Effect of EDM Conditions on Surface Residual Stress of Cr12MoV Steel

被引:7
|
作者
Li, X. S. [1 ]
Cai, A. H. [1 ]
Zeng, J. J. [1 ]
机构
[1] Hunan Inst Sci & Technol, Sch Mech Engn, Yueyang 414006, Peoples R China
关键词
EDM(electric discharge machining); Surface processing; Residual stress; HOLE-DRILLING METHOD;
D O I
10.4028/www.scientific.net/MSF.697-698.171
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this paper, surface residual stress in the cold working tool steel (Cr12MoV) by EDM was investigated by X-350 X-ray residual stress analyzer and method of DJP-2 electrolytic polishing instrument to remove layer by layer in the different EDM conditions. The results show that the distribution of surface residual stress generated not only by the peak discharge current and pulse width, but also by pulse interval. The same depth from the surface, residual stress of material after hardening is larger than the residual stress after annealing, With the different combination of tool electrode and work-piece material, the form of the discharge between two electrodes and the proportion of energy put between two electrodes are different, surface residual stress are also different. Different processing liquid for processing, the depth of residual stress generated is much the same, but closer to the surface, the worse the cooling capacity (quench degrees) and surface physical properties of processing fluids, the greater the residual stress. EDM, the generation and control of the surface residual stress depends on the choice such as processing power criteria, work-piece material, electrode materials and processing liquid. Surface residual stress after processing can be used to eliminate high-temperature heat treatment.
引用
收藏
页码:171 / 175
页数:5
相关论文
共 50 条
  • [1] Study of Surface Residual Stress in Hard Turning of Die Steel Cr12MoV
    Yue, Caixu
    Liu, Xianli
    Ma, Jing
    Liu, Xue
    Ren, Guangxu
    ADVANCES IN MACHINING AND MANUFACTURING TECHNOLOGY XII, 2014, 589-590 : 33 - 37
  • [2] Analysis of Grinding Residual Stress for Cr12MoV Die Steel by Simulation
    Zhou, Li-Qun
    Long, Ting
    Ouyang, Mu-Ying
    Qiu, Yi
    MECHANICS AND MATERIALS SCIENCE, 2018, : 477 - 482
  • [3] Effects of high-frequency vibration on quenched residual stress in Cr12MoV steel
    Bang-ping Gu
    Xiong Hu
    Jin-tao Lai
    Zi-di Jin
    Hui Zhou
    Zhen-sheng Yang
    Long Pan
    Journal of Materials Research, 2016, 31 : 3588 - 3596
  • [4] Effects of high-frequency vibration on quenched residual stress in Cr12MoV steel
    Gu, Bang-Ping
    Hu, Xiong
    Lai, Jin-tao
    Jin, Zi-di
    Zhou, Hui
    Yang, Zhen-sheng
    Pan, Long
    JOURNAL OF MATERIALS RESEARCH, 2016, 31 (22) : 3588 - 3596
  • [5] Effect of ultrasonic surface rolling processing on wear properties of Cr12MoV steel
    Gong, Lichao
    Pan, Yongzhi
    Peng, Chao
    Fu, Xiuli
    Jiang, Zhenfeng
    Jiang, Shuai
    MATERIALS TODAY COMMUNICATIONS, 2022, 33
  • [6] Effect of spray forming and aging treatment on Cr12MoV steel
    Xu, H.B.
    Tang, L.
    Wu, J.S.
    Zhang, J.G.
    Shanghai Jiaotong Daxue Xuebao/Journal of Shanghai Jiaotong University, 2000, 34 (12): : 1601 - 1605
  • [7] Optimization of Cr12MoV Steel Boronizing Technology
    Chen, Jing
    Yang, Anjie
    Hao, Shaoxiang
    OPTICAL, ELECTRONIC MATERIALS AND APPLICATIONS, PTS 1-2, 2011, 216 : 687 - 691
  • [10] Microstructure of laser melted layer on Cr12MoV steel
    Li, Xiaodong
    Yin, Zhongda
    Jinshu Xuebao/Acta Metallurgica Sinica, 1991, 27 (01):