摘要
The present paper presents a two-phase model for the fatigue damage evolution in welded steel joints. The argument for choosing a two-phase model is that crack initiation and subsequent crack propagation involve different damage mechanisms and should be treated separately. The crack initiation phase is defined as the number of cycles to reach a crack depth of 0.1 mm. This phase is modelled based on the Dang Van multiaxial stress approach. Both a multiaxial stress situation introduced by the acting loads and the presence of the multiaxial welding residual stresses are accounted for. The local notch effect at the weld toe becomes very important and the irregular weld toe geometry is characterized by extreme value statistics for the weld toe angle and radius. The subsequent crack growth is based in classical fracture based on the Paris law including the effect of the Stress Intensity Factor Range (SIFR) threshold value. The unique fatigue crack growth rate curve suggested by Huang, Moan and Cui is adopted. This approach keeps the growth rate parameters C and m constant whereas an effective SIFR is calculated for the actual stress range and loading ratio. The model is developed and verified based on fatigue crack growth data from fillet welded joints where cracks are emanating from the weld toe. For this test series measured crack depths below 0.1 mm are available. The two-phase model was in addition calibrated to fit the life prediction in the rule based S-N curve designated category 71 (or class F). A supplementary S-N curve is obtained by the Random Fatigue Limit Method (RFLM). The test results and the fitted model demonstrated that the crack initiation phase in welded joins is significant and cannot be ignored. The results obtained by the Dang Van approach for the initiation phase are promising but the modelling is not yet completed. The fracture mechanics model for the propagation phase gives good agreement with measured crack growth. However, it seems that the prediction of crack retardation based on a threshold value for the SIFR gives a fatigue limit that is overly optimistic for small cracks at the weld toe. The threshold value has been determined based on tests with rather large central cracks in plates. The validity for applying this threshold value for small cracks at the weld toe is questioned. As the present two-phase model is based on applied mechanics for both phases the parameters that have an influence on the fatigue damage evolution are directly entering into the model. Any change in these parameters can then be explicitly taken into account in logical and rational manner for fatigue life predictions. This not the case with the rule based S-N curves that are based on pure statistical treatment of the bulk fatigue life.
引用
收藏
页数:16
相关论文
共 50 条
  • [1] Modeling of welded joints for design against fatigue
    J. Rudolph
    E. Weiß
    M. Forster
    Engineering with Computers, 2003, 19 : 142 - 151
  • [2] Fatigue damage evolution and lifetime prediction of welded joints with the consideration of residual stresses and porosity
    Shen, Fei
    Zhao, Bo
    Li, Lin
    Chua, Chee Kai
    Zhou, Kun
    INTERNATIONAL JOURNAL OF FATIGUE, 2017, 103 : 272 - 279
  • [3] Modeling of welded joints for design against fatigue
    Rudolph, J
    Weiss, E
    Forster, M
    ENGINEERING WITH COMPUTERS, 2003, 19 (2-3) : 142 - 151
  • [4] Fatigue durability and damage tolerance verification of welded joints
    Lassen, T
    FATIGUE '99: PROCEEDINGS OF THE SEVENTH INTERNATIONAL FATIGUE CONGRESS, VOLS 1-4, 1999, : 1239 - 1244
  • [5] The evolution of the welded joints structure at low cycle fatigue
    Poyarkova, Ekaterina
    Kuzeev, Iskander
    INTERNATIONAL CONFERENCE ON MODERN TRENDS IN MANUFACTURING TECHNOLOGIES AND EQUIPMENT (ICMTMTE 2017), 2017, 129
  • [6] Acoustic emission detection of fatigue damage in cruciform welded joints
    Yu, Jianguo
    Ziehl, Paul
    Matta, Fabio
    Pollock, Adrian
    JOURNAL OF CONSTRUCTIONAL STEEL RESEARCH, 2013, 86 : 85 - 91
  • [7] FATIGUE BEHAVIOR AND DAMAGE MONITORING OF ULTRASONIC WELDED HYBRID JOINTS
    Huxhold, Stefan
    Balle, Frank
    Wagner, Guntram
    Eifler, Dietmar
    PROCEEDINGS OF THE 13TH INTERNATIONAL CONFERENCE ON ALUMINUM ALLOYS (ICAA13), 2012, : 505 - 510
  • [8] Rolling Contact Fatigue Damage in Welded Rail Steel Joints
    Torskaya, E. V.
    Goryacheva, I. G.
    Muravyeva, T. I.
    Shcherbakova, O. O.
    Tsukanov, I. Yu.
    Meshcheryakova, A. R.
    Shkaley, I. V.
    Zagranichek, K. L.
    Zakharov, S. M.
    Shur, E. A.
    PHYSICAL MESOMECHANICS, 2023, 26 (01) : 7 - 18
  • [9] Rolling Contact Fatigue Damage in Welded Rail Steel Joints
    E. V. Torskaya
    I. G. Goryacheva
    T. I. Muravyеva
    O. O. Shcherbakova
    I. Yu. Tsukanov
    A. R. Meshcheryakova
    I. V. Shkaley
    K. L. Zagranichek
    S. M. Zakharov
    E. A. Shur
    Physical Mesomechanics, 2023, 26 : 7 - 18
  • [10] FATIGUE DAMAGE ESTIMATION OF WELDED JOINTS CONSIDERING MECHANOCHEMICAL INTERACTION
    Liu, Gang
    Huang, Yi
    Zhang, Qi
    Li, Zhiyuan
    Chen, Jingjie
    Dong, Leilei
    PROCEEDINGS OF THE ASME 36TH INTERNATIONAL CONFERENCE ON OCEAN, OFFSHORE AND ARCTIC ENGINEERING, 2017, VOL 3A, 2017,