, and an obvious separation inflection point appeared on the stress intensity factor curve with the increase of the pre-crack length. (5) The implications of these findings particularly regarding the test method for dynamic fracture of materials tested by explosion method are discussed.
引用
收藏
页码:7731 / 7745
页数:15
相关论文
共 50 条
  • [1] Testing of Mode-I Fracture Toughness of Sandstone Based on the Fracturing Mechanism of an Explosion Stress Wave
    Dingjun Xiao
    Wentao Yang
    Chuanju Liu
    Rong Hu
    Rock Mechanics and Rock Engineering, 2022, 55 : 7731 - 7745
  • [2] Mode-I Fracture Toughness and Fracturing Damage Model for Sandstone Subjected to Cryogenic Treatment to-160 °C
    Zhang, Yuliang
    Gu, Yiming
    Ma, Guowei
    ROCK MECHANICS AND ROCK ENGINEERING, 2024, 57 (10) : 7929 - 7943
  • [3] Mode-I fracture toughness and damage mechanism of dry and saturated sandstone subject to cryogenic condition
    Zhang, Yuliang
    Ma, Guowei
    Li, Xudong
    INTERNATIONAL JOURNAL OF ROCK MECHANICS AND MINING SCIENCES, 2024, 180
  • [4] Study of mode-I fracture toughness and its correlation with strength parameters of sandstone
    Deng, H.-F. (dhf8010@ctgu.edu.cn), 2012, Academia Sinica (33):
  • [5] Effect of T-stress on the mode-I fracture toughness of concrete
    Zhao, Yan-hua
    Xu, Bo-han
    COMPTES RENDUS MECANIQUE, 2014, 342 (08): : 490 - 500
  • [6] MODE-I FRACTURE-TOUGHNESS OF COAL
    BHAGAT, RB
    INTERNATIONAL JOURNAL OF MINING ENGINEERING, 1985, 3 (03): : 229 - 236
  • [7] Influence of distinct testing methods on the mode-I fracture toughness of Longmaxi shale
    Zheng, Kun
    Zhao, Yu
    Wang, Chaolin
    Bi, Jing
    THEORETICAL AND APPLIED FRACTURE MECHANICS, 2024, 129
  • [8] A SUGGESTED PROCEDURE FOR COMBINED MODE-I - MODE-III FRACTURE-TOUGHNESS TESTING
    MANOHARAN, M
    HIRTH, JP
    ROSENFIELD, AR
    JOURNAL OF TESTING AND EVALUATION, 1990, 18 (02) : 106 - 114
  • [9] ANALYTICAL COMPLIANCE METHOD FOR MODE-I INTERLAMINAR FRACTURE-TOUGHNESS TESTING OF COMPOSITES
    KAGEYAMA, K
    KOBAYASHI, T
    CHOU, TW
    COMPOSITES, 1987, 18 (05): : 393 - 399
  • [10] Testing method study of mode-I dynamic fracture toughness under blasting loads
    College of Architecture and Environment, Sichuan University, Chengdu
    Sichuan
    610065, China
    Yanshilixue Yu Gongcheng Xuebao, (2767-2772):