Metal dusting and coking of alloy 803

被引:0
|
作者
Han, GW [1 ]
Feng, D [1 ]
Deng, B [1 ]
机构
[1] Cent Iron & Steel Res Inst, Dept High Temp Mat Res, Beijing 100081, Peoples R China
关键词
superalloys; SEM; metal dusting; coking;
D O I
10.1016/S0010-938X(03)00147-1
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Investigation was made by SEM examination on metal dusting and coking behaviours of alloy 803 in a flowing gas mixture of H-2-CO-H2O, It was found that an oxide scale arisen on the sample surface at the beginning of exposure, Metal dusting started when graphite deposition occurred earlier at the local defects in the oxide settle than the defects were repaired by enough supply of chromium from the interior of alloy matrix. Coke consisted of graphite filaments and metallic particles produced by disintegrating of alloy matrix, and grow up from the defects in the oxide scale with pit left in the sample surface, Increasing chromium content, doping a small amount of silicon and reducing grain size to create fast diffusion paths for chromium and silicon to alloy surface, all promote the formation of a dense oxide scale and favor early self-repairing or the defects in the oxide scale before occurrence of graphite deposition, The resistance of an alloy to metal dusting can be improved generally by means of these methods, (C) 2003 Elsevier Ltd. All rights reserved.
引用
收藏
页码:443 / 452
页数:10
相关论文
共 50 条
  • [1] Coking by metal dusting of steels
    Müller-Lorenz, EM
    Grabke, HJ
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 1999, 50 (11): : 614 - 621
  • [2] Relationship between coking and metal dusting
    Chun, CM
    Ramanarayanan, TA
    Mumford, JD
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 1999, 50 (11): : 634 - 639
  • [3] Metal dusting and coking on steels by synthesis gas
    Müller-Lorenz, EM
    Grabke, H
    CORROSION IN REFINERY PETROCHEMICAL AND POWER GENERATION PLANTS, PROCEEDINGS, 2000, : 213 - 220
  • [4] Coking by metal dusting of nickel-base alloys
    Strauss, S
    Krajak, R
    Grabke, HJ
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 1999, 50 (11): : 622 - 627
  • [5] Metal dusting of low alloy steels
    Grabke, H.J.
    Bracho-Troconis, C.B.
    Mueller-Lorenz, E.M.
    Werkstoffe und Korrosion, 1994, 45 (04): : 215 - 221
  • [6] METAL DUSTING OF LOW-ALLOY STEELS
    GRABKE, HJ
    BRACHOTROCONIS, CB
    MULLERLORENZ, EM
    WERKSTOFFE UND KORROSION-MATERIALS AND CORROSION, 1994, 45 (04): : 215 - 221
  • [7] METAL DUSTING OF LOW-ALLOY AND HIGH-ALLOY STEELS
    GRABKE, HJ
    CORROSION, 1995, 51 (09) : 711 - 720
  • [8] MATHEMATICAL MODEL FOR METAL DUSTING ON LOW ALLOY STEELS
    Chen, Cheng
    Zhou, Changyu
    Hu, Guiming
    Lei, Na
    PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE, VOL 6, PTS A AND B, 2010, : 977 - 982
  • [9] Metal dusting of inlet tube made of alloy 800
    Hrivñák, I
    Caplovic, L
    Bakay, G
    Bitter, A
    KOVOVE MATERIALY-METALLIC MATERIALS, 2005, 43 (04): : 290 - 299
  • [10] Metal dusting on an alumina forming Ni-base alloy
    Szakalos, P.
    Lundberg, M.
    Pettersson, R.
    CORROSION SCIENCE, 2006, 48 (07) : 1679 - 1695