The effect of porcelain thickness and surface liner application on the fracture behavior of a ceramic system

被引:50
|
作者
Benetti, Paula [1 ]
Pelogia, Fernanda [1 ]
Valandro, Luiz Felipe [2 ]
Bottino, Marco Antonio [1 ]
Della Bona, Alvaro [3 ]
机构
[1] Sao Paulo State Univ, Dept Dent Mat & Prosthodont, Sao Jose Dos Campos, SP, Brazil
[2] Univ Fed Santa Maria, Dept Restorat Dent Prosthodont, BR-97119900 Santa Maria, RS, Brazil
[3] Univ Passo Fundo, Dept Restorat Dent, Passo Fundo, RS, Brazil
基金
巴西圣保罗研究基金会;
关键词
Ceramic; Flexural strength; Thickness; Liner; Stress concentration; STABILIZED ZIRCONIA; FLEXURAL STRENGTH; THERMAL COMPATIBILITY; VENEERING PORCELAIN; COOLING RATE; PART II; CORE; CROWNS; TRANSLUCENCY; RELIABILITY;
D O I
10.1016/j.dental.2011.05.009
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives. To determine the effect of porcelain thickness and the application of a surface liner (SL) on the flexural strength (sigma) of a ceramic system. Methods. One hundred twenty bar-shaped specimens of yttria-stabilized zirconia-based ceramic were fabricated and randomly divided into two groups according to the application of SL: A-applied; B-not applied. The specimens were further divided according to the porcelain veneer thickness (n = 20): 0-0.5 mm; 1-1.0 mm; 2-2.0 mm. All specimens were tested in 3-point bending with the porcelain under tension. The maximum load was recorded at first sign of fracture, the sigma was calculated and the mode of failure was determined. Data was statistically analyzed using one-way ANOVA, Tukey (alpha = 0.05) and Weibull distribution. Results. The SL application had no effect (p = 0.723) while the porcelain thickness had a significant effect (p = 0.000) on the mean sigma values. No significant differences in mean sigma values were found with same porcelain thickness. A 0.5-mm thick porcelain layer (groups A0 and B0) showed greater mean sigma values than other groups. The Weibull modulus (m) ranged from 6 (groups A1 and B2) to 9 (groups A0, A2 and B0). The predominant mode of failure for all groups was fracture initiation at the porcelain surface propagating to the ceramic interface. Significance. The porcelain thickness influenced the mean sigma values, but the SL had no significant effect on the flexural strength and the mode of failure of the ceramic system examined. (C) 2011 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:948 / 953
页数:6
相关论文
共 50 条
  • [1] Effect of liner and porcelain application on zirconia surface structure and composition
    Alghazzawi, Tariq F.
    Janowski, Gregg M.
    INTERNATIONAL JOURNAL OF ORAL SCIENCE, 2016, 8 (03) : 164 - 171
  • [2] Effect of liner and porcelain application on zirconia surface structure and composition
    Tariq F Alghazzawi
    Gregg M Janowski
    International Journal of Oral Science, 2016, 8 : 164 - 171
  • [3] Effect of liner and porcelain application on zirconia surface structure and composition
    Tariq F Alghazzawi
    Gregg M Janowski
    International Journal of Oral Science, 2016, 8 (03) : 164 - 171
  • [4] The Application of a Novel Ceramic Liner Improves Bonding between Zirconia and Veneering Porcelain
    Lee, Hee-Sung
    Kwon, Tae-Yub
    MATERIALS, 2017, 10 (09)
  • [5] EFFECT OF PORCELAIN THICKNESS AND TYPE OF METAL-CERAMIC ALLOY ON COLOR
    JACOBS, SH
    GOODACRE, CJ
    MOORE, BK
    DYKEMA, RW
    JOURNAL OF PROSTHETIC DENTISTRY, 1987, 57 (02): : 138 - 145
  • [6] Effect of Incisal Porcelain Veneering Thickness on the Fracture Resistance of CAD/CAM Zirconia All-Ceramic Anterior Crowns
    Badran, Noha
    Kader, Sanaa Abdel
    Alabbassy, Fayza
    INTERNATIONAL JOURNAL OF DENTISTRY, 2019, 2019
  • [7] EFFECT OF CRYSTALLITES ON SURFACE DAMAGE AND FRACTURE-BEHAVIOR OF A GLASS-CERAMIC
    MORENA, R
    NIIHARA, K
    HASSELMAN, DPH
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1983, 66 (10) : 673 - 682
  • [8] The surface analysis of metal/ceramic alloys prior to porcelain application.
    Johnson, A
    Van Noort, R
    JOURNAL OF DENTAL RESEARCH, 2003, 82 : 507 - 507
  • [9] Effect of glaze thickness on the fracture toughness and hardness of alumina-reinforced porcelain
    Baharav, H
    Laufer, BZ
    Pilo, R
    Cardash, HS
    JOURNAL OF PROSTHETIC DENTISTRY, 1999, 81 (05): : 515 - 519
  • [10] Temperature effect on dielectric behavior of an industrial porcelain-type ceramic
    Hachicha, O.
    Ghorbel, N.
    Kallel, A.
    Fakhfakh, Z.
    CANADIAN JOURNAL OF PHYSICS, 2009, 87 (09) : 973 - 980